메뉴 건너뛰기




Volumn 22, Issue 1, 2007, Pages 206-216

Hot corrosion behavior of Pt-Ir modified aluminide coatings on the nickel-base single crystal superalloy TMS-82+

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINUM COMPOUNDS; CORROSION RESISTANCE; MAGNETRON SPUTTERING; NICKEL ALLOYS; PHASE TRANSITIONS; PLATINUM ALLOYS; SUPERALLOYS;

EID: 33847653644     PISSN: 08842914     EISSN: None     Source Type: Journal    
DOI: 10.1557/jmr.2007.0022     Document Type: Article
Times cited : (20)

References (36)
  • 1
    • 0028422351 scopus 로고
    • The cyclic-oxidation behavior of several nickel-base single-crystal superalloys without and with coatings
    • M. Gobel, A. Rahmel, and M. Schutze: The cyclic-oxidation behavior of several nickel-base single-crystal superalloys without and with coatings. Oxid. Met. 41, 271 (1994).
    • (1994) Oxid. Met. , vol.41 , pp. 271
    • Gobel, M.1    Rahmel, A.2    Schutze, M.3
  • 2
    • 0028450340 scopus 로고
    • Effects of pretreatments on structure and oxidation behaviour of d.c.-sputtered platinum aluminide coatings
    • J.H. Sun, H.C. Jang, and E. Chang: Effects of pretreatments on structure and oxidation behaviour of d.c.-sputtered platinum aluminide coatings. Surf. Coat. Technol. 64, 195 (1994).
    • (1994) Surf. Coat. Technol. , vol.64 , pp. 195
    • Sun, J.H.1    Jang, H.C.2    Chang, E.3
  • 3
    • 1842715096 scopus 로고    scopus 로고
    • Microstructure of Pt-modified aluminide coatings on Ni-based superalloys
    • J. Benoist, K.F. Badawi, A. Malié, and C. Ramade: Microstructure of Pt-modified aluminide coatings on Ni-based superalloys. Surf. Coat. Technol. 182, 14 (2004).
    • (2004) Surf. Coat. Technol. , vol.182 , pp. 14
    • Benoist, J.1    Badawi, K.F.2    Malié, A.3    Ramade, C.4
  • 6
    • 0001192637 scopus 로고
    • Oxidation behavior of simple and Pt-modified aluminide coatings on IN738 at 1100 °C
    • Y. Niu, W. Wu, D. Boone, J. Smith, J. Zhang, and C. Chen: Oxidation behavior of simple and Pt-modified aluminide coatings on IN738 at 1100 °C. J. Phys. E 3, 511 (1993).
    • (1993) J. Phys. E , vol.3 , pp. 511
    • Niu, Y.1    Wu, W.2    Boone, D.3    Smith, J.4    Zhang, J.5    Chen, C.6
  • 7
    • 0016917216 scopus 로고
    • Use of platinum and rhodium to improve oxide adherence on Ni-8Cr-6Al alloys
    • E.J. Felten: Use of platinum and rhodium to improve oxide adherence on Ni-8Cr-6Al alloys. Oxid. Met. 10, 23 (1976).
    • (1976) Oxid. Met. , vol.10 , pp. 23
    • Felten, E.J.1
  • 9
    • 0031164991 scopus 로고    scopus 로고
    • Degradation of the platinum aluminide coating on CMSX4 at 1100 °C
    • J.H. Chen and J.A. Little: Degradation of the platinum aluminide coating on CMSX4 at 1100 °C. Surf. Coat. Technol. 92, 69 (1997).
    • (1997) Surf. Coat. Technol. , vol.92 , pp. 69
    • Chen, J.H.1    Little, J.A.2
  • 10
    • 0035392082 scopus 로고    scopus 로고
    • Effects of Pt incorporation on the isothermal oxidation behavior of chemical vapor deposition aluminide coatings
    • Y. Zhang, J.A. Haynes, W.Y. Lee, I.G. Wright, B.A. Pint, K.M. Cooley, and P.K. Liaw: Effects of Pt incorporation on the isothermal oxidation behavior of chemical vapor deposition aluminide coatings. Metall. Mater. Trans. A 32, 1727 (2001).
    • (2001) Metall. Mater. Trans. A , vol.32 , pp. 1727
    • Zhang, Y.1    Haynes, J.A.2    Lee, W.Y.3    Wright, I.G.4    Pint, B.A.5    Cooley, K.M.6    Liaw, P.K.7
  • 11
    • 0001610733 scopus 로고
    • Surface instability of platinum modified aluminide coatings during 1100 °C cyclic testing
    • P. Deb, D.H. Boone, and T.F. Manley: Surface instability of platinum modified aluminide coatings during 1100 °C cyclic testing. J. Vac. Sci. Technol., A 5, 3366 (1987).
    • (1987) J. Vac. Sci. Technol., A , vol.5 , pp. 3366
    • Deb, P.1    Boone, D.H.2    Manley, T.F.3
  • 12
    • 0034315645 scopus 로고    scopus 로고
    • Manufacturing, structure and high temperature corrosion of palladium-modified aluminide coatings on nickel-base superalloy M38
    • D. He, H. Guan, X. Sun, and X. Jiang: Manufacturing, structure and high temperature corrosion of palladium-modified aluminide coatings on nickel-base superalloy M38. Thin Solid Films 376, 144 (2000).
    • (2000) Thin Solid Films , vol.376 , pp. 144
    • He, D.1    Guan, H.2    Sun, X.3    Jiang, X.4
  • 13
    • 33847641098 scopus 로고
    • U.S. Patent No. 4880614, 14 Nov
    • T.E. Strangman and P.A. Solfest: U.S. Patent No. 4880614, 14 Nov 1989.
    • (1989)
    • Strangman, T.E.1    Solfest, P.A.2
  • 14
    • 9144237674 scopus 로고    scopus 로고
    • Process dependence of Ir-based bond coatings
    • H. Murakami, T. Yano, and S. Sodeoka: Process dependence of Ir-based bond coatings. Mater. Trans. 45, 2886 (2004).
    • (2004) Mater. Trans. , vol.45 , pp. 2886
    • Murakami, H.1    Yano, T.2    Sodeoka, S.3
  • 15
    • 0034262914 scopus 로고    scopus 로고
    • Potential of IrAl base alloys as ultrahigh-temperature smart coatings
    • H. Hosoda, S. Miyazaki, and S. Hanada: Potential of IrAl base alloys as ultrahigh-temperature smart coatings. Intermetallics 8, 1081 (2000).
    • (2000) Intermetallics , vol.8 , pp. 1081
    • Hosoda, H.1    Miyazaki, S.2    Hanada, S.3
  • 16
    • 0038527329 scopus 로고    scopus 로고
    • Interdiffusion of the platinum-group metals in nickel at elevated temperatures
    • M.S.A. Karunaratne and R.C. Reed: Interdiffusion of the platinum-group metals in nickel at elevated temperatures. Acta Mater. 51, 2905 (2003).
    • (2003) Acta Mater. , vol.51 , pp. 2905
    • Karunaratne, M.S.A.1    Reed, R.C.2
  • 17
    • 0024898332 scopus 로고
    • The oxidation of iridium-aluminum and iridium-hafnium intermetallics at temperatures above 1550 °C
    • K.N. Lee and W.L. Worrell: The oxidation of iridium-aluminum and iridium-hafnium intermetallics at temperatures above 1550 °C. Oxid. Met. 32, 357 (1989).
    • (1989) Oxid. Met. , vol.32 , pp. 357
    • Lee, K.N.1    Worrell, W.L.2
  • 18
    • 0025385359 scopus 로고
    • 3 layers during high-temperature oxidation of IrAl alloys
    • 3 layers during high-temperature oxidation of IrAl alloys. J. Mater. Res. 5, 378 (1990).
    • (1990) J. Mater. Res. , vol.5 , pp. 378
    • Chou, T.C.1
  • 19
    • 0036828988 scopus 로고    scopus 로고
    • Solid-solution hardening of Ir by Pt and Ni
    • Y. Yamabe-Mitarai and H. Aoki: Solid-solution hardening of Ir by Pt and Ni. Mater. Lett. 56, 781 (2002).
    • (2002) Mater. Lett. , vol.56 , pp. 781
    • Yamabe-Mitarai, Y.1    Aoki, H.2
  • 21
    • 29044432522 scopus 로고    scopus 로고
    • Characterization of electroplated platinum-iridium alloys on the nickel-base single crystal superalloy
    • Y.N. Wu, A. Suzuki, H. Murakami, and S. Kuroda: Characterization of electroplated platinum-iridium alloys on the nickel-base single crystal superalloy. Mater. Trans. 46, 2176 (2005).
    • (2005) Mater. Trans. , vol.46 , pp. 2176
    • Wu, Y.N.1    Suzuki, A.2    Murakami, H.3    Kuroda, S.4
  • 22
    • 26944465754 scopus 로고    scopus 로고
    • Microstructual characterization of sputtered Pt-Ir coatings on Ni-base single crystal superalloy
    • A. Suzuki, M. Harada, Y.N. Wu, and H. Murakami: Microstructual characterization of sputtered Pt-Ir coatings on Ni-base single crystal superalloy. Mater. Trans. 46, 1760 (2005).
    • (2005) Mater. Trans. , vol.46 , pp. 1760
    • Suzuki, A.1    Harada, M.2    Wu, Y.N.3    Murakami, H.4
  • 23
    • 0033620310 scopus 로고    scopus 로고
    • An assessment of the oxidation resistance of an iridium and an iridium /platinum low-activity aluminide/MarM002 system at 1100 °C
    • G. Fisher, P.K. Datta, and J.S. Burnell-Gray: An assessment of the oxidation resistance of an iridium and an iridium/platinum low-activity aluminide/MarM002 system at 1100 °C. Surf. Coat. Technol. 113, 259 (1999).
    • (1999) Surf. Coat. Technol. , vol.113 , pp. 259
    • Fisher, G.1    Datta, P.K.2    Burnell-Gray, J.S.3
  • 24
    • 0242468704 scopus 로고    scopus 로고
    • Cyclic oxidation behavior of iridium-modified aluminide coatings for nickel-base single crystal superalloy TMS-75
    • F. Wu, H. Murakami, and H. Harada: Cyclic oxidation behavior of iridium-modified aluminide coatings for nickel-base single crystal superalloy TMS-75. Mater. Trans. 44, 1675 (2003).
    • (2003) Mater. Trans. , vol.44 , pp. 1675
    • Wu, F.1    Murakami, H.2    Harada, H.3
  • 25
    • 3543117309 scopus 로고    scopus 로고
    • A comparative study of cyclic oxidized Ir aluminide and aluminized nickel base single crystal superalloy
    • P. Kuppusami and H. Murakami: A comparative study of cyclic oxidized Ir aluminide and aluminized nickel base single crystal superalloy. Surf. Coat. Technol. 186, 377 (2004).
    • (2004) Surf. Coat. Technol. , vol.186 , pp. 377
    • Kuppusami, P.1    Murakami, H.2
  • 27
    • 0032689702 scopus 로고    scopus 로고
    • 4 and NaCl environments
    • 4 and NaCl environments. Oxid. Met. 51, 353 (1999).
    • (1999) Oxid. Met. , vol.51 , pp. 353
    • Gurrappa, I.1
  • 28
    • 0015574214 scopus 로고
    • Mechanisms for the hot corrosion of nickel-base alloys
    • J.A. Goebel, F.S. Pettit, and G.W. Goward: Mechanisms for the hot corrosion of nickel-base alloys. Metall. Trans. 4, 261 (1973).
    • (1973) Metall. Trans. , vol.4 , pp. 261
    • Goebel, J.A.1    Pettit, F.S.2    Goward, G.W.3
  • 29
    • 0034245770 scopus 로고    scopus 로고
    • Surface rumpling of a (Ni, Pt)Al bond coat induced by cyclic oxidation
    • V.K. Tolpygo and D.R. Clarke: Surface rumpling of a (Ni, Pt)Al bond coat induced by cyclic oxidation. Acta Mater. 48, 3283 (2000).
    • (2000) Acta Mater. , vol.48 , pp. 3283
    • Tolpygo, V.K.1    Clarke, D.R.2
  • 31
    • 0022753747 scopus 로고
    • Vanadic and chloride attack of superalloys
    • P. Hancock: Vanadic and chloride attack of superalloys. Mater. Sci. Technol. 3, 536 (1987).
    • (1987) Mater. Sci. Technol. , vol.3 , pp. 536
    • Hancock, P.1
  • 32
    • 0021474911 scopus 로고
    • 4-induced hot corrosion resistance of aluminum diffusion coatings
    • 4-induced hot corrosion resistance of aluminum diffusion coatings. Oxid. Met. 22, 59 (1984).
    • (1984) Oxid. Met. , vol.22 , pp. 59
    • Wu, W.T.1    Rahmel, A.2    Schrorr, M.3
  • 33
    • 84957224316 scopus 로고
    • Platinum aluminide coating structural effects on hot corrosion resistance at 900 °C
    • P. Deb and D.H. Boone: Platinum aluminide coating structural effects on hot corrosion resistance at 900 °C. J. Vac. Sci. Technol., A 3, 2578 (1985).
    • (1985) J. Vac. Sci. Technol., A , vol.3 , pp. 2578
    • Deb, P.1    Boone, D.H.2
  • 35
    • 8644259345 scopus 로고    scopus 로고
    • Effects of platinum on the interdiffusion and oxidation behavior of Ni-Al-based alloys
    • B. Gleeson, W. Wang, S. Hayashi, and D. Sordelet: Effects of platinum on the interdiffusion and oxidation behavior of Ni-Al-based alloys. Mater. Sci. Forum 461-464, 213 (2004).
    • (2004) Mater. Sci. Forum , vol.461-464 , pp. 213
    • Gleeson, B.1    Wang, W.2    Hayashi, S.3    Sordelet, D.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.