Volumn 47, Issue 14, 2007, Pages 2091-2097

Surface and subsurface integrity in diamond grinding of optical glasses on Tetraform 'C'

Author keywords

Diamond grinding; ELID; Optical glass; Surface and subsurface integrity; Tetraform 'C'

Indexed keywords

ACOUSTIC EMISSIONS; ATOMIC FORCE MICROSCOPY; DIAMONDS; DYNAMOMETERS; GRINDING (MACHINING); PIEZOELECTRIC DEVICES; QUARTZ; SCANNING ELECTRON MICROSCOPY; STIFFNESS;

EID: 34548355106     PISSN: 08906955     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ijmachtools.2007.05.005     Document Type: Article
Times cited : (76)

References (14)
  • 1
    • 0026191119 scopus 로고
    • Subsurface damage mechanisms at high-speed ductile machining of optical glasses
    • Schinker M.G. Subsurface damage mechanisms at high-speed ductile machining of optical glasses. Precision Engineering 13 (1991) 208-218
    • (1991) Precision Engineering , vol.13 , pp. 208-218
    • Schinker, M.G.1
  • 2
    • 0029231067 scopus 로고
    • Analysis of mirror surface generation of hard and brittle materials by ELID grinding with superfine grain metallic bonded wheels
    • Ohmori H., and Nagagawa T. Analysis of mirror surface generation of hard and brittle materials by ELID grinding with superfine grain metallic bonded wheels. Annals of the CIRP 44 (1995) 287-290
    • (1995) Annals of the CIRP , vol.44 , pp. 287-290
    • Ohmori, H.1    Nagagawa, T.2
  • 4
    • 0030231992 scopus 로고    scopus 로고
    • Ductile regime mirror finish grinding of ceramics with electrolytic in-process dressing (ELID) grinding
    • Bandyopadhyay B.P., Ohmori H., and Tahahashi I. Ductile regime mirror finish grinding of ceramics with electrolytic in-process dressing (ELID) grinding. Materials and Manufacturing Processes 11 (1996) 789-801
    • (1996) Materials and Manufacturing Processes , vol.11 , pp. 789-801
    • Bandyopadhyay, B.P.1    Ohmori, H.2    Tahahashi, I.3
  • 8
    • 0030379722 scopus 로고    scopus 로고
    • Grinding mechanisms for ceramics
    • Malkin S., and Hwang T.W. Grinding mechanisms for ceramics. Annals of CIRP 45 (1996) 569-580
    • (1996) Annals of CIRP , vol.45 , pp. 569-580
    • Malkin, S.1    Hwang, T.W.2
  • 9
    • 34548363096 scopus 로고    scopus 로고
    • K.E. Puttick, M.R. Rudman, K.J. Smith, A. Franks, K. Lindsay, Single point diamond machining of glasses, Technical Report, University of Surrey, 1988.
  • 10
    • 0023457764 scopus 로고
    • Brittle fracture mechanisms in single point glass abrasion
    • Molly P., Schinker M.G., and Doell W. Brittle fracture mechanisms in single point glass abrasion. Proceedings of SPIE 802 (1987) 81-88
    • (1987) Proceedings of SPIE , vol.802 , pp. 81-88
    • Molly, P.1    Schinker, M.G.2    Doell, W.3
  • 12
    • 84979434138 scopus 로고
    • Hardness, Toughness and brittleness: an indentation analysis
    • Lawn B.R. Hardness, Toughness and brittleness: an indentation analysis. Journal of the American Ceramic Society 62 (1979) 347-349
    • (1979) Journal of the American Ceramic Society , vol.62 , pp. 347-349
    • Lawn, B.R.1
  • 13
    • 34548344484 scopus 로고    scopus 로고
    • T.G. Bifano, Ductile-regime grinding of brittle materials, Ph.D. Thesis, North Carolina State University, 1988.
  • 14
    • 0024750612 scopus 로고    scopus 로고
    • E. Brinksmeier, State of the art in non-destructive measurement of sub-surface material properties and damages, in: Proceedings of the Fifth International Precision Engineering Seminar, 18-22 September 1989, Monterey, USA, Precision Engineering 11 (1989) 211-224.