A SiC whisker-toughened SiC-CrSi 2 oxidation protective coating for carbon/carbon composites

Author keywords

Carbon carbon composites; Coating; Oxidation

Indexed keywords

CRYSTAL WHISKERS; OXIDATION; PROTECTIVE COATINGS; THERMAL STRESS;

EID: 33846602686     PISSN: 01694332     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.apsusc.2006.07.092     Document Type: Article
Times cited : (34)

References (8)
  • 1
    • 0034960755 scopus 로고    scopus 로고
    • SiC/C multi-layered coating contributing to the antioxidation of C/C composites and the suppression of through-thickness cracks in the layer
    • Takuya A., Hiroshi H., Taku H., Hiroshi F., and Ichiro S. SiC/C multi-layered coating contributing to the antioxidation of C/C composites and the suppression of through-thickness cracks in the layer. Carbon 39 (2001) 1477
    • (2001) Carbon , vol.39 , pp. 1477
    • Takuya, A.1    Hiroshi, H.2    Taku, H.3    Hiroshi, F.4    Ichiro, S.5
  • 2
    • 0029217451 scopus 로고
    • Multilayered coatings for protecting carbon-carbon composites from oxidation
    • Guo M.L., Shen K., and Zheng Y.D. Multilayered coatings for protecting carbon-carbon composites from oxidation. Carbon 33 (1995) 449
    • (1995) Carbon , vol.33 , pp. 449
    • Guo, M.L.1    Shen, K.2    Zheng, Y.D.3
  • 3
    • 2542482759 scopus 로고    scopus 로고
    • 2 -SiC multilayer ceramic coating on oxidation resistance
    • 2 -SiC multilayer ceramic coating on oxidation resistance. J. Chin. Ceram. Soc. 27 1 (1999) 8
    • (1999) J. Chin. Ceram. Soc. , vol.27 , Issue.1 , pp. 8
    • Zeng, X.R.1    Li, H.J.2    Yang, Z.3
  • 5
    • 24144488169 scopus 로고    scopus 로고
    • SiC/yttrium silicate multi-layer coating for oxidation protection of carbon/carbon composites
    • Huang J.F., Zeng X.R., Li H.J., Xiong X.B., Fu Y.W., and Huang M. SiC/yttrium silicate multi-layer coating for oxidation protection of carbon/carbon composites. J. Mater. Sci. 39 (2004) 7383
    • (2004) J. Mater. Sci. , vol.39 , pp. 7383
    • Huang, J.F.1    Zeng, X.R.2    Li, H.J.3    Xiong, X.B.4    Fu, Y.W.5    Huang, M.6
  • 6
    • 27744510122 scopus 로고    scopus 로고
    • SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites
    • Li H.J., Fu Q.G., Shi X.H., Li K.Z., and Hu Z.B. SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites. Carbon 44 (2006) 602
    • (2006) Carbon , vol.44 , pp. 602
    • Li, H.J.1    Fu, Q.G.2    Shi, X.H.3    Li, K.Z.4    Hu, Z.B.5
  • 8
    • 0026115117 scopus 로고
    • Microstructural design of toughened ceramics
    • Becher F. Microstructural design of toughened ceramics. J. Am. Ceram. Soc. 74 (1991) 255
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 255
    • Becher, F.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.