메뉴 건너뛰기




Volumn 89, Issue 9, 2006, Pages 2869-2873

Interface properties in a porous-matrix oxide composite

Author keywords

[No Author keywords available]

Indexed keywords

ELASTIC DEFORMATION; GLASS-CERAMIC MATRICES; POROUS-MATRIX OXIDE COMPOSITE; UNCOATED FIBERS;

EID: 33747604852     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2006.01162.x     Document Type: Article
Times cited : (13)

References (21)
  • 1
    • 0030084731 scopus 로고    scopus 로고
    • Concept for a damage-tolerant ceramic composite with strong interfaces
    • W. C. Tu, F. F. Lange, and A. G. Evans, "Concept for a Damage-Tolerant Ceramic Composite with Strong Interfaces," J. Am. Ceram. Soc., 79 [2] 417-24 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.2 , pp. 417-424
    • Tu, W.C.1    Lange, F.F.2    Evans, A.G.3
  • 2
    • 0032139153 scopus 로고    scopus 로고
    • Processing and performance of an all-oxide ceramic composite
    • C. G. Levi, J. Y. Yang, B. J. Dalgleish, F. W. Zok, and A. G. Evans, "Processing and Performance of an All-Oxide Ceramic Composite," J. Am. Ceram. Soc., 81 [8] 2077-86 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.8 , pp. 2077-2086
    • Levi, C.G.1    Yang, J.Y.2    Dalgleish, B.J.3    Zok, F.W.4    Evans, A.G.5
  • 3
    • 0033225105 scopus 로고    scopus 로고
    • Notched fracture behavior of an oxide/oxide ceramic-matrix composite
    • V. A. Kramb, R. John, and L. P. Zawada, "Notched Fracture Behavior of an Oxide/Oxide Ceramic-Matrix Composite," J. Am. Ceram. Soc., 82 [11] 3087-96 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.11 , pp. 3087-3096
    • Kramb, V.A.1    John, R.2    Zawada, L.P.3
  • 4
    • 0033204919 scopus 로고    scopus 로고
    • In-plane mechanical properties of an all-oxide ceramic composite
    • J. A. Heathcote, X.-Y. Gong, J. Yang, U. Ramamurty, and F. W. Zok, "In-Plane Mechanical Properties of an All-Oxide Ceramic Composite," J. Am. Ceram. Soc., 82 [10] 2721-30 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.10 , pp. 2721-2730
    • Heathcote, J.A.1    Gong, X.-Y.2    Yang, J.3    Ramamurty, U.4    Zok, F.W.5
  • 5
    • 0033322666 scopus 로고    scopus 로고
    • Microstructural design of stable porous matrices for all-oxide ceramic composites
    • C. G. Levi, F. W. Zok, J.-Y. Yang, M. Mattoni, and J. P. A. Lofvander, "Microstructural Design of Stable Porous Matrices for All-Oxide Ceramic Composites," Z. Metallkd., 90 [12] 1037-47 (1999).
    • (1999) Z. Metallkd. , vol.90 , Issue.12 , pp. 1037-1047
    • Levi, C.G.1    Zok, F.W.2    Yang, J.-Y.3    Mattoni, M.4    Lofvander, J.P.A.5
  • 6
    • 0033859284 scopus 로고    scopus 로고
    • Advances in oxide-oxide CMC
    • S. C. Jurf and R. A. Butner, "Advances in Oxide-Oxide CMC," J. Eng. Gas Turb. Power, 122 [2] 202-5 (2000).
    • (2000) J. Eng. Gas Turb. Power , vol.122 , Issue.2 , pp. 202-205
    • Jurf, S.C.1    Butner, R.A.2
  • 7
    • 0033996724 scopus 로고    scopus 로고
    • Aluminosilicate fiber/mullite mullile composites with favorable high-temperature properties
    • B. Kanka and H. Schneider, "Aluminosilicate Fiber/Mullite Mullile Composites with Favorable High-Temperature Properties," J. Eur. Ceram. Soc., 20 [14-15] 619-23 (2000).
    • (2000) J. Eur. Ceram. Soc. , vol.20 , Issue.14-15 , pp. 619-623
    • Kanka, B.1    Schneider, H.2
  • 8
    • 0035421062 scopus 로고    scopus 로고
    • A study of the damage progression from notches in an oxide/oxide ceramic-matrix composite using ultrasonic C-scans
    • V. A. Kramb, R. John, and D. A. Stubbs, "A Study of the Damage Progression from Notches in an Oxide/Oxide Ceramic-Matrix Composite Using Ultrasonic C-Scans," Comp. Sci. Technol., 61 [11] 1561-70 (2001).
    • (2001) Comp. Sci. Technol. , vol.61 , Issue.11 , pp. 1561-1570
    • Kramb, V.A.1    John, R.2    Stubbs, D.A.3
  • 9
    • 0035526636 scopus 로고    scopus 로고
    • Effects of matrix porosity on the mechanical properties of a porous-matrix, all-oxide ceramic composite
    • M. Mattoni, J. Y. Yang, C. G. Levi, and F. W. Zok, "Effects of Matrix Porosity on the Mechanical Properties of a Porous-Matrix, All-Oxide Ceramic Composite," J. Am. Ceram. Soc., 84 [11] 2594-602 (2001).
    • (2001) J. Am. Ceram. Soc. , vol.84 , Issue.11 , pp. 2594-2602
    • Mattoni, M.1    Yang, J.Y.2    Levi, C.G.3    Zok, F.W.4
  • 10
    • 27644509547 scopus 로고    scopus 로고
    • Strength and notch sensitivity of porous-matrix oxide composites
    • M. A. Mattoni and F. W. Zok, "Strength and Notch Sensitivity of Porous-Matrix Oxide Composites," J. Am. Ceram. Soc., 88 [6] 1504-13 (2005).
    • (2005) J. Am. Ceram. Soc. , vol.88 , Issue.6 , pp. 1504-1513
    • Mattoni, M.A.1    Zok, F.W.2
  • 12
    • 1542305548 scopus 로고    scopus 로고
    • Mullite-alumina mixtures for use as porous matrices in oxide fiber composites
    • H. Fujita, G. Jefferson, R. M. McMeeking, and F. W. Zok, "Mullite-Alumina Mixtures for Use as Porous Matrices in Oxide Fiber Composites," J. Am. Ceram. Soc., 87 [2] 261-7 (2004).
    • (2004) J. Am. Ceram. Soc. , vol.87 , Issue.2 , pp. 261-267
    • Fujita, H.1    Jefferson, G.2    McMeeking, R.M.3    Zok, F.W.4
  • 13
    • 27644441785 scopus 로고    scopus 로고
    • Controlling mechanical properties of porous mullite/alumina mixtures via precursor-derived alumina
    • H. Fujita, G. Jefferson, C. G. Levi, and F. W. Zok, "Controlling Mechanical Properties of Porous Mullite/Alumina Mixtures Via Precursor-Derived Alumina," J. Am. Ceram. Soc., 88 [2] 367-75 (2005).
    • (2005) J. Am. Ceram. Soc. , vol.88 , Issue.2 , pp. 367-375
    • Fujita, H.1    Jefferson, G.2    Levi, C.G.3    Zok, F.W.4
  • 14
    • 0023399385 scopus 로고
    • Measurement of interfacial mechanical properties in fiber-reinforced ceramic composites
    • D. B. Marshall and W. C. Oliver, "Measurement of Interfacial Mechanical Properties in Fiber-Reinforced Ceramic Composites," J. Am. Ceram. Soc., 70 [8] 542-8 (1987).
    • (1987) J. Am. Ceram. Soc. , vol.70 , Issue.8 , pp. 542-548
    • Marshall, D.B.1    Oliver, W.C.2
  • 15
    • 0026134355 scopus 로고
    • Experimental examination of the push-down technique for measuring the sliding resistance of silicon carbide fibers in a ceramic matrix
    • T. P. Weihs and W. D. Nix, "Experimental Examination of the Push-Down Technique for Measuring the Sliding Resistance of Silicon Carbide Fibers in a Ceramic Matrix," J. Am. Ceram. Soc., 74 [3] 524-34 (1991).
    • (1991) J. Am. Ceram. Soc. , vol.74 , Issue.3 , pp. 524-534
    • Weihs, T.P.1    Nix, W.D.2
  • 16
    • 0031140724 scopus 로고    scopus 로고
    • Statistical tensile strength of nextel 610 and nextel 720 fibres
    • D. M. Wilson, "Statistical Tensile Strength of Nextel 610 and Nextel 720 Fibres," J. Mater. Sci., 32 [10] 2535-42 (1997).
    • (1997) J. Mater. Sci. , vol.32 , Issue.10 , pp. 2535-2542
    • Wilson, D.M.1
  • 17
    • 0001032417 scopus 로고
    • Packing density of composite powder mixtures
    • F. W. Zok, F. F. Lange, and J. R. Porter, "Packing Density of Composite Powder Mixtures," J. Am. Ceram. Soc., 74 [8] 1880-5 (1991).
    • (1991) J. Am. Ceram. Soc. , vol.74 , Issue.8 , pp. 1880-1885
    • Zok, F.W.1    Lange, F.F.2    Porter, J.R.3
  • 18
    • 0024884622 scopus 로고
    • Crack deflection at an interface between dissimilar elastic materials
    • M.-Y. He and J. W. Hutchinson, "Crack Deflection at an Interface Between Dissimilar Elastic Materials," Int. J. Solids Struct., 25 [9] 1053-67 (1989).
    • (1989) Int. J. Solids Struct. , vol.25 , Issue.9 , pp. 1053-1067
    • He, M.-Y.1    Hutchinson, J.W.2
  • 19
    • 85040875608 scopus 로고
    • Cambridge University Press, Cambridge, U.K.
    • K. L. Johnson, Contact Mechanics. Cambridge University Press, Cambridge, U.K., 1985.
    • (1985) Contact Mechanics
    • Johnson, K.L.1
  • 21
    • 33747619227 scopus 로고    scopus 로고
    • Nanoindentation with spherical indenters: Finite element studies of deformation in the elastic-plastic transition regime
    • Y. J. Park and G. M. Pharr, "Nanoindentation with Spherical Indenters: Finite Element Studies of Deformation in the Elastic-Plastic Transition Regime," Thin Solid Films, 246, 447-8 (2004).
    • (2004) Thin Solid Films , vol.246 , pp. 447-448
    • Park, Y.J.1    Pharr, G.M.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.