메뉴 건너뛰기




Volumn 27, Issue 7, 2007, Pages 2705-2713

High temperature water vapour corrosion of rare earth disilicates (Y,Yb,Lu)2Si2O7 in the presence of Al(OH)3 impurities

Author keywords

Corrosion; Environmental barrier coating; Impurities; Silicate; SiO2

Indexed keywords

COATINGS; CORROSION; CRACK INITIATION; KINETIC THEORY; SILICATES; SOLID SOLUTIONS;

EID: 33846701657     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2006.09.013     Document Type: Article
Times cited : (165)

References (32)
  • 4
    • 31844456154 scopus 로고    scopus 로고
    • Klemm, H., Fritsch, M. and Schenk, B., Corrosion of ceramic materials in hot gas environment, Ceram. Eng. Sci. Proc. 25 (4) 463-468.
  • 6
    • 0036386687 scopus 로고    scopus 로고
    • Corrosion of silicon nitride materials in gas turbine environment
    • Klemm H. Corrosion of silicon nitride materials in gas turbine environment. J. Eur. Ceram. Soc. 22 (2002) 2735-2740
    • (2002) J. Eur. Ceram. Soc. , vol.22 , pp. 2735-2740
    • Klemm, H.1
  • 8
    • 0041328372 scopus 로고    scopus 로고
    • Paralinear oxidation of silicon nitride in a water-vapor/oxygen environment
    • Fox D.S., Opila E.J., Nguyen Q.N., Humphrey D.L., and Lewton S.M. Paralinear oxidation of silicon nitride in a water-vapor/oxygen environment. J. Am. Ceram. Soc. 86 8 (2003) 1256-1261
    • (2003) J. Am. Ceram. Soc. , vol.86 , Issue.8 , pp. 1256-1261
    • Fox, D.S.1    Opila, E.J.2    Nguyen, Q.N.3    Humphrey, D.L.4    Lewton, S.M.5
  • 9
    • 0030868046 scopus 로고    scopus 로고
    • Paralinear oxidation of CVD SiC in water vapor
    • Opila E.J., and Hann Jr. R.E. Paralinear oxidation of CVD SiC in water vapor. J. Am. Ceram. Soc. 80 1 (1997) 197-205
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.1 , pp. 197-205
    • Opila, E.J.1    Hann Jr., R.E.2
  • 11
    • 33846685874 scopus 로고    scopus 로고
    • Yuri, I. and Hisamatsu, T. Recession rate prediction for ceramic materials in combustion gas flow. in ASME TURBO EXPO 2003. GT2003-38886, 10 pp.
  • 12
    • 10244278084 scopus 로고    scopus 로고
    • 7 in combustion gas flow at high temperature and high speed. in ASME Turbo Expo 2004. 2004. GT2004-54277, 6 pp.
  • 13
    • 0033726725 scopus 로고    scopus 로고
    • Yttrium silicate coatings for oxidation protection of carbon-silicon carbide composites
    • Aparacio M., and Durán A. Yttrium silicate coatings for oxidation protection of carbon-silicon carbide composites. J. Am. Ceram. Soc. 83 6 (2000) 1351-1355
    • (2000) J. Am. Ceram. Soc. , vol.83 , Issue.6 , pp. 1351-1355
    • Aparacio, M.1    Durán, A.2
  • 14
    • 0036607724 scopus 로고    scopus 로고
    • Development of a self-forming ytterbium silicate skin on silicon nitride by controlled oxidation
    • Lee S.K., and Readey M.J. Development of a self-forming ytterbium silicate skin on silicon nitride by controlled oxidation. J. Am. Ceram. Soc. 85 6 (2002) 1435-1440
    • (2002) J. Am. Ceram. Soc. , vol.85 , Issue.6 , pp. 1435-1440
    • Lee, S.K.1    Readey, M.J.2
  • 15
    • 33846661726 scopus 로고    scopus 로고
    • Weidenmann, K.A., Oxidationsverhalten flüssigphasenverdichteter Nichtoxidkeramiken an feuchter Atmosphäre, in Institut f. Nichtmetallische Anorganische Materialien. 2003. Diploma Thesis, Universität Stuttgart, Stuttgart, p. 97.
  • 16
    • 0036384568 scopus 로고    scopus 로고
    • Accelerated oxidation of SiC CMC's by water vapor and protection via environmental barrier coating approach
    • Eaton H.E., and Linsey G.D. Accelerated oxidation of SiC CMC's by water vapor and protection via environmental barrier coating approach. J. Eur. Ceram. Soc. 22 (2002) 2741-2747
    • (2002) J. Eur. Ceram. Soc. , vol.22 , pp. 2741-2747
    • Eaton, H.E.1    Linsey, G.D.2
  • 17
    • 2542616886 scopus 로고    scopus 로고
    • Preparation and the hydro thermal corrosion resistance of silicon nitride with a Lu-Si-O EBC layer at high temperature
    • Ueno S., Jayaseelan D.D., Ohji T., Kondo N., and Kanzaki S. Preparation and the hydro thermal corrosion resistance of silicon nitride with a Lu-Si-O EBC layer at high temperature. J. Ceram. Process. Res. 4 4 (2003) 214-216
    • (2003) J. Ceram. Process. Res. , vol.4 , Issue.4 , pp. 214-216
    • Ueno, S.1    Jayaseelan, D.D.2    Ohji, T.3    Kondo, N.4    Kanzaki, S.5
  • 18
    • 33846651936 scopus 로고    scopus 로고
    • Ueno, S., Kondo, N., Jayaseelan, D.D., Ohji, T. and Kanzaki, S. High temperature hydro corrosion resistance of silica based oxide ceramics. in ASME TURBO EXPO 2003. 2003. GT2003-38878, 8 pp.
  • 21
    • 33846697656 scopus 로고    scopus 로고
    • Maier, N., Synthese von Seltenerd-Sisilikaten und deren Korrosionsverhalten an strömender feuchter Atmosphäre, Diploma Thesis, Applied Mineralogy. 2005. University Tuebingen, Tuebingen, 257 pp.
  • 22
    • 33747110299 scopus 로고    scopus 로고
    • Formation and stability of Gd, Y, Yb and Lu disilicates and their solid solutions
    • Maier N., Rixecker G., and Nickel K.G. Formation and stability of Gd, Y, Yb and Lu disilicates and their solid solutions. J. Solid State Chem. 179 (2006) 1630-1635
    • (2006) J. Solid State Chem. , vol.179 , pp. 1630-1635
    • Maier, N.1    Rixecker, G.2    Nickel, K.G.3
  • 23
    • 5444237664 scopus 로고    scopus 로고
    • Alumina volatility in water vapor at elevated temperatures
    • Opila E.J., and Myers D.L. Alumina volatility in water vapor at elevated temperatures. J Am Ceram Soc 87 9 (2004) 1701-1705
    • (2004) J Am Ceram Soc , vol.87 , Issue.9 , pp. 1701-1705
    • Opila, E.J.1    Myers, D.L.2
  • 24
    • 0028403925 scopus 로고
    • Oxidation kinetics of chemically vapor-deposited silicon carbide in wet oxygen
    • Opila E.J. Oxidation kinetics of chemically vapor-deposited silicon carbide in wet oxygen. J. Am. Ceram. Soc. 77 3 (1994) 730-736
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.3 , pp. 730-736
    • Opila, E.J.1
  • 25
    • 0041428202 scopus 로고    scopus 로고
    • Oxidation and volatilization of silica formers in water vapor
    • Opila E.J. Oxidation and volatilization of silica formers in water vapor. J. Am. Ceram. Soc. 86 8 (2003) 1238-1248
    • (2003) J. Am. Ceram. Soc. , vol.86 , Issue.8 , pp. 1238-1248
    • Opila, E.J.1
  • 26
    • 0001518018 scopus 로고
    • Fabrication and secondary phase crystallization of rare-earth disilicate-silicon nitride ceramics
    • Cinibulk M.K., and Thomas G. Fabrication and secondary phase crystallization of rare-earth disilicate-silicon nitride ceramics. J. Am. Ceram. Soc. 75 8 (1992) 2037-2043
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.8 , pp. 2037-2043
    • Cinibulk, M.K.1    Thomas, G.2
  • 27
    • 0026789421 scopus 로고
    • Oxidation behavior of rare-earth disilicate silicon nitride ceramics
    • Cinibulk M.K., Thomas G., and Johnson S.M. Oxidation behavior of rare-earth disilicate silicon nitride ceramics. J. Am. Ceram. Soc. 75 8 (1992) 2044-2049
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.8 , pp. 2044-2049
    • Cinibulk, M.K.1    Thomas, G.2    Johnson, S.M.3
  • 29
    • 0002488967 scopus 로고    scopus 로고
    • Corrosion of hard materials
    • Riedel R. (Ed), VCH-Wiley, Weinheim
    • Nickel K.G., and Gogotsi Y.G. Corrosion of hard materials. In: Riedel R. (Ed). Handbook of ceramic hard materials (2000), VCH-Wiley, Weinheim 140-182
    • (2000) Handbook of ceramic hard materials , pp. 140-182
    • Nickel, K.G.1    Gogotsi, Y.G.2
  • 30
    • 33846652867 scopus 로고
    • Improvement of the oxidation behavior of reaction bonded silicon nitride by addition of aluminium
    • Barlier P., and Torre J.P. Improvement of the oxidation behavior of reaction bonded silicon nitride by addition of aluminium. Mater. Sci. Mon. 6 (1980) 718-728
    • (1980) Mater. Sci. Mon. , vol.6 , pp. 718-728
    • Barlier, P.1    Torre, J.P.2
  • 31
    • 0346294509 scopus 로고
    • Oxidation mechanism of porous silicon nitride
    • Porz F., and Thümmler F. Oxidation mechanism of porous silicon nitride. J. Mater. Sci. 19 (1984) 1283-1295
    • (1984) J. Mater. Sci. , vol.19 , pp. 1283-1295
    • Porz, F.1    Thümmler, F.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.