Volumn 90, Issue 10, 2007, Pages 3341-3344

Contact damage of silicon carbide/boron nitride nanocomposites

Author keywords

[No Author keywords available]

Indexed keywords

BORON NITRIDE; CRACKS; PLASTIC DEFORMATION; SILICON CARBIDE;

EID: 34548845585     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2007.01894.x     Document Type: Article
Times cited : (10)

References (27)
  • 1
    • 0025476409 scopus 로고
    • Fiber-Matrix Bond-Strength Characterization of Silicon Carbide-Silicon Carbide Material
    • F. Abbe J.-L. Chermant Fiber-Matrix Bond-Strength Characterization of Silicon Carbide-Silicon Carbide Material J. Am. Ceram. Soc., 73 [8] 2573 5 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.73 , Issue.8 , pp. 2573-5
    • Abbe, F.1    Chermant, J.-L.2
  • 2
    • 0034251462 scopus 로고    scopus 로고
    • Effects of Grain-Boundary Structure on the Strength, Toughness, and Cyclic-Fatigue Properties of a Monolithic Silicon Carbide
    • D. Chen, X.-F. Zhang R. O. Ritchie Effects of Grain-Boundary Structure on the Strength, Toughness, and Cyclic-Fatigue Properties of a Monolithic Silicon Carbide J. Am. Ceram. Soc., 83 [8] 2079 81 (2000).
    • (2000) J. Am. Ceram. Soc. , vol.83 , Issue.8 , pp. 2079-81
    • Chen, D.1    Zhang, X.-F.2    Ritchie, R.O.3
  • 3
    • 0019657998 scopus 로고
    • 4-BN Composite for Improved Electrical and Thermal Shock Behavior
    • 4-BN Composite for Improved Electrical and Thermal Shock Behavior J. Am. Ceram. Soc., 64 [7] 415 8 (1981).
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.7 , pp. 415-8
    • Mazdiyasni, K.S.1    Ruh, R.2
  • 4
    • 0000806147 scopus 로고
    • A Contribution to the Crystallochemistry of Boron Nitride
    • V. Brozek M. Hubacek A Contribution to the Crystallochemistry of Boron Nitride J. Solid State Chem., 100, 120 9 (1992).
    • (1992) J. Solid State Chem. , vol.100 , pp. 120-9
    • Brozek, V.1    Hubacek, M.2
  • 5
    • 0022787859 scopus 로고
    • Boron Nitride Effect on the Thermal Shock Resistance of an Almina-Based Ceramic Composite
    • D. Goeuriot-Launay, G. Brayet F. Thevenot Boron Nitride Effect on the Thermal Shock Resistance of an Almina-Based Ceramic Composite J. Mater. Sci. Lett., 5, 940 2 (1986).
    • (1986) J. Mater. Sci. Lett. , vol.5 , pp. 940-2
    • Goeuriot-Launay, D.1    Brayet, G.2    Thevenot, F.3
  • 7
    • 33745358910 scopus 로고    scopus 로고
    • Machinable a-SiAlON/BN Composites
    • R. Shuba I.-W. Chen Machinable a-SiAlON/BN Composites J. Am. Ceram. Soc., 89 [7] 2147 53 (2006).
    • (2006) J. Am. Ceram. Soc. , vol.89 , Issue.7 , pp. 2147-53
    • Shuba, R.1    Chen, I.-W.2
  • 8
    • 0036863613 scopus 로고    scopus 로고
    • Fabrication and Microstructure of Silicon Nitride/Boron Nitride Nanocomposites
    • T. Kusunose, T. Sekino, Y.-H. Choa K. Niihara Fabrication and Microstructure of Silicon Nitride/Boron Nitride Nanocomposites J. Am. Ceram. Soc., 85 [11] 2678 88 (2002).
    • (2002) J. Am. Ceram. Soc. , vol.85 , Issue.11 , pp. 2678-88
    • Kusunose, T.1    Sekino, T.2    Choa, Y.-H.3    Niihara, K.4
  • 9
    • 0036864701 scopus 로고    scopus 로고
    • Machinability of Silicon Nitride/Boron Nitride Nanocomposites
    • T. Kusunose, T. Sekino, Y.-H. Choa K. Niihara Machinability of Silicon Nitride/Boron Nitride Nanocomposites J. Am. Ceram. Soc., 85 [11] 2689 95 (2002).
    • (2002) J. Am. Ceram. Soc. , vol.85 , Issue.11 , pp. 2689-95
    • Kusunose, T.1    Sekino, T.2    Choa, Y.-H.3    Niihara, K.4
  • 10
    • 2342461063 scopus 로고    scopus 로고
    • Fabrication of Machinable Silicon Carbide-Boron Nitride Ceramic Nanocomposite
    • X. Wang, G. Qiao Z. Jin Fabrication of Machinable Silicon Carbide-Boron Nitride Ceramic Nanocomposite J. Am. Ceram. Soc., 87 [4] 565 70 (2004).
    • (2004) J. Am. Ceram. Soc. , vol.87 , Issue.4 , pp. 565-70
    • Wang, X.1    Qiao, G.2    Jin, Z.3
  • 11
    • 0035413171 scopus 로고    scopus 로고
    • In Situ Reaction Synthesis of Silicon Carbide-Boron Nitride Composites
    • G.-J. Zhang T. Ohji In Situ Reaction Synthesis of Silicon Carbide-Boron Nitride Composites J. Am. Ceram. Soc., 84 [7] 1475 9 (2001).
    • (2001) J. Am. Ceram. Soc. , vol.84 , Issue.7 , pp. 1475-9
    • Zhang, G.-J.1    Ohji, T.2
  • 12
    • 33244495319 scopus 로고    scopus 로고
    • Fabrication of Boron Nitride Dispersed Nanocomposites by Chemical Processing and Their Mechanical Properties
    • T. Kusunose Fabrication of Boron Nitride Dispersed Nanocomposites by Chemical Processing and Their Mechanical Properties J. Ceram. Soc. Jpn., 114 [2] 167 73.
    • J. Ceram. Soc. Jpn. , vol.114 , Issue.2 , pp. 167-73
    • Kusunose, T.1
  • 13
    • 33644577266 scopus 로고
    • Hertzian Fracture in Single Crystals with the Diamond Structure
    • B. R. Lawn Hertzian Fracture in Single Crystals with the Diamond Structure J. Appl. Phys., 39 [10] 4828 36 (1968).
    • (1968) J. Appl. Phys. , vol.39 , Issue.10 , pp. 4828-36
    • Lawn, B.R.1
  • 14
    • 0001179338 scopus 로고
    • Indentation Plasticity and the Ensuing Fracture of Glass
    • M. V. Swain J. T. Hagan Indentation Plasticity and the Ensuing Fracture of Glass J. Phys. D: Appl. Phys., 9, 2201 14 (1976).
    • (1976) J. Phys. D: Appl. Phys. , vol.9 , pp. 2201-14
    • Swain, M.V.1    Hagan, J.T.2
  • 15
    • 0016521376 scopus 로고
    • Indentation Fracture: Principles and Applications
    • B. R. Lawn T. R. Wilshaw Indentation Fracture: Principles and Applications J. Mater. Sci., 10 [6] 1049 81 (1975).
    • (1975) J. Mater. Sci. , vol.10 , Issue.6 , pp. 1049-81
    • Lawn, B.R.1    Wilshaw, T.R.2
  • 16
    • 0026939155 scopus 로고
    • The Hertzian Stress Field and Formation of Cone Cracks: II. Determination of Fracture Toughness
    • K. Zeng, K. Breder D. J. Rowcliffe The Hertzian Stress Field and Formation of Cone Cracks: II. Determination of Fracture Toughness Acta Metal., 40 [10] 2601 5 (1992).
    • (1992) Acta Metal. , vol.40 , Issue.10 , pp. 2601-5
    • Zeng, K.1    Breder, K.2    Rowcliffe, D.J.3
  • 18
    • 0028529919 scopus 로고
    • Toughness Properties of a Silicon Carbide with an in Situ Induced Heterogeneous Grain Structure
    • N. P. Padture B. R. Lawn Toughness Properties of a Silicon Carbide With an In Situ Induced Heterogeneous Grain Structure J. Am. Ceram. Soc., 77 [10] 2518 22 (1994).
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.10 , pp. 2518-22
    • Padture, N.P.1    Lawn, B.R.2
  • 20
    • 0029172160 scopus 로고
    • Enhanced Machinability of Silicon Carbide Via Microstructural Design
    • N. P. Padture, C. J. Evans, H. H. K. Xu B. R. Lawn Enhanced Machinability of Silicon Carbide Via Microstructural Design J. Am. Ceram. Soc., 78 [1] 215 7 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.1 , pp. 215-7
    • Padture, N.P.1    Evans, C.J.2    Xu, H.H.K.3    Lawn, B.R.4
  • 21
    • 0029324743 scopus 로고
    • Ceramic Composites of Monazite and Alumina
    • P. E. D. Morgan D. B. Marshall Ceramic Composites of Monazite and Alumina J. Am. Ceram. Soc., 78 [6] 1553 63 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.6 , pp. 1553-63
    • Morgan, P.E.D.1    Marshall, D.B.2
  • 23
    • 0029172160 scopus 로고
    • Enhanced Machinability of Silicon Carbide Via Microstructural Design
    • N. P. Padture, C. J. Evans, H. H. K. Xu B. R. Lawn Enhanced Machinability of Silicon Carbide Via Microstructural Design J. Am. Ceram. Soc., 78 [1] 215 7 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.1 , pp. 215-7
    • Padture, N.P.1    Evans, C.J.2    Xu, H.H.K.3    Lawn, B.R.4
  • 24
    • 84884280887 scopus 로고
    • Indentation Fatigue: A Simple Cyclic Hertzian Test for Measuring Damage Accumulation in Polycrystalline Ceramics
    • F. Guiberteau, N. P. Padture, H. Cai B. R. Lawn Indentation Fatigue: A Simple Cyclic Hertzian Test for Measuring Damage Accumulation in Polycrystalline Ceramics Philos. Mag., A68 [5] 1003 16 (1993).
    • (1993) Philos. Mag. , vol.68 , Issue.5 , pp. 1003-16
    • Guiberteau, F.1    Padture, N.P.2    Cai, H.3    Lawn, B.R.4
  • 25
    • 0030259864 scopus 로고    scopus 로고
    • Stress Analysis of Contact Deformation in Quasi-Plastic Ceramics
    • A. C. Fischer-Cripps B. R. Lawn Stress Analysis of Contact Deformation in Quasi-Plastic Ceramics J. Am. Ceram. Soc., 79 [10] 2609 18 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.10 , pp. 2609-18
    • Fischer-Cripps, A.C.1    Lawn, B.R.2
  • 26
    • 0030086772 scopus 로고    scopus 로고
    • Indentation Stress-Strain Curves for 'Quasi-Ductile' Ceramics
    • A. C. Fischer-Cripps B. R. Lawn Indentation Stress-Strain Curves for 'Quasi-Ductile' Ceramics Acta Mater., 44 [2] 519 27 (1996).
    • (1996) Acta Mater. , vol.44 , Issue.2 , pp. 519-27
    • Fischer-Cripps, A.C.1    Lawn, B.R.2
  • 27
    • 0028392231 scopus 로고
    • Deformation and Fracture of Mica-Containing Glass-Ceramics in Hertzian Contacts
    • H. Cai, M. A. Stevens Kalceff B. R. Lawn Deformation and Fracture of Mica-Containing Glass-Ceramics in Hertzian Contacts J. Mater. Res., 9 [3] 762 70 (1994).
    • (1994) J. Mater. Res. , vol.9 , Issue.3 , pp. 762-70
    • Cai, H.1    Stevens Kalceff, M.A.2    Lawn, B.R.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.