Volumn 16, Issue 4, 2006, Pages 922-926

Fracture behaviors of AZ80 magnesium alloy during multiple forging processes

Author keywords

AZ80 magnesium alloy; Cracks; Fracture behaviors; Multiple forging

Indexed keywords

CRACK INITIATION; CRACK PROPAGATION; DEFORMATION; FORGING; FRACTURE; GRAIN BOUNDARIES; INTERFACES (MATERIALS); MICROCRACKING; MICROCRACKS; NUCLEATION; TENSILE STRESS;

EID: 33750998548     PISSN: 10036326     EISSN: None     Source Type: Journal    
DOI: 10.1016/S1003-6326(06)60352-X     Document Type: Article
Times cited : (24)

References (20)
  • 1
    • 0035871499 scopus 로고    scopus 로고
    • Magnesium properties-applications-potential
    • MORDIKE B L, EBERT T. Magnesium properties-applications-potential[J]. Mater Sci Eng A, 2001, A302: 37-45.
    • (2001) Mater Sci Eng A , vol.A302 , pp. 37-45
    • Mordike, B.L.1    Ebert, T.2
  • 2
    • 14644394318 scopus 로고    scopus 로고
    • Geometrical criterion for the activation of prismatic slip in AZ61 Mg alloy sheets deformed at room temperature
    • KOIKE J, OHYAMA R. Geometrical criterion for the activation of prismatic slip in AZ61 Mg alloy sheets deformed at room temperature[J]. Acta Mater, 2005, 53: 1963-1972.
    • (2005) Acta Mater , vol.53 , pp. 1963-1972
    • Koike, J.1    Ohyama, R.2
  • 3
    • 0036532818 scopus 로고    scopus 로고
    • Forming limit of magnesium alloy at elevated temperatures for precision forging
    • OGAWA N, SHIOMI M, OSAKADA K. Forming limit of magnesium alloy at elevated temperatures for precision forging[J]. Int J Mach Tool Manu, 2002, 42(5): 607-614.
    • (2002) Int J Mach Tool Manu , vol.42 , Issue.5 , pp. 607-614
    • Ogawa, N.1    Shiomi, M.2    Osakada, K.3
  • 4
    • 0034307154 scopus 로고    scopus 로고
    • Micromechanisms of deformation in high-purity hot-pressed alumina
    • STAEHLER J M, PREDEBON W W. Micromechanisms of deformation in high-purity hot-pressed alumina[J]. Mater Sci Eng A, 2000, A291: 37-45.
    • (2000) Mater Sci Eng A , vol.A291 , pp. 37-45
    • Staehler, J.M.1    Predebon, W.W.2
  • 5
    • 0842334593 scopus 로고    scopus 로고
    • Investigation of surface fatigue microcrack growth behavior of cast Mg-Al alloy
    • WANG X S, LU X, WANG D H. Investigation of surface fatigue microcrack growth behavior of cast Mg-Al alloy[J]. Mater Sci Eng A, 2004, A364: 11-16.
    • (2004) Mater Sci Eng A , vol.A364 , pp. 11-16
    • Wang, X.S.1    Lu, X.2    Wang, D.H.3
  • 6
    • 0033688663 scopus 로고    scopus 로고
    • Fracture behavior of AZ91 magnesium alloy
    • LU Y Z, WANG Q D, DING W J. Fracture behavior of AZ91 magnesium alloy[J]. Mater Lett, 2000, 44: 265-268.
    • (2000) Mater Lett , vol.44 , pp. 265-268
    • Lu, Y.Z.1    Wang, Q.D.2    Ding, W.J.3
  • 7
    • 0036165274 scopus 로고    scopus 로고
    • High temperature deformation behavior of permanent casting AZ91 alloy with and without Sb addition
    • YUAN G Y, WANG Q D, DING W J. High temperature deformation behavior of permanent casting AZ91 alloy with and without Sb addition[J]. J Mater Sci, 2002, 37: 127-132.
    • (2002) J Mater Sci , vol.37 , pp. 127-132
    • Yuan, G.Y.1    Wang, Q.D.2    Ding, W.J.3
  • 8
    • 2942668167 scopus 로고    scopus 로고
    • Microstructure evolution during reheating of an extruded Mg-Al-Zn alloy into the semisolid state
    • KLEINER S, BEFFORT O, UGGOWITZER P J. Microstructure evolution during reheating of an extruded Mg-Al-Zn alloy into the semisolid state[J]. Scripta Mater, 2004, 51: 405-410.
    • (2004) Scripta Mater , vol.51 , pp. 405-410
    • Kleiner, S.1    Beffort, O.2    Uggowitzer, P.J.3
  • 9
    • 0042807566 scopus 로고    scopus 로고
    • w/AZ91 magnesium matrix composite during in-situ TEM straining
    • w/AZ91 magnesium matrix composite during in-situ TEM straining[J]. J Mater Sci, 2003, 38: 2647-2654.
    • (2003) J Mater Sci , vol.38 , pp. 2647-2654
    • Zheng, M.Y.1    Zhang, W.C.2    Wu, K.3    Yao, C.K.4
  • 10
    • 0036877084 scopus 로고    scopus 로고
    • Microstructure and mechanical properties of squeeze cast and semi-solid cast Mg-Al alloys
    • KLEINER S, BEFFORT O, WAHLEN A, UGGOWITZER P J. Microstructure and mechanical properties of squeeze cast and semi-solid cast Mg-Al alloys[J]. J Light Met, 2002, 2: 277-280.
    • (2002) J Light Met , vol.2 , pp. 277-280
    • Kleiner, S.1    Beffort, O.2    Wahlen, A.3    Uggowitzer, P.J.4
  • 12
    • 0029734947 scopus 로고    scopus 로고
    • Recent developments in light alloys
    • POLMEAR I J. Recent developments in light alloys[J]. Mater Trans, JIM, 1996, 37: 12-31.
    • (1996) Mater Trans, JIM , vol.37 , pp. 12-31
    • Polmear, I.J.1
  • 13
    • 7244221735 scopus 로고    scopus 로고
    • Microstructural instability and strength of an AZ31 Mg alloy after severe plastic deformation
    • KIM H K, KIM W J. Microstructural instability and strength of an AZ31 Mg alloy after severe plastic deformation[J]. Mater Sci Eng A, 2004, A385: 300-308.
    • (2004) Mater Sci Eng A , vol.A385 , pp. 300-308
    • Kim, H.K.1    Kim, W.J.2
  • 14
    • 0033900777 scopus 로고    scopus 로고
    • Bulk nanostructured materials from severe plastic deformation
    • VALIEV R Z, ISLAMGALIEV R K, ALEXANDROV I V. Bulk nanostructured materials from severe plastic deformation[J]. Prog Mater Sci, 2000, 45: 103-189.
    • (2000) Prog Mater Sci , vol.45 , pp. 103-189
    • Valiev, R.Z.1    Islamgaliev, R.K.2    Alexandrov, I.V.3
  • 15
    • 0034301966 scopus 로고    scopus 로고
    • Microstructural evolution, microhardness and thermal stability of HPT-processed Cu
    • JIANG H, ZHU Y T, BUTT D P. Microstructural evolution, microhardness and thermal stability of HPT-processed Cu[J]. Mater Sci Eng A, 2000, A290: 128-138.
    • (2000) Mater Sci Eng A , vol.A290 , pp. 128-138
    • Jiang, H.1    Zhu, Y.T.2    Butt, D.P.3
  • 16
    • 1942466369 scopus 로고    scopus 로고
    • The dislocation structure evolution of deformation band and crack formation in a copper bicrystal with a perpendicular grain boundary
    • LI Y, LI S X, LI G Y. The dislocation structure evolution of deformation band and crack formation in a copper bicrystal with a perpendicular grain boundary[J]. Mater Sci Eng A, 2004, A372: 221-228.
    • (2004) Mater Sci Eng A , vol.A372 , pp. 221-228
    • Li, Y.1    Li, S.X.2    Li, G.Y.3
  • 17
    • 0033896728 scopus 로고    scopus 로고
    • Substructures and internal stress developed under warm severe deformation of austenitic stainless steel
    • BELYAKOV A, SAKAI T, MIURA H, KAIBYSHEV R. Substructures and internal stress developed under warm severe deformation of austenitic stainless steel[J]. Scripta Mater, 2000, 42: 319-325.
    • (2000) Scripta Mater , vol.42 , pp. 319-325
    • Belyakov, A.1    Sakai, T.2    Miura, H.3    Kaibyshev, R.4
  • 18
    • 0000141561 scopus 로고    scopus 로고
    • Grain refinement in copper under large strain deformation
    • BELYAKOV A, SAKAI T, MIURA H, TSUZAKI K. Grain refinement in copper under large strain deformation[J]. Philo Mag A, 2001, 18(11): 2629-2643.
    • (2001) Philo Mag A , vol.18 , Issue.11 , pp. 2629-2643
    • Belyakov, A.1    Sakai, T.2    Miura, H.3    Tsuzaki, K.4
  • 19
    • 0032295667 scopus 로고    scopus 로고
    • Strain-induced grain evolution in polycrystalline copper during warm deformation
    • BELYAKOV A, GAO W, MIURA H, SAKAI T. Strain-induced grain evolution in polycrystalline copper during warm deformation[J]. Metall Mater Trans A, 1998, 29A: 2957-2965.
    • (1998) Metall Mater Trans A , vol.29 A , pp. 2957-2965
    • Belyakov, A.1    Gao, W.2    Miura, H.3    Sakai, T.4
  • 20
    • 0037465013 scopus 로고    scopus 로고
    • The fracture behaviors in an Fe-Mn-Al alloy during quenching processes
    • CHENG W C, LIN Y C, LIU C F. The fracture behaviors in an Fe-Mn-Al alloy during quenching processes[J]. Mater Sci Eng A, 2003, A343: 28-35.
    • (2003) Mater Sci Eng A , vol.A343 , pp. 28-35
    • Cheng, W.C.1    Lin, Y.C.2    Liu, C.F.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.