1
-
-
0030674572
-
Binder removal from ceramics
-
J. A. Lewis, "Binder Removal from Ceramics," Annu. Rev. Mater. Sci., 27, 147-73 1997.
-
(1997)
Annu. Rev. Mater. Sci.
, vol.27
, pp. 147-173
-
-
Lewis, J.A.1
-
3
-
-
0032049941
-
Fabrication of microconfigured multi-component ceramics
-
A. T. Crumm and J. W. Halloran, "Fabrication of Microconfigured Multi-component Ceramics," J. Am. Ceram. Soc., 81 [4] 1053-7 (1998).
-
(1998)
J. Am. Ceram. Soc.
, vol.81
, Issue.4
, pp. 1053-1057
-
-
Crumm, A.T.1
Halloran, J.W.2
-
4
-
-
0348196878
-
Macrochanneled tetragonal zirconia polycrystals coated by a calcium phosphate layer
-
Y-H Koh, H-W Kim, H-E Kim, and J. W. Halloran, "Macrochanneled Tetragonal Zirconia Polycrystals Coated by a Calcium Phosphate Layer," J. Am. Ceram. Soc., 86 [12] 2027-30 (2003).
-
(2003)
J. Am. Ceram. Soc.
, vol.86
, Issue.12
, pp. 2027-2030
-
-
Koh, Y.-H.1
Kim, H.-W.2
Kim, H.-E.3
Halloran, J.W.4
-
6
-
-
0032093309
-
Chemistry of removal of ethylene vinyl acetate binders
-
K. E. Hrdina and J. W. Halloran, "Chemistry of Removal of Ethylene Vinyl Acetate Binders," J. Maler. Sci., 33, 2795-803 (1998).
-
(1998)
J. Maler. Sci.
, vol.33
, pp. 2795-2803
-
-
Hrdina, K.E.1
Halloran, J.W.2
-
7
-
-
0032089395
-
Dimensional changes during binder removal in a moldable ceramic system
-
K. E. Hrdina and J. W. Halloran, "Dimensional Changes During Binder Removal in a Moldable Ceramic System," J. Mater. Sci., 33, 2805-15 (1998).
-
(1998)
J. Mater. Sci.
, vol.33
, pp. 2805-2815
-
-
Hrdina, K.E.1
Halloran, J.W.2
-
8
-
-
0344549159
-
Mass diffusion-controlled bubbling and optimal schedule of thermal degradation of polymeric binder in molded powders
-
A. A. M. Oliveira, M. Kaviany, K. Hrdina, and J. Halloran, "Mass Diffusion-Controlled Bubbling and Optimal Schedule of Thermal Degradation of Polymeric Binder in Molded Powders," Int. J. Heal Mass Transfer, 42 [17] 3307-29 (1999).
-
(1999)
Int. J. Heal Mass Transfer
, vol.42
, Issue.17
, pp. 3307-3329
-
-
Oliveira, A.A.M.1
Kaviany, M.2
Hrdina, K.3
Halloran, J.4
-
9
-
-
0024754721
-
Degradation of polyolefin blends used for ceramic injection molding
-
J. K. Wright, J. R. F. Evans, and M. J. Edirisinghe, "Degradation of Polyolefin Blends Used for Ceramic Injection Molding," J. Am. Ceram. Soc., 72 [10] 1822-8 (1989).
-
(1989)
J. Am. Ceram. Soc.
, vol.72
, Issue.10
, pp. 1822-1828
-
-
Wright, J.K.1
Evans, J.R.F.2
Edirisinghe, M.J.3
-
10
-
-
33747586808
-
Determination of binder decomposition kinetics for specifying heating parameters in binder burnout cycles
-
R. V. Shende and S. J. Lombardo, "Determination of Binder Decomposition Kinetics for Specifying Heating Parameters in Binder Burnout Cycles," J. Am. Ceram. Soc., 81 [4] 1053-7 (1998).
-
(1998)
J. Am. Ceram. Soc.
, vol.81
, Issue.4
, pp. 1053-1057
-
-
Shende, R.V.1
Lombardo, S.J.2
-
11
-
-
0034319573
-
Role of length scale on pressure increase and yield of poly(vinyl butyral) barium titanate-platinum multilayer ceramic capacitors during binder burnout
-
L. C.-K. Liau, B. Peters, D. S. Krueger, A. Fordon, D. S. Viswanath, and S. J. Lombardo, "Role of Length Scale on Pressure Increase and Yield of Poly(Vinyl Butyral) Barium Titanate-Platinum Multilayer Ceramic Capacitors During Binder Burnout," J. Am. Ceram. Soc., 83 [11] 2645-53 (2000).
-
(2000)
J. Am. Ceram. Soc.
, vol.83
, Issue.11
, pp. 2645-2653
-
-
Liau, L.C.-K.1
Peters, B.2
Krueger, D.S.3
Fordon, A.4
Viswanath, D.S.5
Lombardo, S.J.6
-
12
-
-
0036883847
-
Thermal removal of multicomponent binder from ceramic injection mouldings
-
M. Trunec and J. Cihlar, "Thermal Removal of Multicomponent Binder from Ceramic Injection Mouldings," J. Eur. Ceram. Soc., 22, 2231-41 (2002).
-
(2002)
J. Eur. Ceram. Soc.
, vol.22
, pp. 2231-2241
-
-
Trunec, M.1
Cihlar, J.2
-
13
-
-
0024681102
-
Effects of oxides on binder burnout during ceramics processing
-
S. Masia, P. D. Calvert, W. E. Rhine, and H. K. Bowen, "Effects of Oxides on Binder Burnout During Ceramics Processing," J. Mater. Sci., 24 [6] 1907-12 (1989).
-
(1989)
J. Mater. Sci.
, vol.24
, Issue.6
, pp. 1907-1912
-
-
Masia, S.1
Calvert, P.D.2
Rhine, W.E.3
Bowen, H.K.4
-
14
-
-
28144446004
-
Thermoplastic green machining of textured dielectric substrate for broadband miniature antenna
-
Young-Hag Koh, John W. Halloran, Gullu Kiziltas, Dimitris Psychoudakis, and John Volakis, "Thermoplastic Green Machining of Textured Dielectric Substrate for Broadband Miniature Antenna," J. Am. Ceram. Soc., 88 [2] 297-302 (2005).
-
(2005)
J. Am. Ceram. Soc.
, vol.88
, Issue.2
, pp. 297-302
-
-
Koh, Y.-H.1
Halloran, J.W.2
Kiziltas, G.3
Psychoudakis, D.4
Volakis, J.5
-
15
-
-
0142063040
-
Topology design optimization of dielectric substrates for bandwidth improvement of a patch antenna
-
G. Kiziltas, D. Psychoudakis, J. L. Volakis, and N. Kikuchi, "Topology Design Optimization of Dielectric Substrates for Bandwidth Improvement of a Patch Antenna," IEEE Trans. Antennas Propagat., 51 [10] 2732-43 (2003).
-
(2003)
IEEE Trans. Antennas Propagat
, vol.51
, Issue.10
, pp. 2732-2743
-
-
Kiziltas, G.1
Psychoudakis, D.2
Volakis, J.L.3
Kikuchi, N.4
-
16
-
-
0041440205
-
Textured LTCC substrates for printed antenna miniaturization
-
Vol. 1.3, June
-
D. Psychoudakis, A. Knapp, G. Kiziltas, J. L. Volakis, and J. W. Halloran, "Textured LTCC Substrates for Printed Antenna Miniaturization"; Proceedings of the IEEE Soceity International Conference, Antennas and Propagation, Vol. 1.3, pp. 375-8, June 2003.
-
(2003)
Proceedings of the IEEE Soceity International Conference, Antennas and Propagation
, pp. 375-378
-
-
Psychoudakis, D.1
Knapp, A.2
Kiziltas, G.3
Volakis, J.L.4
Halloran, J.W.5
-
17
-
-
0029235356
-
A comparison of the thormal degradation behaviour of ethylene-ethyl acrylate copolymer, low density polyethylene and poly(ethyl acrylate)
-
I. C. McNeill and M. H. Mohammed, "A Comparison of the Thormal Degradation Behaviour of Ethylene-Ethyl Acrylate Copolymer, Low Density Polyethylene and Poly(Ethyl Acrylate)," Poly. Degrad. Stability, 48 [1] 175-87 1995.
-
(1995)
Poly. Degrad. Stability
, vol.48
, Issue.1
, pp. 175-187
-
-
McNeill, I.C.1
Mohammed, M.H.2
-
18
-
-
0034559823
-
The thermal degradation of poly(iso-butyl methacrylate) and poly(sec-butyl methacrylate)
-
K. Novaković, L. Katsikas, and I. G. Popović, "The Thermal Degradation of Poly(Iso-Butyl Methacrylate) and Poly(Sec-Butyl Methacrylate)," J. Serb. Chem. Soc., 65 [12] 867-75 (2000).
-
(2000)
J. Serb. Chem. Soc.
, vol.65
, Issue.12
, pp. 867-875
-
-
Novaković, K.1
Katsikas, L.2
Popović, I.G.3
-
19
-
-
0039015453
-
The thermal degradation of poly(ethylene glycol)/poly(vinyl alcohol) binder in alumina ceramics
-
K. J. Voorhees, S. F. Baugh, and D. N. Stevenson, "The Thermal Degradation of Poly(Ethylene Glycol)/Poly(Vinyl Alcohol) Binder in Alumina Ceramics," Therm. Acta, 274, 187-207.
-
Therm. Acta
, vol.274
, pp. 187-207
-
-
Voorhees, K.J.1
Baugh, S.F.2
Stevenson, D.N.3
|