Fiber damage and high temperature tensile properties of Al2O3 fiber reinforced NiAl-matrix composites with and without hBN-interlayer

Author keywords

Al2O3 fiber; Fiber damage; Intermetallic composites; Tensile strength; Thermal residual stress

Indexed keywords

ALUMINUM; BONDING; COMPRESSIVE STRESS; FIBER REINFORCED METALS; INTERMETALLICS; RESIDUAL STRESSES; TENSILE STRENGTH; THERMAL EXPANSION; THERMAL STRESS; VOLUME FRACTION;