1
-
-
0028256905
-
Improving the delamination resistance of CFRP by stitching - A review
-
Dransfield K., Baillie C., and Mai Y.W. Improving the delamination resistance of CFRP by stitching - A review. Compos Sci Technol 50 (1994) 305-317
-
(1994)
Compos Sci Technol
, vol.50
, pp. 305-317
-
-
Dransfield, K.1
Baillie, C.2
Mai, Y.W.3
-
2
-
-
0037198011
-
An analytical delamination model for laminated plates including bridging effects
-
Greco F., Lonetti P., and Zinno R. An analytical delamination model for laminated plates including bridging effects. Int J Solids Struct 39 (2002) 2435-2463
-
(2002)
Int J Solids Struct
, vol.39
, pp. 2435-2463
-
-
Greco, F.1
Lonetti, P.2
Zinno, R.3
-
3
-
-
34548034532
-
A mechanistic approach to the properties of stitched laminates
-
Mouritz A.P., and Cox B.N. A mechanistic approach to the properties of stitched laminates. Compos A 21 (2000) 1-27
-
(2000)
Compos A
, vol.21
, pp. 1-27
-
-
Mouritz, A.P.1
Cox, B.N.2
-
4
-
-
0032096528
-
On the effects of stitching in CFRPs-I. Mode I delamination toughness
-
Dransfield K.A., Jain L.K., and Mai Y.W. On the effects of stitching in CFRPs-I. Mode I delamination toughness. Compos Sci Technol 58 (1998) 815-827
-
(1998)
Compos Sci Technol
, vol.58
, pp. 815-827
-
-
Dransfield, K.A.1
Jain, L.K.2
Mai, Y.W.3
-
5
-
-
0025747678
-
Fracture behavior of interleaved fiber-resin composites
-
Chen S.F., and Jang B.Z. Fracture behavior of interleaved fiber-resin composites. Compos Sci Technol 41 (1991) 77-97
-
(1991)
Compos Sci Technol
, vol.41
, pp. 77-97
-
-
Chen, S.F.1
Jang, B.Z.2
-
6
-
-
1242321197
-
Interlaminar fracture toughness of CF/PEI composites at elevated temperatures: roles of matrix toughness and fibre/matrix adhesion
-
Kim K., and Ye L. Interlaminar fracture toughness of CF/PEI composites at elevated temperatures: roles of matrix toughness and fibre/matrix adhesion. Compos A 35 (2004) 477-487
-
(2004)
Compos A
, vol.35
, pp. 477-487
-
-
Kim, K.1
Ye, L.2
-
7
-
-
0029288464
-
Approach to improving the toughness of TGMDA/DDS epoxy resin by blending with thermoplastic polymer powders
-
Pascal T., Bonneau J.L., Biolley N., Mercier R., and Sillion B. Approach to improving the toughness of TGMDA/DDS epoxy resin by blending with thermoplastic polymer powders. Polym Adv Technol 6 4 (1995) 219-229
-
(1995)
Polym Adv Technol
, vol.6
, Issue.4
, pp. 219-229
-
-
Pascal, T.1
Bonneau, J.L.2
Biolley, N.3
Mercier, R.4
Sillion, B.5
-
8
-
-
4444333046
-
Mechanism of crack bridging by composite and metallic rods
-
Cartié D.D.R., Cox B.N., and Fleck R. Mechanism of crack bridging by composite and metallic rods. Compos A Appl Sci Manuf 35 11 (2004) 1325-1336
-
(2004)
Compos A Appl Sci Manuf
, vol.35
, Issue.11
, pp. 1325-1336
-
-
Cartié, D.D.R.1
Cox, B.N.2
Fleck, R.3
-
9
-
-
0001897922
-
Fiber insertion process for improved damage tolerance in aircraft laminates
-
Freitas G., Magee C., Dardzinski P., and Fusco T. Fiber insertion process for improved damage tolerance in aircraft laminates. Int J Adv Mater 25 4 (1994) 36-43
-
(1994)
Int J Adv Mater
, vol.25
, Issue.4
, pp. 36-43
-
-
Freitas, G.1
Magee, C.2
Dardzinski, P.3
Fusco, T.4
-
10
-
-
33846226019
-
-
Allegri G, Zhanga X. On the delamination and debond suppression in structural joints by Z-fibre pinning. Compos A Appl Sci Manuf, in press, doi:10.1016/j.compositesa.2006.06.013.
-
-
-
-
11
-
-
6444234247
-
® pinning: Part I. Manufacture and fracture performance
-
® pinning: Part I. Manufacture and fracture performance. Compos A Appl Sci Manuf 36 1 (2005) 55-64
-
(2005)
Compos A Appl Sci Manuf
, vol.36
, Issue.1
, pp. 55-64
-
-
Ivana, K.P.1
Cartié, D.D.R.2
-
12
-
-
0038007603
-
Numerical study on the mode-I delamination toughness of Z-pinned laminates
-
Yan W., Liu H.Y., and Mai Y.W. Numerical study on the mode-I delamination toughness of Z-pinned laminates. Compos Sci Technol 63 (2003) 1481-1493
-
(2003)
Compos Sci Technol
, vol.63
, pp. 1481-1493
-
-
Yan, W.1
Liu, H.Y.2
Mai, Y.W.3
-
13
-
-
34548034069
-
-
Beaumont PWR, Riewald PG, Zweben C. Methods for improving the impact resistance of composite materials in foreign object impact damage. ASTM STP 568; 1974. p. 134-58.
-
-
-
-
14
-
-
0019707231
-
One-dimensional modeling of failure in laminated plates by delamination buckling
-
Chai H., Babcock C.D., and Knauss W.B. One-dimensional modeling of failure in laminated plates by delamination buckling. Int J Solids Struct 17 11 (1981) 1069-1083
-
(1981)
Int J Solids Struct
, vol.17
, Issue.11
, pp. 1069-1083
-
-
Chai, H.1
Babcock, C.D.2
Knauss, W.B.3
-
15
-
-
0022128707
-
Effect of delamination of axially loaded homogeneous laminated plates
-
Simitses G.J., Sallam S., and Yin W.L. Effect of delamination of axially loaded homogeneous laminated plates. AIAA J 23 9 (1985) 1437-1444
-
(1985)
AIAA J
, vol.23
, Issue.9
, pp. 1437-1444
-
-
Simitses, G.J.1
Sallam, S.2
Yin, W.L.3
-
16
-
-
0027540058
-
Layer-wise approach for the bifurcation problem in laminated composites with delaminations
-
Lee J., Gurdal Z., and Griffin O.H. Layer-wise approach for the bifurcation problem in laminated composites with delaminations. AIAA J 31 2 (1993) 331-338
-
(1993)
AIAA J
, vol.31
, Issue.2
, pp. 331-338
-
-
Lee, J.1
Gurdal, Z.2
Griffin, O.H.3
-
17
-
-
0027202952
-
Buckling of delaminated composites re-examined
-
Shu D., and Mai Y.W. Buckling of delaminated composites re-examined. Compos Sci Technol 47 1 (1993) 35-41
-
(1993)
Compos Sci Technol
, vol.47
, Issue.1
, pp. 35-41
-
-
Shu, D.1
Mai, Y.W.2
-
18
-
-
0032063907
-
Buckling of orthotropic beam-plates with multiple central delaminations
-
Haiying H., and Kardomateas G.A. Buckling of orthotropic beam-plates with multiple central delaminations. Int J Solids Struct 35 13 (1998) 1355-1362
-
(1998)
Int J Solids Struct
, vol.35
, Issue.13
, pp. 1355-1362
-
-
Haiying, H.1
Kardomateas, G.A.2
-
19
-
-
0032064640
-
Buckling of multiple delaminated beams
-
Shu D. Buckling of multiple delaminated beams. Int J Solids Struct 35 13 (1998) 1451-1465
-
(1998)
Int J Solids Struct
, vol.35
, Issue.13
, pp. 1451-1465
-
-
Shu, D.1
-
20
-
-
0035307405
-
Application of DQM as an effect solution tool for buckling response of delaminated composite plates
-
Moradi S., and Taheri F. Application of DQM as an effect solution tool for buckling response of delaminated composite plates. Compos Struct 51 4 (2001) 439-449
-
(2001)
Compos Struct
, vol.51
, Issue.4
, pp. 439-449
-
-
Moradi, S.1
Taheri, F.2
-
21
-
-
1842584596
-
Buckling of two-layer beams with an asymmetric delamination
-
Parlapalli M., and Shu D. Buckling of two-layer beams with an asymmetric delamination. Eng Struct 26 5 (2004) 651-658
-
(2004)
Eng Struct
, vol.26
, Issue.5
, pp. 651-658
-
-
Parlapalli, M.1
Shu, D.2
-
22
-
-
17044432989
-
Buckling analysis of tri-layer beams with overlapped delaminations
-
MSRao P., Hao S., and Shu D. Buckling analysis of tri-layer beams with overlapped delaminations. J Compos Mater 39 2 (2005) 109-125
-
(2005)
J Compos Mater
, vol.39
, Issue.2
, pp. 109-125
-
-
MSRao, P.1
Hao, S.2
Shu, D.3
-
23
-
-
0027147169
-
Delamination buckling with bridging
-
Shu D., and Mai Y.W. Delamination buckling with bridging. Compos Sci Technol 47 1 (1993) 25-33
-
(1993)
Compos Sci Technol
, vol.47
, Issue.1
, pp. 25-33
-
-
Shu, D.1
Mai, Y.W.2
-
24
-
-
0028563416
-
Delamination and buckling in 3D composites
-
Cox B.N. Delamination and buckling in 3D composites. J Compos Mater 28 12 (1994) 1114-1126
-
(1994)
J Compos Mater
, vol.28
, Issue.12
, pp. 1114-1126
-
-
Cox, B.N.1
-
25
-
-
0031650633
-
Crack bridging by through-thickness reinforcement in delaminating curved structures
-
He M., and Cox B.N. Crack bridging by through-thickness reinforcement in delaminating curved structures. Compos A Appl Sci Manuf 29 4 (1998) 377-393
-
(1998)
Compos A Appl Sci Manuf
, vol.29
, Issue.4
, pp. 377-393
-
-
He, M.1
Cox, B.N.2
-
26
-
-
0033317709
-
Local buckling of stitched composite laminate
-
Pan T.S., and Herrington P.D. Local buckling of stitched composite laminate. Compos B 30 8 (1999) 833-840
-
(1999)
Compos B
, vol.30
, Issue.8
, pp. 833-840
-
-
Pan, T.S.1
Herrington, P.D.2
-
27
-
-
18244379322
-
Initial post-buckling and growth of a circular delamination bridged by nonlinear fibers
-
Li S., Nie J., Qian J., Huang Y., and Hu Y. Initial post-buckling and growth of a circular delamination bridged by nonlinear fibers. J Appl Mech 67 4 (2000) 777-784
-
(2000)
J Appl Mech
, vol.67
, Issue.4
, pp. 777-784
-
-
Li, S.1
Nie, J.2
Qian, J.3
Huang, Y.4
Hu, Y.5
-
28
-
-
0035304422
-
Delamination buckling of stitched laminates
-
Gui L., and Li Z. Delamination buckling of stitched laminates. Compos Sci Technol 61 5 (2001) 629-636
-
(2001)
Compos Sci Technol
, vol.61
, Issue.5
, pp. 629-636
-
-
Gui, L.1
Li, Z.2
-
29
-
-
0036173779
-
The stabilizing effects of fiber bridges on delamination cracks
-
Daridon L., and Zidani K. The stabilizing effects of fiber bridges on delamination cracks. Compos Sci Technol 62 11 (2002) 83-90
-
(2002)
Compos Sci Technol
, vol.62
, Issue.11
, pp. 83-90
-
-
Daridon, L.1
Zidani, K.2
-
30
-
-
33748713615
-
Buckling analysis of two-layer delaminated beam with bridging
-
Parlapalli M., and Shu D. Buckling analysis of two-layer delaminated beam with bridging. Eur J Mech A - Solids 25 5 (2006) 834-853
-
(2006)
Eur J Mech A - Solids
, vol.25
, Issue.5
, pp. 834-853
-
-
Parlapalli, M.1
Shu, D.2
-
31
-
-
33749259271
-
Effects of bridging on buckling of tri-layer beams with separated delaminations
-
Parlapalli M., and Shu D. Effects of bridging on buckling of tri-layer beams with separated delaminations. AIAA J 44 9 (2006) 2108-2117
-
(2006)
AIAA J
, vol.44
, Issue.9
, pp. 2108-2117
-
-
Parlapalli, M.1
Shu, D.2
-
32
-
-
0031147960
-
Flexural and interlaminar shear strengths of stitched GRP laminates following repeated impacts
-
Mouritz A.P., Gallagher J., and Goodwin A.A. Flexural and interlaminar shear strengths of stitched GRP laminates following repeated impacts. Compos Sci Technol 57 5 (1997) 509-522
-
(1997)
Compos Sci Technol
, vol.57
, Issue.5
, pp. 509-522
-
-
Mouritz, A.P.1
Gallagher, J.2
Goodwin, A.A.3
-
33
-
-
34548012710
-
-
Standard test method for compressive properties of unidirectional or crossply fiber-resin composites, ASTM D204-93, American Society for Testing and Materials. West Conshohocken, Pa.1993.
-
-
-
|