메뉴 건너뛰기




Volumn 18, Issue 4, 2006, Pages 297-304

Laser clad WC reinforced Ni-based intermetallic-matrix composites to improve cavitation erosion resistance

Author keywords

Cavitation erosion; Intermetallic composite coating; Laser cladding; Ni3Al; NiAl

Indexed keywords

CAVITATION CORROSION; CLADDING (COATING); HEAT TREATMENT; INTERMETALLICS; MICROHARDNESS; MICROSTRUCTURE; NICKEL COMPOUNDS; STAINLESS STEEL;

EID: 33845255053     PISSN: 1042346X     EISSN: None     Source Type: Journal    
DOI: 10.2351/1.2355521     Document Type: Article
Times cited : (17)

References (26)
  • 1
    • 0020103006 scopus 로고
    • "Cavitation erosion of cast iron diesel engine liners"
    • Y. K. Zhou, J. G. He, and F. G. Hammit, "Cavitation erosion of cast iron diesel engine liners," Wear 76, 329-335 (1982).
    • (1982) Wear , vol.76 , pp. 329-335
    • Zhou, Y.K.1    He, J.G.2    Hammit, F.G.3
  • 2
    • 0022737693 scopus 로고
    • "Effects of titanium implantation on cavitation erosion of cobalt-based metal-carbide systems"
    • N. V. H. Gately and S. A. Dillich, "Effects of titanium implantation on cavitation erosion of cobalt-based metal-carbide systems," Mater. Sci. Eng. 90, 333-338 (1987).
    • (1987) Mater. Sci. Eng. , vol.90 , pp. 333-338
    • Gately, N.V.H.1    Dillich, S.A.2
  • 3
    • 0022062624 scopus 로고
    • "Cavitation erosion characteristics of nickel-based alloy-composite coatings obtained by plasma spraying"
    • B. S. Mann, P. R. Krishnamoorthy, and P. Vivekananda, "Cavitation erosion characteristics of nickel-based alloy-composite coatings obtained by plasma spraying," Wear 103, 43-55 (1985).
    • (1985) Wear , vol.103 , pp. 43-55
    • Mann, B.S.1    Krishnamoorthy, P.R.2    Vivekananda, P.3
  • 4
    • 1342331925 scopus 로고    scopus 로고
    • "Coating fracture toughness determined by vickers indentation: An important parameter in cavitation erosion resistance of WC-Co thermally sprayed coatings"
    • M. M. Lima, C. Godoy, P. J. Modenesi, J. C. Avelar-Batista, A. Davison, and A. Matthews, "Coating fracture toughness determined by vickers indentation: an important parameter in cavitation erosion resistance of WC-Co thermally sprayed coatings," Surf. Coat. Technol, 177-178, 489-496 (2004).
    • (2004) Surf. Coat. Technol, , vol.177-178 , pp. 489-496
    • Lima, M.M.1    Godoy, C.2    Modenesi, P.J.3    Avelar-Batista, J.C.4    Davison, A.5    Matthews, A.6
  • 5
    • 0042740597 scopus 로고    scopus 로고
    • "Laser transformation hardening of AISI 440C martensitic stainless steel for higher cavitation erosion resistance"
    • K. H. Lo, F. T. Cheng, and H. C. Man, "Laser transformation hardening of AISI 440C martensitic stainless steel for higher cavitation erosion resistance," Surf. Coat. Technol. 173, 96-104 (2003).
    • (2003) Surf. Coat. Technol. , vol.173 , pp. 96-104
    • Lo, K.H.1    Cheng, F.T.2    Man, H.C.3
  • 6
    • 0034072153 scopus 로고    scopus 로고
    • "Cavitation erosion and pitting corrosion behaviour of laser surface-melted martensitic stainless steel UNS S42000"
    • C. T. Kwok, H. C. Man, and F. T. Cheng, "Cavitation erosion and pitting corrosion behaviour of laser surface-melted martensitic stainless steel UNS S42000," Surf. Coat. Technol. 126, 238-255 (2000).
    • (2000) Surf. Coat. Technol. , vol.126 , pp. 238-255
    • Kwok, C.T.1    Man, H.C.2    Cheng, F.T.3
  • 7
    • 0037450473 scopus 로고    scopus 로고
    • "Improvement of cavitation erosion resistance of AISI 316 stainless steel by laser surface alloying using fine WC powder"
    • K. H. Lo, F. T. Cheng, C. T. Kwok, and H. C. Man, "Improvement of cavitation erosion resistance of AISI 316 stainless steel by laser surface alloying using fine WC powder," Surf. Coat. Technol. 165, 258-267 (2003).
    • (2003) Surf. Coat. Technol. , vol.165 , pp. 258-267
    • Lo, K.H.1    Cheng, F.T.2    Kwok, C.T.3    Man, H.C.4
  • 8
    • 0036894402 scopus 로고    scopus 로고
    • "Cavitation erosion resistance of stainless steel laser-clad with WC-reinforced MMC"
    • F. T. Cheng, C. T. Kwok, and H. C. Man, "Cavitation erosion resistance of stainless steel laser-clad with WC-reinforced MMC," Mater. Lett. 57, 969-974 (2002).
    • (2002) Mater. Lett. , vol.57 , pp. 969-974
    • Cheng, F.T.1    Kwok, C.T.2    Man, H.C.3
  • 10
    • 0034262777 scopus 로고    scopus 로고
    • "Emerging applications of intermetallics"
    • N. S. Stoloff, C. T. Liu, and S. C. Deevi, "Emerging applications of intermetallics," Intermetallics 8, 1313-1320 (2000).
    • (2000) Intermetallics , vol.8 , pp. 1313-1320
    • Stoloff, N.S.1    Liu, C.T.2    Deevi, S.C.3
  • 11
    • 0035484533 scopus 로고    scopus 로고
    • "Optimization of toughness and strength in multiphase intermetallics"
    • A. Misra, R. Gibala, and R. D. Noebe, "Optimization of toughness and strength in multiphase intermetallics," Intermetallics 9, 971-978 (2001).
    • (2001) Intermetallics , vol.9 , pp. 971-978
    • Misra, A.1    Gibala, R.2    Noebe, R.D.3
  • 12
    • 0034262913 scopus 로고    scopus 로고
    • "Plasticity in multiphase intermetallics"
    • A. Misra and R. Gibala, "Plasticity in multiphase intermetallics," Intermetallics 8, 1025-1034 (2000).
    • (2000) Intermetallics , vol.8 , pp. 1025-1034
    • Misra, A.1    Gibala, R.2
  • 14
    • 0142091610 scopus 로고    scopus 로고
    • 3Al intermetallic matrix composite coating by laser powder deposition"
    • 3Al intermetallic matrix composite coating by laser powder deposition," J. Mater. Sci. Lett. 22, 1369-1372 (2003).
    • (2003) J. Mater. Sci. Lett. , vol.22 , pp. 1369-1372
    • Xu, X.Y.1    Liu, W.J.2    Zhong, M.L.3    Sun, H.Q.4
  • 15
    • 4544377323 scopus 로고    scopus 로고
    • "Laser synthesizing NiAl intermetallic and TiC reinforced NiAl intermetallic matrix composite"
    • M. L. Zhong, X. Y. Xu, W. J. Liu, and H. Q. Sun, "Laser synthesizing NiAl intermetallic and TiC reinforced NiAl intermetallic matrix composite," J. Laser Appl. 16, 160-166 (2004).
    • (2004) J. Laser Appl. , vol.16 , pp. 160-166
    • Zhong, M.L.1    Xu, X.Y.2    Liu, W.J.3    Sun, H.Q.4
  • 18
    • 1542377524 scopus 로고    scopus 로고
    • "Microstructure and wear resistance of a laser clad TiC reinforced nickel aluminides matrix composite coating"
    • Y. Chen and H. M. Wang, "Microstructure and wear resistance of a laser clad TiC reinforced nickel aluminides matrix composite coating," Mater. Sci. Eng., A 368, 80-87 (2004).
    • (2004) Mater. Sci. Eng., A , vol.368 , pp. 80-87
    • Chen, Y.1    Wang, H.M.2
  • 19
    • 33845247763 scopus 로고    scopus 로고
    • "Standard test method for cavitation erosion using vibratory apparatus"
    • ASTM Standard G32-98
    • ASTM Standard G32-98, "Standard test method for cavitation erosion using vibratory apparatus," Annual Book of ASTM Standards, 1998, Vol. 03.02, pp. 115-128.
    • (1998) Annual Book of ASTM Standards , vol.3 , Issue.2 , pp. 115-128
  • 20
    • 32644479195 scopus 로고    scopus 로고
    • "Particle-laden liquid impact erosion characteristics of laser clad Ni-based intermetallic matrix composites with TiC and WC reinforcements"
    • M. Duraiselvam, R. Galun, S. Siegmann, V. Wesling, and B. L. Mordike, "Particle-laden liquid impact erosion characteristics of laser clad Ni-based intermetallic matrix composites with TiC and WC reinforcements," Lasers Eng. 15, 355-373 (2005).
    • (2005) Lasers Eng. , vol.15 , pp. 355-373
    • Duraiselvam, M.1    Galun, R.2    Siegmann, S.3    Wesling, V.4    Mordike, B.L.5
  • 21
  • 22
    • 0031223568 scopus 로고    scopus 로고
    • "Mechanical alloying synthesis and structural characterization of ternary Ni-Al-Fe alloys"
    • Z. G. Liu, J. T. Guo, L. Z. Zhou, Z. H. Hu, and M. Umemoto, "Mechanical alloying synthesis and structural characterization of ternary Ni-Al-Fe alloys," J. Mater. Sci. 32, 4857-4864 (1997).
    • (1997) J. Mater. Sci. , vol.32 , pp. 4857-4864
    • Liu, Z.G.1    Guo, J.T.2    Zhou, L.Z.3    Hu, Z.H.4    Umemoto, M.5
  • 23
    • 0037454550 scopus 로고    scopus 로고
    • "Cavitation erosion-corrosion characteristics of laser surface modified NiTi shape memory alloy"
    • Z. D. Cui, H. C. Man, F. T. Cheng, and T. M. Yue, "Cavitation erosion-corrosion characteristics of laser surface modified NiTi shape memory alloy," Surf. Coat. Technol. 162, 147-153 (2003).
    • (2003) Surf. Coat. Technol. , vol.162 , pp. 147-153
    • Cui, Z.D.1    Man, H.C.2    Cheng, F.T.3    Yue, T.M.4
  • 24
    • 0023530809 scopus 로고
    • "Cavitation erosion of composites - A materials perspective"
    • R. B. Bhagat, "Cavitation erosion of composites - a materials perspective," J. Mater. Sci. Lett. 6, 1473-1475 (1987).
    • (1987) J. Mater. Sci. Lett. , vol.6 , pp. 1473-1475
    • Bhagat, R.B.1
  • 25
    • 0032131442 scopus 로고    scopus 로고
    • "Laser surface modification of UNS S31603 stainless steel using NiCrBSi alloy for enhancing cavitation erosion resistance"
    • C. T. Kwok, F. T. Cheng, and H. C. Man, "Laser surface modification of UNS S31603 stainless steel using NiCrBSi alloy for enhancing cavitation erosion resistance," Surf. Coat. Technol. 107, 31-40 (1998).
    • (1998) Surf. Coat. Technol. , vol.107 , pp. 31-40
    • Kwok, C.T.1    Cheng, F.T.2    Man, H.C.3
  • 26
    • 0030215125 scopus 로고    scopus 로고
    • "Mechanism of cavitation erosion of TiAl-based titanium aluminide intermetallic alloys"
    • R. L. Howards and A. Ball, "Mechanism of cavitation erosion of TiAl-based titanium aluminide intermetallic alloys," Acta Mater. 44, 3157-3168 (1996).
    • (1996) Acta Mater. , vol.44 , pp. 3157-3168
    • Howards, R.L.1    Ball, A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.