메뉴 건너뛰기




Volumn 33, Issue 8, 2007, Pages 1563-1567

Sintering of MgO-based refractories with added WO3

Author keywords

D. MgO; Liquid sintering; Microstructure

Indexed keywords

DENSIFICATION; GRAIN BOUNDARIES; MAGNESIA; MICROSTRUCTURE; SCANNING ELECTRON MICROSCOPY; SINTERING; THERMAL SHOCK;

EID: 34548818742     PISSN: 02728842     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ceramint.2006.07.014     Document Type: Article
Times cited : (30)

References (19)
  • 1
    • 34548840154 scopus 로고    scopus 로고
    • A consideration on corrosion of magnesia refractory brick by silicate slag
    • Matsui T., Hiragushi K., Ikemoto T., and Sawano K. A consideration on corrosion of magnesia refractory brick by silicate slag. Taikabutsu 54 2 (2002) 67-71
    • (2002) Taikabutsu , vol.54 , Issue.2 , pp. 67-71
    • Matsui, T.1    Hiragushi, K.2    Ikemoto, T.3    Sawano, K.4
  • 2
    • 0032677603 scopus 로고    scopus 로고
    • Melt corrosion of oxide and oxide-C refractories
    • Lee W.E., and Zhang S. Melt corrosion of oxide and oxide-C refractories. Int. Mater. Rev. 44 (1999) 77-104
    • (1999) Int. Mater. Rev. , vol.44 , pp. 77-104
    • Lee, W.E.1    Zhang, S.2
  • 3
    • 0035427241 scopus 로고    scopus 로고
    • Thermochemistry and microstructures of MgO-C refractories containing various antioxidants
    • Zhang S., Marriott N.J., and Lee W.E. Thermochemistry and microstructures of MgO-C refractories containing various antioxidants. J. Eur. Ceram. Soc. 21 (2001) 1037-1047
    • (2001) J. Eur. Ceram. Soc. , vol.21 , pp. 1037-1047
    • Zhang, S.1    Marriott, N.J.2    Lee, W.E.3
  • 5
    • 0033284796 scopus 로고    scopus 로고
    • Secondary phases in natural magnesite sintered with addition of titania, ilmenite and zirconia
    • Chaudhuri M., Banerjee G., Kumar A., and Sarkar S.L. Secondary phases in natural magnesite sintered with addition of titania, ilmenite and zirconia. J. Mater. Sci. 34 (1999) 5821-5825
    • (1999) J. Mater. Sci. , vol.34 , pp. 5821-5825
    • Chaudhuri, M.1    Banerjee, G.2    Kumar, A.3    Sarkar, S.L.4
  • 6
    • 0024770333 scopus 로고
    • Dual-phase magnesia-zirconia ceramics with strength retention at elevated temperatures
    • Yuan T.C., Srinivasan G.V., Jue J.F., and Virkar A.V. Dual-phase magnesia-zirconia ceramics with strength retention at elevated temperatures. J. Mater. Sci. 24 11 (1989) 3855-3864
    • (1989) J. Mater. Sci. , vol.24 , Issue.11 , pp. 3855-3864
    • Yuan, T.C.1    Srinivasan, G.V.2    Jue, J.F.3    Virkar, A.V.4
  • 9
    • 34548846032 scopus 로고
    • 3 on properties of refractories
    • (in Chinese)
    • 3 on properties of refractories. Refractories 25 6 (1991) 352-358 (in Chinese)
    • (1991) Refractories , vol.25 , Issue.6 , pp. 352-358
    • Chen, Zh.1
  • 11
    • 33645136505 scopus 로고
    • Development of magnesia-zircon castable for steel ladle slag line
    • Hideo Y., Hitoshi N., et al. Development of magnesia-zircon castable for steel ladle slag line. Taikabutsu 45 8 (1993) 491-492
    • (1993) Taikabutsu , vol.45 , Issue.8 , pp. 491-492
    • Hideo, Y.1    Hitoshi, N.2
  • 13
    • 0034643155 scopus 로고    scopus 로고
    • Other catalytic properties
    • Centi G. Other catalytic properties. Catal. Today 56 (2000) 443-453
    • (2000) Catal. Today , vol.56 , pp. 443-453
    • Centi, G.1
  • 14
    • 0024613618 scopus 로고
    • 4, prepared at moderate temperature
    • 4, prepared at moderate temperature. Solid State Ionics 32-33 Part 1 (1989) 141-146
    • (1989) Solid State Ionics , vol.32-33 , Issue.PART 1 , pp. 141-146
    • Günter, J.R.1    Amberg, M.2
  • 17
    • 0002574198 scopus 로고    scopus 로고
    • 4, determined by high-temperature direct synthesis calorimetry.
    • 4, determined by high-temperature direct synthesis calorimetry. Thermochim. Acta 288 1-2 (1996) 53-61
    • (1996) Thermochim. Acta , vol.288 , Issue.1-2 , pp. 53-61
    • Guo, Q.1    Kleppa, O.J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.