Volumn 21, Issue 1, 2006, Pages 49-73

Laser surface modification of Ti-6Al-4V: Wear and corrosion characterization in simulated biofluid

Author keywords

Anodic polarization; Corrosion; Laser surface treatment; Microstructure; Ringer's solution; Ti 6Al 4V; Wear corrosion

Indexed keywords

ANODIC POLARIZATION; CHARACTERIZATION; CORROSION; LASER APPLICATIONS; METALLOGRAPHIC MICROSTRUCTURE; SURFACE TREATMENT; WEAR OF MATERIALS; WEAR RESISTANCE;

EID: 33746403800     PISSN: 08853282     EISSN: 15308022     Source Type: Journal    
DOI: 10.1177/0885328206055998     Document Type: Article
Times cited : (71)

References (38)
  • 1
    • 0033492058 scopus 로고    scopus 로고
    • Tribological Behavior of Alumina Sliding against Ti-6Al-4V in Unlubricated Contact
    • Dong, H. and Bell, T. (1999). Tribological Behavior of Alumina Sliding against Ti-6Al-4V in Unlubricated Contact, Wear, 225-229 (2): 874-884.
    • (1999) Wear , vol.225-229 , Issue.2 , pp. 874-884
    • Dong, H.1    Bell, T.2
  • 2
    • 1242272814 scopus 로고    scopus 로고
    • Effect of Thermal Oxidation on Corrosion and Corrosion Wear Behavior of a Ti-6Al-4V Alloy
    • Guleryuz, H. and Cimenoglu, H. (2004). Effect of Thermal Oxidation on Corrosion and Corrosion Wear Behavior of a Ti-6Al-4V Alloy, Biomaterials, 25 (16): 3325-3333.
    • (2004) Biomaterials , vol.25 , Issue.16 , pp. 3325-3333
    • Guleryuz, H.1    Cimenoglu, H.2
  • 3
    • 0043023458 scopus 로고    scopus 로고
    • Friction and Wear Characteristics of Various Prosthetic Materials Sliding against Smooth Diamond-coated Titanium Alloy
    • Met, C., Vandenbulcke, L. and Catherrine, M.C.S. (2003). Friction and Wear Characteristics of Various Prosthetic Materials Sliding against Smooth Diamond-coated Titanium Alloy, Wear, 255 (7-12): 1022-1029.
    • (2003) Wear , vol.255 , Issue.7-12 , pp. 1022-1029
    • Met, C.1    Vandenbulcke, L.2    Catherrine, M.C.S.3
  • 4
    • 0032846283 scopus 로고    scopus 로고
    • In vivo Metallic Biomaterials and Surface Modification
    • Hanawa, T. (1999). In vivo Metallic Biomaterials and Surface Modification, Mater. Sci. & Eng., A267 (2): A260-A266.
    • (1999) Mater. Sci. & Eng. , vol.A267 , Issue.2
    • Hanawa, T.1
  • 5
    • 0028450061 scopus 로고
    • Electrochemical Studies of Laser-treated Co-Cr-Mo Alloy in a Simulated Physiological Solution
    • Silva, R.A., Barbosa, M.A., Vilar, R., Conde, O., Cunha, M. and Sutherland, I. (1994). Electrochemical Studies of Laser-treated Co-Cr-Mo Alloy in a Simulated Physiological Solution, J. Mater. Sci. Mater. Med., 5 (4): 353-356.
    • (1994) J. Mater. Sci. Mater. Med. , vol.5 , Issue.4 , pp. 353-356
    • Silva, R.A.1    Barbosa, M.A.2    Vilar, R.3    Conde, O.4    Cunha, M.5    Sutherland, I.6
  • 8
    • 0032144923 scopus 로고    scopus 로고
    • Corrosion Properties of TiN Prepared by Laser Gas Alloying of Ti and Ti6Al4V
    • Gracia, I. and Damborenea, J.D. (1998). Corrosion Properties of TiN Prepared by Laser Gas Alloying of Ti and Ti6Al4V, Corros. Sci., 40 (8): 1411-1419.
    • (1998) Corros. Sci. , vol.40 , Issue.8 , pp. 1411-1419
    • Gracia, I.1    Damborenea, J.D.2
  • 9
    • 0033881352 scopus 로고    scopus 로고
    • The Effects of Laser Surface Treatment on the Corrosion Properties of Ti-6Al-4V Alloy in Hank's Solution
    • Yue, T.M., Cheung, T.M. and Man, H.C. (2000). The Effects of Laser Surface Treatment on the Corrosion Properties of Ti-6Al-4V Alloy in Hank's Solution, J. Mater. Sci. Lett., 19 (3): 205-208.
    • (2000) J. Mater. Sci. Lett. , vol.19 , Issue.3 , pp. 205-208
    • Yue, T.M.1    Cheung, T.M.2    Man, H.C.3
  • 10
    • 0036132091 scopus 로고    scopus 로고
    • Excimer Laser Surface Treatment of Ti-6Al-4V Alloy for Corrosion Resistance Enhancement
    • Yue, T.M., Yu, J.K., Mei, Z. and Man, H.C. (2002). Excimer Laser Surface Treatment of Ti-6Al-4V Alloy for Corrosion Resistance Enhancement, Mater. Lett., 52 (3): 206-212.
    • (2002) Mater. Lett , vol.52 , Issue.3 , pp. 206-212
    • Yue, T.M.1    Yu, J.K.2    Mei, Z.3    Man, H.C.4
  • 11
    • 0037465941 scopus 로고    scopus 로고
    • Effects of Laser Surface Remelting on the Corrosion Behavior of Commercially Pure Titanium Sheet
    • Sun, Z., Annergren, I., Pan, D. and Mai, T.A. (2003). Effects of Laser Surface Remelting on the Corrosion Behavior of Commercially Pure Titanium Sheet, Mater. Sci. Eng., A345 (1-2): 293-300.
    • (2003) Mater. Sci. Eng. , vol.A345 , Issue.1-2 , pp. 293-300
    • Sun, Z.1    Annergren, I.2    Pan, D.3    Mai, T.A.4
  • 12
    • 0033930431 scopus 로고    scopus 로고
    • Wear Resistance of a Laser Surface Alloyed Ti6Al4V Alloy
    • Jiang, P., He, X.L., Li, X.X., Yu, L.G. and Wang, H.M. (2000). Wear Resistance of a Laser Surface Alloyed Ti6Al4V Alloy, Surf. Coat. Technol., 130 (1): 24-28.
    • (2000) Surf. Coat. Technol. , vol.130 , Issue.1 , pp. 24-28
    • Jiang, P.1    He, X.L.2    Li, X.X.3    Yu, L.G.4    Wang, H.M.5
  • 13
    • 0344330602 scopus 로고    scopus 로고
    • Wear Measurements
    • In: Henry, S.D. (ed.) Lubrication and Wear Technology, Materials Park, Ohio, USA
    • Ruff, A.W. (1998). Wear Measurements, In: Henry, S.D. (ed.), ASM Handbook on Friction, Vol. 18, pp. 362-369, Lubrication and Wear Technology, Materials Park, Ohio, USA.
    • (1998) ASM Handbook on Friction , vol.18 , pp. 362-369
    • Ruff, A.W.1
  • 15
    • 33746405338 scopus 로고
    • Melting and Alloying of Steel with Chromium
    • 2 Laser) Michigan State University, East Lansing, Michigan, USA
    • 2 Laser) Melting and Alloying of Steel with Chromium, Michigan State University, East Lansing, Michigan, USA, pp. 83-86.
    • (1987) , pp. 83-86
    • Dahotre, N.B.1
  • 16
    • 0033349559 scopus 로고    scopus 로고
    • Laser Welding of Thin Sheet Steel with Surface Oxidation
    • Xie, J. and Kar, A. (1999). Laser Welding of Thin Sheet Steel with Surface Oxidation, Welding Research Supplement, 343S-348S.
    • (1999) Welding Research Supplement
    • Xie, J.1    Kar, A.2
  • 17
    • 0021439542 scopus 로고
    • Damage in Aluminum, Zinc and Tin from a Nanosecond Electric Pulse Discharge
    • Wakade, C.G., Dahotre, N.B. and Mukherjee, K. (1984). Damage in Aluminum, Zinc and Tin from a Nanosecond Electric Pulse Discharge, Mater. Sci. & Eng., 64: 247-254.
    • (1984) Mater. Sci. & Eng. , vol.64 , pp. 247-254
    • Wakade, C.G.1    Dahotre, N.B.2    Mukherjee, K.3
  • 18
    • 0015489462 scopus 로고
    • The Influence of Grain Boundaries on Mechanical Properties
    • Hirth, J.P. (1972). The Influence of Grain Boundaries on Mechanical Properties, Metall. Trans., 3 (10): 3047-3067.
    • (1972) Metall. Trans. , vol.3 , Issue.10 , pp. 3047-3067
    • Hirth, J.P.1
  • 19
    • 33746396765 scopus 로고
    • Influence of Grain Size on the Constitutive Response and Substructure Evolution of MONEL 400
    • Gray, G.T., Rong, Shuh C. and Vecchio, S.K. (1972). Influence of Grain Size on the Constitutive Response and Substructure Evolution of MONEL 400, Metall. Trans., 3A (4): 1235-1247.
    • (1972) Metall. Trans , vol.3 A , Issue.4 , pp. 1235-1247
    • Gray, G.T.1    Rong Shuh, C.2    Vecchio, S.K.3
  • 20
    • 24944541844 scopus 로고    scopus 로고
    • Influence of Laser Surface Modification on Corrosion Behavior of Stainless Steel 316L and Ti6Al4V Alloy in Simulated Body Fluid
    • Singh, R., Martin, M. and Dahotre, N.B. (2005). Influence of Laser Surface Modification on Corrosion Behavior of Stainless Steel 316L and Ti6Al4V Alloy in Simulated Body Fluid, Surf. Eng., 21: 297-306.
    • (2005) Surf. Eng. , vol.21 , pp. 297-306
    • Singh, R.1    Martin, M.2    Dahotre, N.B.3
  • 21
    • 0032173185 scopus 로고    scopus 로고
    • Depth Distributions and Anodic Polarization Behavior of Ion Implanted Ti-6Al-4V
    • Schmidt, H., Stechemesser, G., Witte, J. and Soltani-Farshi, M. (1998). Depth Distributions and Anodic Polarization Behavior of Ion Implanted Ti-6Al-4V, Corros. Sci., 40 (9): 1533-1545.
    • (1998) Corros. Sci , vol.40 , Issue.9 , pp. 1533-1545
    • Schmidt, H.1    Stechemesser, G.2    Witte, J.3    Soltani-Farshi, M.4
  • 22
    • 0037788185 scopus 로고    scopus 로고
    • The Influence of Niobium and Vanadium on Passivity of Titanium-based Implants in Physiological Solution
    • Metiko, M., Hukovic, S., Kwokal, A. and Piljac, J. (2003). The Influence of Niobium and Vanadium on Passivity of Titanium-based Implants in Physiological Solution, Biomaterials, 24 (21): 3765-3775.
    • (2003) Biomaterials , vol.24 , Issue.21 , pp. 3765-3775
    • Metiko, M.1    Hukovic, S.2    Kwokal, A.3    Piljac, J.4
  • 23
    • 0028517697 scopus 로고
    • The Passivity and Electrochemistry of a Ti-15V-3Cr-3Al Titanium Alloy in Ambient Temperature Aqueous Sodium Chloride Solutions
    • Kolman, D.G. and Scully, J.R. (1994). The Passivity and Electrochemistry of a Ti-15V-3Cr-3Al Titanium Alloy in Ambient Temperature Aqueous Sodium Chloride Solutions, J. Electrochem. Soc., 141 (10): 2633-2641.
    • (1994) J. Electrochem. Soc. , vol.141 , Issue.10 , pp. 2633-2641
    • Kolman, D.G.1    Scully, J.R.2
  • 24
    • 0023435633 scopus 로고
    • Surface and Interface Characterization of Heat-Treated (Ti, Al)N Coatings on High Speed Steel Substrates
    • John, H.A., Hofmann, S. and Muknz, W.-D. (1987). Surface and Interface Characterization of Heat-Treated (Ti, Al)N Coatings on High Speed Steel Substrates, Thin Solid Films, 153 (1-3): 45-53.
    • (1987) Thin Solid Films , vol.153 , Issue.1-3 , pp. 45-53
    • John, H.A.1    Hofmann, S.2    Muknz, W.-D.3
  • 25
    • 0242607121 scopus 로고    scopus 로고
    • The Electrochemical and Mechanical Behavior of Passivated and TiN/ AlN-coated Co-Cr-Mo and Ti-6Al-4V Alloys
    • Goldberg, J.R. and Gilbert, J.L. (2004). The Electrochemical and Mechanical Behavior of Passivated and TiN/AlN-coated Co-Cr-Mo and Ti-6Al-4V Alloys, Biomaterials, 25 (5): 851-864.
    • (2004) Biomaterials , vol.25 , Issue.5 , pp. 851-864
    • Goldberg, J.R.1    Gilbert, J.L.2
  • 26
    • 0004034927 scopus 로고
    • McGraw-Hill Co., Singapore
    • Fontana, M.G. (1987). Corrosion Engineering, pp. 505-519, McGraw-Hill Co., Singapore.
    • (1987) Corrosion Engineering , pp. 505-519
    • Fontana, M.G.1
  • 29
    • 33746412631 scopus 로고    scopus 로고
    • Laser Surface Processing
    • In: Henry, S.D. (ed.) Materials Park, Ohio, USA
    • Cooper, K.P. (1998). Laser Surface Processing, In: Henry, S.D. (ed.), Friction, Lubrication and Wear Technology, ASM Handbook, Vol. 18, p. 862, Materials Park, Ohio, USA.
    • (1998) Friction, Lubrication and Wear Technology, ASM Handbook , vol.18 , pp. 862
    • Cooper, K.P.1
  • 30
    • 0024591990 scopus 로고
    • Optimizing Ion Implantation Conditions for Improving Wear, Fatigue, and Fretting Fatigue of Ti6Al4V
    • Elder, J.E., Thamburaj, R. and Patnaik, P.C. (1989). Optimizing Ion Implantation Conditions for Improving Wear, Fatigue, and Fretting Fatigue of Ti6Al4V, Surface Eng., 5 (1): 55-78.
    • (1989) Surface Eng. , vol.5 , Issue.1 , pp. 55-78
    • Elder, J.E.1    Thamburaj, R.2    Patnaik, P.C.3
  • 31
    • 0000825105 scopus 로고
    • Surface Engineering of Titanium and Titanium Alloys
    • In: Materials Park, Ohio, USA
    • Bloyce, A., Morton, P.H. and Bell, T. (1994). Surface Engineering of Titanium and Titanium Alloys, In: ASM Handbook on Surface Engineering, Vol. 5, pp. 835-851, Materials Park, Ohio, USA.
    • (1994) ASM Handbook on Surface Engineering , vol.5 , pp. 835-851
    • Bloyce, A.1    Morton, P.H.2    Bell, T.3
  • 32
    • 0019482182 scopus 로고
    • An Electrochemical Polarization Technique for Evaluation of Wear-corrosion in Moving Components under Stress
    • In: Ludema, I.C.C. (ed.) San Francisco, CA, ASME, New York
    • Kim, K.Y., Bhattacharyya, S. and Agarwal, V. (1981). An Electrochemical Polarization Technique for Evaluation of Wear-corrosion in Moving Components under Stress, In: Ludema, I.C.C. (ed.), Wear of Materials, pp. 772-778, San Francisco, CA, ASME, New York.
    • (1981) Wear of Materials , pp. 772-778
    • Kim, K.Y.1    Bhattacharyya, S.2    Agarwal, V.3
  • 33
    • 1642278756 scopus 로고    scopus 로고
    • Third Body Effects and Material Fluxes in Tribocorrosion Systems Involving a Sliding Contact
    • Landolt, D., Mischler, S., Stemp, M. and Barril, S. (2004). Third Body Effects and Material Fluxes in Tribocorrosion Systems Involving a Sliding Contact, Wear, 256 (5): 517-524.
    • (2004) Wear , vol.256 , Issue.5 , pp. 517-524
    • Landolt, D.1    Mischler, S.2    Stemp, M.3    Barril, S.4
  • 34
    • 0033332224 scopus 로고    scopus 로고
    • Fretting Corrosion of Materials for Orthopaedic Implants: A Study of a Metal/Polymer Contact in an Artificial Physiological Medium
    • Tritschler, B., Forest, B. and Rieu, J. (1999). Fretting Corrosion of Materials for Orthopaedic Implants: A Study of a Metal/Polymer Contact in an Artificial Physiological Medium, Tribol. Int., 32 (10): 587-596.
    • (1999) Tribol. Int. , vol.32 , Issue.10 , pp. 587-596
    • Tritschler, B.1    Forest, B.2    Rieu, J.3
  • 35
    • 0041568339 scopus 로고    scopus 로고
    • Mapping Sliding Wear of Steels in Aqueous Conditions
    • Stack, M.M. and Chi, K. (2003). Mapping Sliding Wear of Steels in Aqueous Conditions, Wear, 255 (1-6): 456-465.
    • (2003) Wear , vol.255 , Issue.1-6 , pp. 456-465
    • Stack, M.M.1    Chi, K.2
  • 36
    • 0002381317 scopus 로고    scopus 로고
    • Friction and Wear of Titanium Alloys
    • In: Henry, S.D. (ed.) Materials Park, Ohio, USA
    • Kustas, F.M. and Mishra, M.S. (1998). Friction and Wear of Titanium Alloys, In: Henry, S.D. (ed.), Friction, Lubrication and Wear Technology, ASM Handbook, Vol. 18, p. 778, Materials Park, Ohio, USA.
    • (1998) Friction, Lubrication and Wear Technology, ASM Handbook , vol.18 , pp. 778
    • Kustas, F.M.1    Mishra, M.S.2
  • 37
    • 0036957512 scopus 로고    scopus 로고
    • Wear-corrosion Mechanism of Hard Chromium Coatings
    • Fedrizzi, L., Rossi, S., Bellei, F. and Deflorian, F. (2002). Wear-corrosion Mechanism of Hard Chromium Coatings, Wear, 253 (11-12): 1173-1181.
    • (2002) Wear , vol.253 , Issue.11-12 , pp. 1173-1181
    • Fedrizzi, L.1    Rossi, S.2    Bellei, F.3    Deflorian, F.4
  • 38
    • 29244469616 scopus 로고    scopus 로고
    • Transfer of 319 Al Alloy to Titanium Diboride and Titanium Nitride based (TiAlN, TiCN, TiN) Coatings: Effects of Sliding Speed, Temperature and Environment
    • Konca, E., Cheng, Y.-T., Weiner, A.M., Dasch, J.M., Erdemir, A. and Alpas, A.T. (2005). Transfer of 319 Al Alloy to Titanium Diboride and Titanium Nitride based (TiAlN, TiCN, TiN) Coatings: Effects of Sliding Speed, Temperature and Environment, Surf. & Coat. Tech., 200: 2260-2270.
    • (2005) Surf. & Coat. Tech. , vol.200 , pp. 2260-2270
    • Konca, E.1    Cheng, Y.-T.2    Weiner, A.M.3    Dasch, J.M.4    Erdemir, A.5    Alpas, A.T.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.