메뉴 건너뛰기




Volumn 74, Issue 16, 2007, Pages 2535-2546

On internal cone cracks induced by conical indentation in brittle materials

Author keywords

Cone cracks; Finite element analysis; Instrumented indentation

Indexed keywords

COMPUTATIONAL GEOMETRY; COMPUTER SIMULATION; CRACKS; ELASTICITY; FINITE ELEMENT METHOD; FRACTURE TOUGHNESS; INDENTATION; PLASTICITY;

EID: 34547482093     PISSN: 00137944     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.engfracmech.2006.12.005     Document Type: Article
Times cited : (15)

References (32)
  • 1
    • 27744527765 scopus 로고    scopus 로고
    • Representative strain of indentation analysis
    • Ogasawara N., Chiba N., and Chen X. Representative strain of indentation analysis. J Mater Res 20 (2005) 2225-2234
    • (2005) J Mater Res , vol.20 , pp. 2225-2234
    • Ogasawara, N.1    Chiba, N.2    Chen, X.3
  • 2
    • 27344445466 scopus 로고    scopus 로고
    • Measuring the plastic properties of bulk materials by single indentation test
    • Ogasawara N., Chiba N., and Chen X. Measuring the plastic properties of bulk materials by single indentation test. Scripta Mater 54 (2006) 65-70
    • (2006) Scripta Mater , vol.54 , pp. 65-70
    • Ogasawara, N.1    Chiba, N.2    Chen, X.3
  • 3
    • 30844445808 scopus 로고    scopus 로고
    • On the determination of residual stress and mechanical properties by indentation
    • Chen X., Yan J., and Karlsson A.M. On the determination of residual stress and mechanical properties by indentation. Mater Sci Eng: A 416 (2006) 139-149
    • (2006) Mater Sci Eng: A , vol.416 , pp. 139-149
    • Chen, X.1    Yan, J.2    Karlsson, A.M.3
  • 4
    • 33646536355 scopus 로고    scopus 로고
    • Determination of uniaxial residual stress and mechanical properties by instrumented indentation
    • Zhao M., Chen X., Yan J., and Karlsson A.M. Determination of uniaxial residual stress and mechanical properties by instrumented indentation. Acta Mater 54 (2006) 2823-2832
    • (2006) Acta Mater , vol.54 , pp. 2823-2832
    • Zhao, M.1    Chen, X.2    Yan, J.3    Karlsson, A.M.4
  • 5
    • 34547419293 scopus 로고    scopus 로고
    • Yan J, Karlsson AM, Chen X. Determining plastic properties of a bulk material with residual stress by using conical indentation. Int J Solids Struct, in press.
  • 6
    • 0025418269 scopus 로고
    • Direct observation and analysis of indentation cracking in glasses and ceramics
    • Cook R.F., and Pharr G.M. Direct observation and analysis of indentation cracking in glasses and ceramics. J Am Ceram Soc 73 (1990) 787-817
    • (1990) J Am Ceram Soc , vol.73 , pp. 787-817
    • Cook, R.F.1    Pharr, G.M.2
  • 7
    • 0032137856 scopus 로고    scopus 로고
    • Indentation of ceramics with spheres: a century of Hertz
    • Lawn B.R. Indentation of ceramics with spheres: a century of Hertz. J Am Ceram Soc 81 (1998) 1977-1985
    • (1998) J Am Ceram Soc , vol.81 , pp. 1977-1985
    • Lawn, B.R.1
  • 8
    • 0035811672 scopus 로고    scopus 로고
    • An elastic-plastic-cracking model for finite element analysis of indentation crack in brittle materials
    • Zhang W., and Subhash G. An elastic-plastic-cracking model for finite element analysis of indentation crack in brittle materials. Int J Solids Struct 38 (2001) 5893-5913
    • (2001) Int J Solids Struct , vol.38 , pp. 5893-5913
    • Zhang, W.1    Subhash, G.2
  • 9
    • 0037440260 scopus 로고    scopus 로고
    • Finite element analysis of Vickers indentation crack processes in brittle solids using elements exhibiting cohesive post-failure behavior
    • Muchtar A., Lim L.C., and Lee K.H. Finite element analysis of Vickers indentation crack processes in brittle solids using elements exhibiting cohesive post-failure behavior. J Mater Sci 38 (2003) 235-243
    • (2003) J Mater Sci , vol.38 , pp. 235-243
    • Muchtar, A.1    Lim, L.C.2    Lee, K.H.3
  • 10
    • 27644525527 scopus 로고    scopus 로고
    • The mechanics of indentation induced lateral cracking
    • Chen X., Hutchinson J.W., and Evans A.G. The mechanics of indentation induced lateral cracking. J Am Ceram Soc 88 (2005) 1233-1238
    • (2005) J Am Ceram Soc , vol.88 , pp. 1233-1238
    • Chen, X.1    Hutchinson, J.W.2    Evans, A.G.3
  • 11
    • 84987335986 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements
    • Anstis G.R., Chantikul P., Lawn B.R., and Marshall D.B. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements. J Am Ceram Soc 64 (1981) 533-545
    • (1981) J Am Ceram Soc , vol.64 , pp. 533-545
    • Anstis, G.R.1    Chantikul, P.2    Lawn, B.R.3    Marshall, D.B.4
  • 12
    • 0019058952 scopus 로고
    • Elastic-plastic indentation damage in ceramics - the median-radial crack system
    • Lawn B., Evans A., and Marshall D. Elastic-plastic indentation damage in ceramics - the median-radial crack system. J Am Ceram Soc 63 (1980) 574-581
    • (1980) J Am Ceram Soc , vol.63 , pp. 574-581
    • Lawn, B.1    Evans, A.2    Marshall, D.3
  • 13
    • 0016648164 scopus 로고
    • Equilibrium penny-like cracks in indentation fracture
    • Lawn B.R., and Fuller E.R. Equilibrium penny-like cracks in indentation fracture. J Mater Sci 10 (1975) 2016-2020
    • (1975) J Mater Sci , vol.10 , pp. 2016-2020
    • Lawn, B.R.1    Fuller, E.R.2
  • 14
    • 0017555307 scopus 로고
    • A model for crack initiation in elastic/plastic indentation fields
    • Lawn B.R., and Evans A.G. A model for crack initiation in elastic/plastic indentation fields. J Mater Sci 12 (1977) 2195-2201
    • (1977) J Mater Sci , vol.12 , pp. 2195-2201
    • Lawn, B.R.1    Evans, A.G.2
  • 15
    • 0020704350 scopus 로고
    • Controlled surface flaws in ceramics: a comparison of Knoop and Vickers indentation
    • Marshall D.B. Controlled surface flaws in ceramics: a comparison of Knoop and Vickers indentation. J Am Ceram Soc 66 (1983) 127-133
    • (1983) J Am Ceram Soc , vol.66 , pp. 127-133
    • Marshall, D.B.1
  • 16
    • 0000738741 scopus 로고
    • Fracture toughness determinations by indentation
    • Evans A., and Charles E. Fracture toughness determinations by indentation. J Am Ceram Soc 59 (1976) 371-372
    • (1976) J Am Ceram Soc , vol.59 , pp. 371-372
    • Evans, A.1    Charles, E.2
  • 17
    • 0020751889 scopus 로고
    • A fracture mechanics analysis of indentation-induced Palmqvist cracks in ceramics
    • Niihara K. A fracture mechanics analysis of indentation-induced Palmqvist cracks in ceramics. J Mater Sci Lett 2 (1983) 221-223
    • (1983) J Mater Sci Lett , vol.2 , pp. 221-223
    • Niihara, K.1
  • 18
    • 0001554960 scopus 로고
    • Indentation microfracture in the Palmqvist crack regime: implications for fracture toughness evaluation by the indentation method
    • Lankford J. Indentation microfracture in the Palmqvist crack regime: implications for fracture toughness evaluation by the indentation method. J Mater Sci Lett 1 (1982) 493-495
    • (1982) J Mater Sci Lett , vol.1 , pp. 493-495
    • Lankford, J.1
  • 20
    • 23844442534 scopus 로고    scopus 로고
    • Hydraulically pumped cone fracture in brittle solids
    • Chai H., and Lawn B.R. Hydraulically pumped cone fracture in brittle solids. Acta Mater 53 (2005) 4237-4244
    • (2005) Acta Mater , vol.53 , pp. 4237-4244
    • Chai, H.1    Lawn, B.R.2
  • 21
    • 33645768421 scopus 로고    scopus 로고
    • Scaling laws governing the erosion and impact resistance of thermal barrier coatings
    • Evans A.G., Fleck N.A., Faulhaber S., Vermaak N., Maloney M., and Darolia R. Scaling laws governing the erosion and impact resistance of thermal barrier coatings. Wear 260 (2006) 886-894
    • (2006) Wear , vol.260 , pp. 886-894
    • Evans, A.G.1    Fleck, N.A.2    Faulhaber, S.3    Vermaak, N.4    Maloney, M.5    Darolia, R.6
  • 22
    • 1642479006 scopus 로고    scopus 로고
    • Simulation of the high temperature impression of thermal barrier coatings with columnar microstructure
    • Chen X., Hutchinson J.W., and Evans A.G. Simulation of the high temperature impression of thermal barrier coatings with columnar microstructure. Acta Mater 52 (2004) 565-571
    • (2004) Acta Mater , vol.52 , pp. 565-571
    • Chen, X.1    Hutchinson, J.W.2    Evans, A.G.3
  • 23
    • 0026940305 scopus 로고
    • The Hertzian stress-field and formation of cone cracks. 1. Theoretical approach
    • Zeng K., Breder K., and Rowcliffe D.J. The Hertzian stress-field and formation of cone cracks. 1. Theoretical approach. Acta Metall Mater 40 (1992) 2595-2600
    • (1992) Acta Metall Mater , vol.40 , pp. 2595-2600
    • Zeng, K.1    Breder, K.2    Rowcliffe, D.J.3
  • 24
    • 0026939155 scopus 로고
    • The Hertzian stress-field and formation of cone cracks. 2. Determination of fracture-toughness
    • Zeng K., Breder K., and Rowcliffe D.J. The Hertzian stress-field and formation of cone cracks. 2. Determination of fracture-toughness. Acta Metall Mater 40 (1992) 2601-2605
    • (1992) Acta Metall Mater , vol.40 , pp. 2601-2605
    • Zeng, K.1    Breder, K.2    Rowcliffe, D.J.3
  • 25
    • 0032805719 scopus 로고    scopus 로고
    • Simulation of contact-induced fracture
    • Bush M.B. Simulation of contact-induced fracture. Engng Anal Bound Elem 23 (1999) 59-66
    • (1999) Engng Anal Bound Elem , vol.23 , pp. 59-66
    • Bush, M.B.1
  • 26
    • 0037399881 scopus 로고    scopus 로고
    • An automated incremental finite element study of Hertzian cone crack growth
    • Kocer C. An automated incremental finite element study of Hertzian cone crack growth. Finite Elem Anal Des 39 (2003) 639-660
    • (2003) Finite Elem Anal Des , vol.39 , pp. 639-660
    • Kocer, C.1
  • 27
    • 4944262806 scopus 로고    scopus 로고
    • The indentation fracture toughness (K-C) and its parameters: the case of silica-rich glasses
    • Deriano S., Jarry A., Rouxel T., Sangleboeuf J., and Hampshire S. The indentation fracture toughness (K-C) and its parameters: the case of silica-rich glasses. J Non-Cryst Solids 344 (2004) 44-50
    • (2004) J Non-Cryst Solids , vol.344 , pp. 44-50
    • Deriano, S.1    Jarry, A.2    Rouxel, T.3    Sangleboeuf, J.4    Hampshire, S.5
  • 28
    • 0842329841 scopus 로고    scopus 로고
    • Elastic constants, Vickers hardness, and fracture toughness of fluorrichterite-based glass-ceramics
    • Denry I., and Holloway J. Elastic constants, Vickers hardness, and fracture toughness of fluorrichterite-based glass-ceramics. Dental Mater 20 (2004) 213-219
    • (2004) Dental Mater , vol.20 , pp. 213-219
    • Denry, I.1    Holloway, J.2
  • 29
    • 4944238551 scopus 로고    scopus 로고
    • Soda-borosilicate glass: normal or anomalous behavior under Vickers indentation
    • Bertoldi M., and Sglavo V.M. Soda-borosilicate glass: normal or anomalous behavior under Vickers indentation. J Non-Cryst Solids 344 (2004) 51-59
    • (2004) J Non-Cryst Solids , vol.344 , pp. 51-59
    • Bertoldi, M.1    Sglavo, V.M.2
  • 30
    • 0033276986 scopus 로고    scopus 로고
    • Pyramidal indentation load-depth curve of viscoelastic materials
    • Shimizu S., Yanagimoto T., and Sakai M. Pyramidal indentation load-depth curve of viscoelastic materials. J Mater Res 14 (1999) 4075-4086
    • (1999) J Mater Res , vol.14 , pp. 4075-4086
    • Shimizu, S.1    Yanagimoto, T.2    Sakai, M.3
  • 31
    • 34249686936 scopus 로고    scopus 로고
    • Interfacial fracture toughness measurement of thick ceramic coatings by indentation
    • Bartsch M., Mircea I., Suffner J., and Baufeld B. Interfacial fracture toughness measurement of thick ceramic coatings by indentation. Fractography Adv Ceram Ii 290 (2005) 183-190
    • (2005) Fractography Adv Ceram Ii , vol.290 , pp. 183-190
    • Bartsch, M.1    Mircea, I.2    Suffner, J.3    Baufeld, B.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.