메뉴 건너뛰기




Volumn 25, Issue 2, 2006, Pages 177-183

Research on semi-solid slurry of a hypoeutectic Al-Si alloy prepared by low superheat pouring and weak electromagnetic stirring

Author keywords

A356 Al alloy; Hypoeutectic Al Si alloy; Low superheat pouring; Semi solid; Weak electromagnetic stirring

Indexed keywords

GRAIN SIZE AND SHAPE; METAL WORKING; MORPHOLOGY; NUCLEATION; SILICON ALLOYS;

EID: 33745648768     PISSN: 10010521     EISSN: None     Source Type: Journal    
DOI: 10.1016/S1001-0521(06)60036-3     Document Type: Article
Times cited : (31)

References (19)
  • 1
    • 51249189971 scopus 로고
    • Rheological behaviour of Sn-15Pct Pb in the crystallization range
    • Spencer D.B., Mehrabian R., and Flemings M.C., Rheological behaviour of Sn-15Pct Pb in the crystallization range, Metall. Trans., 1972, 3A: 1925.
    • (1972) Metall. Trans. , vol.3 A , pp. 1295
    • Spencer, D.B.1    Mehrabian, R.2    Flemings, M.C.3
  • 2
    • 51649146713 scopus 로고
    • Behavior of metal alloys in the semisolid state
    • Flemings M.C., Behavior of metal alloys in the semisolid state, Metall. Trans., 1991, 22A: 957.
    • (1991) Metall. Trans. , vol.22 A , Issue.957
    • Flemings, M.C.1
  • 3
    • 84976803064 scopus 로고
    • Semisolid metal processing
    • Kirkwood D.K., Semisolid metal processing, Int. Mater. Rev., 1994, 39(5): 173.
    • (1994) Int. Mater. Rev. , vol.39 , Issue.5 , pp. 173
    • Kirkwood, D.K.1
  • 4
    • 0004256378 scopus 로고
    • (Ed.) by Flemings M.C., Mcgraw-Hill, New York
    • Flemings M.C., Solidification Process, Edited by Flemings M.C., Mcgraw-Hill, New York, 1974.
    • (1974) Solidification Process
    • Flemings, M.C.1
  • 6
    • 0036585515 scopus 로고    scopus 로고
    • Compressing deforming characteristics of semi-solid Al alloy prepared by controlling crystal method, Special Casting and Nonferrous Alloys
    • Chinese source
    • Cao H.B., Pan Y., and Zhang C., Compressing deforming characteristics of semi-solid Al alloy prepared by controlling crystal method, Special Casting and Nonferrous Alloys (in Chinese), 2002, (3): 9.
    • (2002) , Issue.3 , pp. 9
    • Cao, H.B.1    Pan, Y.2    Zhang, C.3
  • 7
    • 0032070704 scopus 로고    scopus 로고
    • Liquidus casting of a wrought Al alloy 2618 for thixoforming
    • Xia K., and Tausig G., Liquidus casting of a wrought Al alloy 2618 for thixoforming, Mater. Sci. Eng., 1998, A246: 1.
    • (1998) Mater. Sci. Eng. , vol.A246 , pp. 1
    • Xia, K.1    Tausig, G.2
  • 8
    • 33745657377 scopus 로고    scopus 로고
    • Application of nanocast method
    • Masao K. and Osamu N., Application of nanocast method, Alutop, 2004, (11): 21.
    • (2004) Alutop , Issue.11 , pp. 21
    • Masao, K.1    Osamu, N.2
  • 10
    • 0346020708 scopus 로고    scopus 로고
    • Spherical structure and formation condition of semi-solid Al-Mg-Si alloy
    • Nanjing, China
    • Pan Y., Aoyama S., and Liu C., Spherical structure and formation condition of semi-solid Al-Mg-Si alloy, [in] Proc. of the 5th Asian Foundry Congress, Nanjing, China, 1997: 443.
    • (1997) Proc. of the 5th Asian Foundry Congress , pp. 443
    • Pan, Y.1    Aoyama, S.2    Liu, C.3
  • 12
    • 33745182079 scopus 로고    scopus 로고
    • Evolution of globular and dendritic structures in solidification of Al-Si alloys
    • Chinese source
    • Zhao J.X., Zhu M.F., and Kim J.M., Evolution of globular and dendritic structures in solidification of Al-Si alloys, Phys. Testing and Chem. Anal. Part A Phys. Testing (in Chinese), 2004, 40(9): 433.
    • (2004) Phys. Testing and Chem. Anal. Part A Phys. Testing , vol.40 , Issue.9 , pp. 433
    • Zhao, J.X.1    Zhu, M.F.2    Kim, J.M.3
  • 14
    • 0347155246 scopus 로고    scopus 로고
    • Effect of melt flow at initial solidification on granular primary crystal formation in semi-solid alloy
    • Chinese source
    • Pan Y., Zhang C.Y., and Yuan H.Y., Effect of melt flow at initial solidification on granular primary crystal formation in semi-solid alloy, Acta Metall. Sin. (in Chinese), 2001, 37(10): 1035.
    • (2001) Acta Metall. Sin. , vol.37 , Issue.10 , pp. 1035
    • Pan, Y.1    Zhang, C.Y.2    Yuan, H.Y.3
  • 15
    • 18344396253 scopus 로고    scopus 로고
    • Chinese source, Machinery Industry Press, Beijing
    • Hu H.Q., The Metal Solidification Theory (in Chinese), Machinery Industry Press, Beijing, 2000: 109.
    • (2000) The Metal Solidification Theory , pp. 109
    • Hu, H.Q.1
  • 17
    • 0042224779 scopus 로고    scopus 로고
    • The formation mechanism of non-dendritic primary α-Al phases in semi-solid AlSi7Mg alloy
    • Chinese source
    • Mao W.M., Zhao A.M., and Cui C.L., The formation mechanism of non-dendritic primary α-Al phases in semi-solid AlSi7Mg alloy, Acta Metall Sin. (in Chinese), 1999, 35(9): 971.
    • (1999) Acta Metall Sin. , vol.35 , Issue.9 , pp. 971
    • Mao, W.M.1    Zhao, A.M.2    Cui, C.L.3
  • 19
    • 0347283447 scopus 로고    scopus 로고
    • Formation mechanism of non-dendritic structure in semi-solid metals produced by ES process
    • Chinese source
    • Zhang J.X., Zhang K., and Liu G.J., Formation mechanism of non-dendritic structure in semi-solid metals produced by ES process, Chin. J. Nonferrous Met. (in Chinese), 2000, 10(4): 511.
    • (2000) Chin. J. Nonferrous Met. , vol.10 , Issue.4 , pp. 511
    • Zhang, J.X.1    Zhang, K.2    Liu, G.J.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.