Volumn 161, Issue 2, 2006, Pages 1002-1011

High voltage stability of nanostructured thin film catalysts for PEM fuel cells

Author keywords

Catalyst agglomeration; Catalyst support corrosion; Catalyst surface area stability; Electrocatalyst ageing mechanisms; Nanostructured thin film catalyst; Polymer electrolyte fuel cells

Indexed keywords

CATALYST SUPPORTS; CATHODES; CORROSION; ELECTROLYTES; FUEL CELLS; NANOSTRUCTURED MATERIALS; POLYMERS;

EID: 33751113010     PISSN: 03787753     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jpowsour.2006.05.033     Document Type: Article
Times cited : (403)

References (20)
  • 3
    • 30344474640 scopus 로고    scopus 로고
    • Ex situ and in situ stability studies of PEMFC catalysts: effect of carbon type and humidification on degradation of the carbon
    • Stevens D., Hicks M., Haugen G., and Dahn J. Ex situ and in situ stability studies of PEMFC catalysts: effect of carbon type and humidification on degradation of the carbon. J. Electrochem. Soc. 152 12 (2005) A2309
    • (2005) J. Electrochem. Soc. , vol.152 , Issue.12
    • Stevens, D.1    Hicks, M.2    Haugen, G.3    Dahn, J.4
  • 9
    • 33751291839 scopus 로고    scopus 로고
    • M.K. Debe, S.M. Hendricks, A.K. Schmoeckel, R.T. Atanasoski, G.D. Vernstrom, G.M. Haugen, Durability aspects of nanostructured thin film catalysts for PEM fuel cells, in: ECS Transactions, vol. 1, Durability and Reliability of Low-Temperature Fuel Cells Systems, 208th ECS Meeting, 2005.
  • 12
    • 84860038868 scopus 로고    scopus 로고
    • Advanced catalyst and membrane technology with enhanced performance and durability for automotive requirements
    • Kofu, Japan
    • Debe M.K. Advanced catalyst and membrane technology with enhanced performance and durability for automotive requirements. Proceedings of the 4th International Fuel Cell Workshop 2005. Kofu, Japan (September 22-24, 2005) 62
    • (2005) Proceedings of the 4th International Fuel Cell Workshop 2005 , pp. 62
    • Debe, M.K.1
  • 13
    • 85070156668 scopus 로고    scopus 로고
    • M.K. Debe et al., VII.A.2 Advanced MEAs for enhanced operating conditions, in: DOE Hydrogen, Fuel Cells and Infrastructure Technologies Program FY 2005 Progress Report, p. 672
  • 14
    • 85070143140 scopus 로고    scopus 로고
    • in: DOE Hydrogen Program FY 2004 Progress Report, p. 301.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.