메뉴 건너뛰기




Volumn 90, Issue 2, 2007, Pages 523-532

Is glass infiltration beneficial to improve fretting wear properties for alumina?

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINA; ATOMIC FORCE MICROSCOPY; INFILTRATION; THERMODYNAMIC PROPERTIES; WEAR OF MATERIALS; X RAY DIFFRACTION ANALYSIS;

EID: 33846517574     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2006.01380.x     Document Type: Article
Times cited : (12)

References (39)
  • 2
    • 0003749418 scopus 로고
    • Cambridge University Press. Cambridge, U.K
    • B. Lawn. Fracture of Brittle Solids. Cambridge University Press. Cambridge, U.K., 1993.
    • (1993) Fracture of Brittle Solids
    • Lawn, B.1
  • 3
    • 33846521509 scopus 로고    scopus 로고
    • M. W. Barsoum, Fundamentals of Ceramics. Mograw-Hill International Editions, U.K., 1997.
    • M. W. Barsoum, Fundamentals of Ceramics. Mograw-Hill International Editions, U.K., 1997.
  • 4
    • 84985166065 scopus 로고
    • Mullite/Alumina Particulate Composites by Infiltration Processing: III, Mechanical Properties
    • B. R. Marple and D. J. Green, "Mullite/Alumina Particulate Composites by Infiltration Processing: III, Mechanical Properties," J. Am. Ceram. Soc., 74 [10] 2453-59 (1991).
    • (1991) J. Am. Ceram. Soc , vol.74 , Issue.10 , pp. 2453-2459
    • Marple, B.R.1    Green, D.J.2
  • 5
    • 0038345481 scopus 로고    scopus 로고
    • Wear of Hydroxyapalite Sliding Against Glass-Infiltrated Alumina
    • M. Kalin, B. Hockey, and S. Jahanmir, "Wear of Hydroxyapalite Sliding Against Glass-Infiltrated Alumina," J. Mater. Res., 18 [1] 27-36 (2003).
    • (2003) J. Mater. Res , vol.18 , Issue.1 , pp. 27-36
    • Kalin, M.1    Hockey, B.2    Jahanmir, S.3
  • 6
    • 0034285033 scopus 로고    scopus 로고
    • Fabrication of Composite Coatings using a Combination of Electrochemical Methods and Reaction Bonding Process
    • Z. C. Wang, J. Shemilt, and P. Xiao, "Fabrication of Composite Coatings using a Combination of Electrochemical Methods and Reaction Bonding Process," J. Ear. Ceram. Soc., 20, 1469-73 (2000).
    • (2000) J. Ear. Ceram. Soc , vol.20 , pp. 1469-1473
    • Wang, Z.C.1    Shemilt, J.2    Xiao, P.3
  • 7
    • 20444386226 scopus 로고    scopus 로고
    • Plasma-Sprayed Glass-Ceramic Coatings on Ceramic Tiles: Microstructure, Chemical Resistance and Mechanical Properties
    • B. Giovanni, C. Valeria, L. Luca, M. Tiziano, S. Cristina, B. Cecilia, L. Alessio, and V. Teodoro. "Plasma-Sprayed Glass-Ceramic Coatings on Ceramic Tiles: Microstructure, Chemical Resistance and Mechanical Properties," J. Eur. Ceram. Soc., 25, 1835-53 (2005).
    • (2005) J. Eur. Ceram. Soc , vol.25 , pp. 1835-1853
    • Giovanni, B.1    Valeria, C.2    Luca, L.3    Tiziano, M.4    Cristina, S.5    Cecilia, B.6    Alessio, L.7    Teodoro, V.8
  • 8
    • 0035568794 scopus 로고    scopus 로고
    • Abrasive Wear Resistance of Plasma-Sprayed Glass-Composite Coatings
    • D. T. Gawne, Z. Qiu, Y. Bao, T. Zhang, and K. Zhang, "Abrasive Wear Resistance of Plasma-Sprayed Glass-Composite Coatings," J. Thermal Spray Technol., 10 [4] 599-603 (2001).
    • (2001) J. Thermal Spray Technol , vol.10 , Issue.4 , pp. 599-603
    • Gawne, D.T.1    Qiu, Z.2    Bao, Y.3    Zhang, T.4    Zhang, K.5
  • 9
    • 0033605128 scopus 로고    scopus 로고
    • Crack Arrest and Multiple Cracking in Glass Through the Use of Designed Residual Stress Profiles
    • D. J. Green, R. Tandon, and V. M. Sglavo, "Crack Arrest and Multiple Cracking in Glass Through the Use of Designed Residual Stress Profiles," Science, 283 [5406] 1295-7 (1999).
    • (1999) Science , vol.283 , Issue.5406 , pp. 1295-1297
    • Green, D.J.1    Tandon, R.2    Sglavo, V.M.3
  • 11
    • 0030111760 scopus 로고    scopus 로고
    • Thermal Stresses in Diamond Coatings and their Influence on Coating Wear and Failure
    • J. Gunnars and A. Alahelisten, "Thermal Stresses in Diamond Coatings and their Influence on Coating Wear and Failure," Surf. Coatings Technol., 80, 303-12 (1996).
    • (1996) Surf. Coatings Technol , vol.80 , pp. 303-312
    • Gunnars, J.1    Alahelisten, A.2
  • 12
    • 84985044951 scopus 로고
    • Crack Stability and T-Curves Due to Macroscopic Residual Compressive Stress Profiles
    • R. Tandon and D. J. Green, "Crack Stability and T-Curves Due to Macroscopic Residual Compressive Stress Profiles," J. Am. Ceram. Soc., 74 [8] 1981-6 (1991).
    • (1991) J. Am. Ceram. Soc , vol.74 , Issue.8 , pp. 1981-1986
    • Tandon, R.1    Green, D.J.2
  • 13
    • 5544283215 scopus 로고
    • Mullite/Alumina Particulate Composites by Infiltration Processing: IV, Residual Stress Profiles
    • B. R. Marple and D. J. Green, "Mullite/Alumina Particulate Composites by Infiltration Processing: IV, Residual Stress Profiles," J. Am. Ceram. Soc., 75 [1] 44-51 (1992).
    • (1992) J. Am. Ceram. Soc , vol.75 , Issue.1 , pp. 44-51
    • Marple, B.R.1    Green, D.J.2
  • 14
    • 0031193072 scopus 로고    scopus 로고
    • Strengthening of Alumina by Formation of a Mullite/Glass Layer on the Surface
    • H. E. Kim, A. J. Moorhead, and S. H. Kim, "Strengthening of Alumina by Formation of a Mullite/Glass Layer on the Surface," J. Am. Ceram. Soc., 80 [7] 1877-80 (1997).
    • (1997) J. Am. Ceram. Soc , vol.80 , Issue.7 , pp. 1877-1880
    • Kim, H.E.1    Moorhead, A.J.2    Kim, S.H.3
  • 15
    • 0041568275 scopus 로고    scopus 로고
    • Influence of Roughness on Wear Transition in Glass-Infiltrated Alumina
    • M. Kalin and S. Jahanmir, "Influence of Roughness on Wear Transition in Glass-Infiltrated Alumina," Wear, 255, 669-76 (2003).
    • (2003) Wear , vol.255 , pp. 669-676
    • Kalin, M.1    Jahanmir, S.2
  • 16
    • 27744581119 scopus 로고    scopus 로고
    • Wear Mechanisms of Glass-Infiltrated Alumina Sliding Against Alumina in Water
    • M. Kalin, S. Jahanmir, and G. Dražič, "Wear Mechanisms of Glass-Infiltrated Alumina Sliding Against Alumina in Water," J. Am. Ceram. Soc., 88 [2] 346-52 (2005).
    • (2005) J. Am. Ceram. Soc , vol.88 , Issue.2 , pp. 346-352
    • Kalin, M.1    Jahanmir, S.2    Dražič, G.3
  • 17
    • 84987335986 scopus 로고
    • A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I. Direct Crack Measurements
    • G. R. Anstis, P. Chantikul, B. R. Lawn, and D. B. Marshall, "A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I. Direct Crack Measurements," J. Am. Ceram. Soc., 64, 533 (1981).
    • (1981) J. Am. Ceram. Soc , vol.64 , pp. 533
    • Anstis, G.R.1    Chantikul, P.2    Lawn, B.R.3    Marshall, D.B.4
  • 21
    • 33846545273 scopus 로고    scopus 로고
    • R. B. Waterhouse, Fretting Wear, p. 242, ASM Handbook, 18. ASM International VA, U.S.A., (1992).
    • R. B. Waterhouse, "Fretting Wear," p. 242, ASM Handbook, Vol. 18. ASM International VA, U.S.A., (1992).
  • 22
    • 45549118580 scopus 로고
    • Analysis of Elastic and Plastic Deformation Associated with Indentation Testing of Thin Films on Substrates
    • A. K. Bhattacharya and W. D. Nix, "Analysis of Elastic and Plastic Deformation Associated with Indentation Testing of Thin Films on Substrates," Int. J. Solids Struc., 24, 1287-98 (1988).
    • (1988) Int. J. Solids Struc , vol.24 , pp. 1287-1298
    • Bhattacharya, A.K.1    Nix, W.D.2
  • 25
    • 0041353432 scopus 로고    scopus 로고
    • Wear and Friction Behavior of Alumina Ceramics in Aqueous Solutions with Different pH
    • M. Kalin, S. Novak, and J. Vižntin, "Wear and Friction Behavior of Alumina Ceramics in Aqueous Solutions with Different pH," Wear, 254, 1141-6 (2003).
    • (2003) Wear , vol.254 , pp. 1141-1146
    • Kalin, M.1    Novak, S.2    Vižntin, J.3
  • 26
    • 33745668708 scopus 로고    scopus 로고
    • Understanding the Fretting Wear of Ti3SiC2
    • D. Sarkar, B. V. M. Kumar, and B. Basu, "Understanding the Fretting Wear of Ti3SiC2," J. Eur. Ceram. Soc., 26 [13] 2441-52 (2006).
    • (2006) J. Eur. Ceram. Soc , vol.26 , Issue.13 , pp. 2441-2452
    • Sarkar, D.1    Kumar, B.V.M.2    Basu, B.3
  • 28
    • 0019899515 scopus 로고
    • 4) Between 5.1 and 383 K: Comparison of Calorimetric and Equilibrium Values for the QFM Buffer Reaction
    • 4) Between 5.1 and 383 K: Comparison of Calorimetric and Equilibrium Values for the QFM Buffer Reaction," Am. Mineralogist, 67, 463-9 (1982).
    • (1982) Am. Mineralogist , vol.67 , pp. 463-469
    • Robie, R.A.1    Finch, C.B.2    Hemingway, B.S.3
  • 29
    • 85024713483 scopus 로고
    • Principles and Applications of Aquatic Chemistry
    • NY, U.S.A
    • R M. M. Morel and J. G. Hering, Principles and Applications of Aquatic Chemistry. Willey-IEEE, NY, U.S.A., 1993.
    • (1993) Willey-IEEE
    • Morel, R.M.M.1    Hering, J.G.2
  • 30
    • 29744464486 scopus 로고    scopus 로고
    • Crack Repairing in Alumina by Penetrating Glass
    • M. C. Chu, S. J. Cho, K. J. Yoon, and H. M. Park, "Crack Repairing in Alumina by Penetrating Glass," J. Am, Ceram. Soc., 88 [2] 491-3 (2005).
    • (2005) J. Am, Ceram. Soc , vol.88 , Issue.2 , pp. 491-493
    • Chu, M.C.1    Cho, S.J.2    Yoon, K.J.3    Park, H.M.4
  • 31
    • 33846520240 scopus 로고    scopus 로고
    • 2 Composites, Advanced in Ceramics, 12. Edited by N. Claussen, M. Rühlc and A. H. Heuer. Am Ceram Soc, Inc, Columbus, OH, 1984.
    • 2 Composites, Advanced in Ceramics, Vol. 12. Edited by N. Claussen, M. Rühlc and A. H. Heuer. Am Ceram Soc, Inc, Columbus, OH, 1984.
  • 32
    • 0346724195 scopus 로고    scopus 로고
    • Characterization of Ceramic Coatings Sintering Using Residual Stress Measurements
    • X. Wang and P. Xiao, "Characterization of Ceramic Coatings Sintering Using Residual Stress Measurements," J. Eur. Ceram. Soc., 24, 283-8 (2004).
    • (2004) J. Eur. Ceram. Soc , vol.24 , pp. 283-288
    • Wang, X.1    Xiao, P.2
  • 34
    • 0032483849 scopus 로고    scopus 로고
    • Depths of Cracks Produced by Abrasion of Brittle Materials
    • S. G. Roberts, "Depths of Cracks Produced by Abrasion of Brittle Materials," Scripta. Mater., 40 [1] 101-8 (1999).
    • (1999) Scripta. Mater , vol.40 , Issue.1 , pp. 101-108
    • Roberts, S.G.1
  • 35
    • 84977695915 scopus 로고
    • Influence of Water Vapor on Crack Propagation in Soda-Lime Glass
    • S. M. Wiederhon, "Influence of Water Vapor on Crack Propagation in Soda-Lime Glass," J. Am. Ceram. Soc., 50, 407-14 (1967).
    • (1967) J. Am. Ceram. Soc , vol.50 , pp. 407-414
    • Wiederhon, S.M.1
  • 37
    • 33846478496 scopus 로고    scopus 로고
    • A. R. C. Westwood, Environment-Sensitive Fracture of Ionic and Ceramic Solids; pp. 283-297 in Proc. Int. Conf. on Mechanisms of Environmnent Sensitive Cracking of Materials, Edited by A. R. C. Westwoos el al. Metals Society, London, 1974.
    • A. R. C. Westwood, "Environment-Sensitive Fracture of Ionic and Ceramic Solids"; pp. 283-297 in Proc. Int. Conf. on Mechanisms of Environmnent Sensitive Cracking of Materials, Edited by A. R. C. Westwoos el al. Metals Society, London, 1974.
  • 38
    • 0041721258 scopus 로고    scopus 로고
    • Role of Water Vapor on the Wear of Mn-Zn Ferrite Heads Sliding Against Magnetic Tapes
    • B. Bhushan and D. V. Khatavkar, "Role of Water Vapor on the Wear of Mn-Zn Ferrite Heads Sliding Against Magnetic Tapes," Wear, 202, 30-34 (1996).
    • (1996) Wear , vol.202 , pp. 30-34
    • Bhushan, B.1    Khatavkar, D.V.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.