Volumn 263, Issue 1-6 SPEC. ISS., 2007, Pages 745-755

Studies on the dry sliding wear behaviour of hypoeutectic and eutectic Al-Si alloys

Author keywords

Al Si alloys; Al Ti B grain refiners; and Al Sr modifier; Sliding wear behaviour

Indexed keywords

ALUMINUM ALLOYS; DENDRITES (METALLOGRAPHY); EUTECTICS; GRAIN REFINEMENT; MICROSTRUCTURE; TRIBOLOGY;

EID: 34748867907     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.wear.2006.11.026     Document Type: Article
Times cited : (101)

References (22)
  • 1
    • 0016876948 scopus 로고
    • Wear characteristics of metals
    • Eyre T.S. Wear characteristics of metals. Tribol. Int. 9 (1976) 1-10
    • (1976) Tribol. Int. , vol.9 , pp. 1-10
    • Eyre, T.S.1
  • 2
    • 0035803518 scopus 로고    scopus 로고
    • Study on wear properties of aluminium-silicon piston alloy
    • Haque M.M., and Sharif A. Study on wear properties of aluminium-silicon piston alloy. J. Mater. Process. Technol. 118 (2001) 69-73
    • (2001) J. Mater. Process. Technol. , vol.118 , pp. 69-73
    • Haque, M.M.1    Sharif, A.2
  • 4
    • 0035418565 scopus 로고    scopus 로고
    • Influence of Ti addition on wear properties of Al-Si eutectic alloys
    • Saheb N., Laoui T., Daud A.R., Harun M., Radiman S., and Yahaya R. Influence of Ti addition on wear properties of Al-Si eutectic alloys. Wear 249 (2001) 656-662
    • (2001) Wear , vol.249 , pp. 656-662
    • Saheb, N.1    Laoui, T.2    Daud, A.R.3    Harun, M.4    Radiman, S.5    Yahaya, R.6
  • 6
    • 0024881950 scopus 로고
    • Grain refining of aluminium and its alloys using inoculants
    • McCartney D.G. Grain refining of aluminium and its alloys using inoculants. Int. Mater. Rev. 34 (1989) 247-260
    • (1989) Int. Mater. Rev. , vol.34 , pp. 247-260
    • McCartney, D.G.1
  • 7
    • 34748840734 scopus 로고
    • A new combination grain refiner/modifier for hypoeutectic Al-Si foundry alloys
    • Dunville B.T., Young D.K., and Boone G.W. A new combination grain refiner/modifier for hypoeutectic Al-Si foundry alloys. Light Metals (1994) 1065-1071
    • (1994) Light Metals , pp. 1065-1071
    • Dunville, B.T.1    Young, D.K.2    Boone, G.W.3
  • 8
    • 34748854766 scopus 로고    scopus 로고
    • S. A. Kori, Studies on the Grain Refinement and Modification of some hypoeutectic and eutectic Al-Si alloys, Ph.D. Thesis, IIT Kharagpur, 2000.
  • 9
    • 0033879804 scopus 로고    scopus 로고
    • Development of an efficient grain refiner for Al-7Si alloy and its modified with strontium
    • Kori S.A., Murty B.S., and Chakraborty M. Development of an efficient grain refiner for Al-7Si alloy and its modified with strontium. Mater. Sci. Eng. A 280 (2000) 94-104
    • (2000) Mater. Sci. Eng. A , vol.280 , pp. 94-104
    • Kori, S.A.1    Murty, B.S.2    Chakraborty, M.3
  • 11
    • 0016452647 scopus 로고
    • Wear of aluminium-silicon alloys
    • Sarkar A.D. Wear of aluminium-silicon alloys. Wear 31 (1975) 331-343
    • (1975) Wear , vol.31 , pp. 331-343
    • Sarkar, A.D.1
  • 12
    • 0018468706 scopus 로고
    • Wear characteristics of as-cast binary aluminium silicon alloys
    • Clarke J., and Sarkar A.D. Wear characteristics of as-cast binary aluminium silicon alloys. Wear 54 (1979) 7-16
    • (1979) Wear , vol.54 , pp. 7-16
    • Clarke, J.1    Sarkar, A.D.2
  • 13
    • 45949118566 scopus 로고
    • Characteristics of dry sliding wear of Al-Si alloys
    • Pramila Bai B.N., and Biswas S.K. Characteristics of dry sliding wear of Al-Si alloys. Wear 120 (1987) 61-74
    • (1987) Wear , vol.120 , pp. 61-74
    • Pramila Bai, B.N.1    Biswas, S.K.2
  • 14
    • 84996184995 scopus 로고
    • Wear characteristics of castings used in internal combustion engines
    • Eyre T.S. Wear characteristics of castings used in internal combustion engines. Met. Technol. 11 (1984) 81-90
    • (1984) Met. Technol. , vol.11 , pp. 81-90
    • Eyre, T.S.1
  • 15
    • 0029257021 scopus 로고
    • Mechanism of seizure of aluminium-silicon alloys dry sliding against steel
    • Somi Reddy A., Pramila Bai B.N., Murthy K.S.S., and Biswas S.K. Mechanism of seizure of aluminium-silicon alloys dry sliding against steel. Wear 181-183 (1995) 658-667
    • (1995) Wear , vol.181-183 , pp. 658-667
    • Somi Reddy, A.1    Pramila Bai, B.N.2    Murthy, K.S.S.3    Biswas, S.K.4
  • 17
    • 0028381863 scopus 로고
    • Wear characteristics of Al-Si alloys
    • Torabian H., Patak J.P., and Tiwari S.N. Wear characteristics of Al-Si alloys. Wear 172 (1994) 49-58
    • (1994) Wear , vol.172 , pp. 49-58
    • Torabian, H.1    Patak, J.P.2    Tiwari, S.N.3
  • 18
    • 34748845607 scopus 로고    scopus 로고
    • Abrasive wear characteristics of as cast aluminium silicon alloys sliding against corundum disc
    • Pathak J.P., and Mohan S. Abrasive wear characteristics of as cast aluminium silicon alloys sliding against corundum disc. Indian Foundry J. (1998) 1-9
    • (1998) Indian Foundry J. , pp. 1-9
    • Pathak, J.P.1    Mohan, S.2
  • 19
    • 0030153166 scopus 로고    scopus 로고
    • Effect of element addition on wear properties of eutectic aluminium-silicon alloys
    • Harun M., Talib I.A., and Daud A.R. Effect of element addition on wear properties of eutectic aluminium-silicon alloys. Wear 194 (1996) 54-59
    • (1996) Wear , vol.194 , pp. 54-59
    • Harun, M.1    Talib, I.A.2    Daud, A.R.3
  • 20
    • 0029518092 scopus 로고
    • Effect of copper on the tribological properties of Al-Si base alloys
    • Dasgupta A., and Bose S.K. Effect of copper on the tribological properties of Al-Si base alloys. J. Mater. Sci. Lett. 14 (1995) 1661-1663
    • (1995) J. Mater. Sci. Lett. , vol.14 , pp. 1661-1663
    • Dasgupta, A.1    Bose, S.K.2
  • 21
    • 0017551508 scopus 로고
    • The influence of structural modification on the wear resistance of a hypereutectic aluminium-silicon alloy
    • Clegg A.J., and Das A.A. The influence of structural modification on the wear resistance of a hypereutectic aluminium-silicon alloy. Br. Foundryman (1977) 333-349
    • (1977) Br. Foundryman , pp. 333-349
    • Clegg, A.J.1    Das, A.A.2
  • 22
    • 0004056939 scopus 로고
    • Pergaman Press, England 50-160
    • Sarkar A.D. Wear of Metals (1976), Pergaman Press, England 50-160
    • (1976) Wear of Metals
    • Sarkar, A.D.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.