The construction of the two-dimensional array of the fibrous objects from the mixture of RFDF16-PEG and RFDF16 at air/water interface

Author keywords

[No Author keywords available]

Indexed keywords


EID: 34248554167     PISSN: 03667022     EISSN: None     Source Type: Journal    
DOI: 10.1246/cl.2007.562     Document Type: Article
Times cited : (5)

References (13)
  • 13
    • 34248597219 scopus 로고    scopus 로고
    • The monolayer was prepared by spreading a solution of the peptide in benzene/2,2,2-trifluoroethanol (6:4 v/v) at a concentration of approximately 0.1 mg/mL through a microsyringe onto the deionized water surface. After evaporation of organic solvents, the monolayer was compressed at a speed of 5 mm/min, and the surface pressure was measured by Wilhelmy plate. The monolayer was transferred onto the mica substrate in vertical method at a speed of 5 mm/min.
    • The monolayer was prepared by spreading a solution of the peptide in benzene/2,2,2-trifluoroethanol (6:4 v/v) at a concentration of approximately 0.1 mg/mL through a microsyringe onto the deionized water surface. After evaporation of organic solvents, the monolayer was compressed at a speed of 5 mm/min, and the surface pressure was measured by Wilhelmy plate. The monolayer was transferred onto the mica substrate in vertical method at a speed of 5 mm/min.