Volumn 55, Issue 1, 2006, Pages 67-70

Impact resistance of PVD films and milling performance of coated tools at various temperature levels

Author keywords

Impact test; PVD coatings; Wear

Indexed keywords

CUTTING; FINITE ELEMENT METHOD; IMPACT RESISTANCE; IMPACT TESTING; MILLING (MACHINING); PHYSICAL VAPOR DEPOSITION; WEAR OF MATERIALS;

EID: 33750049068     PISSN: 00078506     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0007-8506(07)60368-0     Document Type: Article
Times cited : (26)

References (8)
  • 2
    • 0030242833 scopus 로고    scopus 로고
    • Indentation induced dislocation nucleation: The initial yield point
    • Gerberich, W.W., et. al. 1996, Indentation induced dislocation nucleation: the initial yield point, Acta metal, mater. 44/9:3585-3598.
    • (1996) Acta Metal, Mater. , vol.44 , Issue.9 , pp. 3585-3598
    • Gerberich, W.W.1
  • 5
    • 0035473161 scopus 로고    scopus 로고
    • Characterization of cohesion, adhesion and creep-properties of dynamically loaded coatings through the impact tester
    • Bouzakis, K.-D., et. al., 2001, Characterization of Cohesion, Adhesion and Creep-Properties of Dynamically Loaded Coatings through the Impact Tester, Zeitschrift fuer Metallkunde, 92:1180-1185.
    • (2001) Zeitschrift fuer Metallkunde , vol.92 , pp. 1180-1185
    • Bouzakis, K.-D.1
  • 6
    • 0035387366 scopus 로고    scopus 로고
    • Thin hard coatings stress-strain curves determination through a FEM supported evaluation of nanohardness results
    • Bouzakis, K.-D., et. al., G., 2001, Thin hard coatings stress-strain curves determination through a FEM supported evaluation of nanohardness results, Surface and Coatings Technology, 142-144:102-109.
    • (2001) Surface and Coatings Technology , vol.142-144 , pp. 102-109
    • Bouzakis, K.-D.1
  • 7
    • 0034498269 scopus 로고    scopus 로고
    • Mechanical behaviour of (Ti,Al)N coatings exposed to elevated temperatures and an oxidative environment
    • Schäffer, E., Kleer, G., 2000, Mechanical behaviour of (Ti,Al)N coatings exposed to elevated temperatures and an oxidative environment, Surface and Coatings Technology, 133-134:215-219.
    • (2000) Surface and Coatings Technology , vol.133-134 , pp. 215-219
    • Schäffer, E.1    Kleer, G.2
  • 8
    • 85030595391 scopus 로고    scopus 로고
    • Operational manual
    • DEFORM 3D
    • DEFORM 3D, Operational manual, DEFORM 2005.
    • DEFORM 2005


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.