-
1
-
-
8744300756
-
The mechanism of the high-temperature oxidation of iron-chromium alloys in water vapor
-
Fujii C.T., and Meussner R.A. The mechanism of the high-temperature oxidation of iron-chromium alloys in water vapor. J. Electrochem. Soc. 111 (1964) 1215
-
(1964)
J. Electrochem. Soc.
, vol.111
, pp. 1215
-
-
Fujii, C.T.1
Meussner, R.A.2
-
2
-
-
0002086438
-
Effects of water vapour on oxide growth on 304 stainless steel at 900 °C
-
Institute of Materials, London, UK
-
Khanna A.S., and Kofstad P. Effects of water vapour on oxide growth on 304 stainless steel at 900 °C. Proceedings of the International Conference on Microscopy of Oxidation, Cambridge, UK (1990), Institute of Materials, London, UK 113-118
-
(1990)
Proceedings of the International Conference on Microscopy of Oxidation, Cambridge, UK
, pp. 113-118
-
-
Khanna, A.S.1
Kofstad, P.2
-
4
-
-
0035178020
-
Microstructure of oxidised 304L steel and the effects of surface roughness on oxidation behaviour
-
Tang J.E., Halvarsson M., Asteman H., and Svensson J.-E. Microstructure of oxidised 304L steel and the effects of surface roughness on oxidation behaviour. Materials Science Forum 369-372 (2001) 205-214
-
(2001)
Materials Science Forum
, vol.369-372
, pp. 205-214
-
-
Tang, J.E.1
Halvarsson, M.2
Asteman, H.3
Svensson, J.-E.4
-
5
-
-
0003823494
-
Oxidation of alloys: II. Formation of external scales and overall oxidation behaviour
-
Elsevier Applied Science, London and New York
-
Kofstad P. Oxidation of alloys: II. Formation of external scales and overall oxidation behaviour. High Temperature Corrosion (1988), Elsevier Applied Science, London and New York 382-385
-
(1988)
High Temperature Corrosion
, pp. 382-385
-
-
Kofstad, P.1
-
6
-
-
0025596516
-
A SIMS study of reactions in the metal-oxygen-hydrogen-water system
-
Hultquist G., Chuah G.K., and Tan K.L. A SIMS study of reactions in the metal-oxygen-hydrogen-water system. Corrosion Science 31 (1990) 149-154
-
(1990)
Corrosion Science
, vol.31
, pp. 149-154
-
-
Hultquist, G.1
Chuah, G.K.2
Tan, K.L.3
-
7
-
-
0028463038
-
3. Part II high temperatures (<1000 °C)
-
3. Part II high temperatures (<1000 °C). Solid State Ionics 69 (1994) 137-143
-
(1994)
Solid State Ionics
, vol.69
, pp. 137-143
-
-
Holt, A.1
Kofstad, P.2
-
8
-
-
33746353498
-
High temperature corrosion of pure nickel and Ni-Cr, Fe-Ni-Cr or Co-Cr-W-Ni alloys-influence of water vapour contents
-
Kirman, et al. (Ed), The Metals Society, London 266, 423-434
-
Armanet F., Vejux A., and Beranger G. High temperature corrosion of pure nickel and Ni-Cr, Fe-Ni-Cr or Co-Cr-W-Ni alloys-influence of water vapour contents. In: Kirman, et al. (Ed). Proceedings of the Behaviour of High-Temperature Alloys in Aggressive Environments, Petten, Holland (1980), The Metals Society, London 266, 423-434
-
(1980)
Proceedings of the Behaviour of High-Temperature Alloys in Aggressive Environments, Petten, Holland
-
-
Armanet, F.1
Vejux, A.2
Beranger, G.3
-
9
-
-
0035184376
-
Abnormal oxidation of stabilized ferritic stainless steels in water vapor
-
Henry S., Galerie A., and Antoni L. Abnormal oxidation of stabilized ferritic stainless steels in water vapor. Materials Science Forum 369-372 (2001) 353-360
-
(2001)
Materials Science Forum
, vol.369-372
, pp. 353-360
-
-
Henry, S.1
Galerie, A.2
Antoni, L.3
-
10
-
-
0031248718
-
High-temperature oxidation of Fe-Cr alloys in wet oxygen
-
Jianian S., Longjiang Z., and Tiefan L. High-temperature oxidation of Fe-Cr alloys in wet oxygen. Oxidation of Metals 48 (1997) 347-356
-
(1997)
Oxidation of Metals
, vol.48
, pp. 347-356
-
-
Jianian, S.1
Longjiang, Z.2
Tiefan, L.3
-
11
-
-
0017427711
-
High-temperature oxidation of Fe-13%Cr-Al alloys in air/water vapour mixtures
-
Kvernes I., Oliveira M., and Kofstad P. High-temperature oxidation of Fe-13%Cr-Al alloys in air/water vapour mixtures. Corrosion Science 17 (1977) 237-252
-
(1977)
Corrosion Science
, vol.17
, pp. 237-252
-
-
Kvernes, I.1
Oliveira, M.2
Kofstad, P.3
-
12
-
-
0032625652
-
Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873 K in the presence of 10% water vapor
-
Asteman H., Svensson J.-E., Johansson L.-G., and Norell M. Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873 K in the presence of 10% water vapor. Oxidation of Metals 52 1/2 (1999) 95-111
-
(1999)
Oxidation of Metals
, vol.52
, Issue.1-2
, pp. 95-111
-
-
Asteman, H.1
Svensson, J.-E.2
Johansson, L.-G.3
Norell, M.4
-
13
-
-
0034247310
-
Influence of water vapor and flow rate on the high-temperature oxidation of 304L; effect of chromium oxide hydroxide evaporation
-
Asteman H., Svensson J.-E., Norell M., and Johansson L.-G. Influence of water vapor and flow rate on the high-temperature oxidation of 304L; effect of chromium oxide hydroxide evaporation. Oxidation of Metals 54 1/2 (2000) 11-26
-
(2000)
Oxidation of Metals
, vol.54
, Issue.1-2
, pp. 11-26
-
-
Asteman, H.1
Svensson, J.-E.2
Norell, M.3
Johansson, L.-G.4
-
15
-
-
0026821399
-
Diffusion of cations in chromia layers grown on iron-base alloys
-
Lobnig R.E., Schmidt H.P., Hennesen K., and Grabke H.J. Diffusion of cations in chromia layers grown on iron-base alloys. Oxidation of Metals 37 1/2 (1992) 81-93
-
(1992)
Oxidation of Metals
, vol.37
, Issue.1-2
, pp. 81-93
-
-
Lobnig, R.E.1
Schmidt, H.P.2
Hennesen, K.3
Grabke, H.J.4
-
16
-
-
24944508406
-
The effect of oxide volatilization on the oxidation kinetics of Cr and Fe-Cr alloys
-
Tedmond C.S. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe-Cr alloys. J. Electrochem. Soc. 113 (1966) 766-768
-
(1966)
J. Electrochem. Soc.
, vol.113
, pp. 766-768
-
-
Tedmond, C.S.1
|