Volumn 88, Issue 11, 2005, Pages 3024-3031

Particulate-reinforced precursor-derived Si-C-N ceramics: Optimization of pyrolysis atmosphere and schedules

Author keywords

[No Author keywords available]

Indexed keywords

PARTICULATE-REINFORCED COMPOSITES (PRC); PRECURSOR-IMPREGNATION; SI-C-N CERAMICS; SI-C-N MATRIX;

EID: 33745299684     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2005.00587.x     Document Type: Article
Times cited : (22)

References (35)
  • 1
    • 0008646853 scopus 로고
    • SiC sintered bodies with three-dimensional polycarbosilane as binder
    • S. Yajima, T. Shishido, H. Kayano, K. Okamura, M. Omiri, and J. Hayashi, "SiC Sintered Bodies with Three-Dimensional Polycarbosilane as Binder," Nature, 264 [5583] 238-9 (1976).
    • (1976) Nature , vol.264 , Issue.5583 , pp. 238-239
    • Yajima, S.1    Shishido, T.2    Kayano, H.3    Okamura, K.4    Omiri, M.5    Hayashi, J.6
  • 2
    • 0345761441 scopus 로고    scopus 로고
    • Development of SiC fiber-reinforced SiC composites by radiation-cured preceramic polymer
    • Edited by K. Niihara. Trans Tech Publication, Zurich
    • M. Sugimoto, Y. Morita, T. Seguchi, and K. Okamura, "Development of SiC Fiber-Reinforced SiC Composites by Radiation-Cured Preceramic Polymer"; pp. 11-4 in Key Engineering Materials, Vols. 164-165, Edited by K. Niihara. Trans Tech Publication, Zurich, 1999.
    • (1999) Key Engineering Materials , vol.164-165 , pp. 11-14
    • Sugimoto, M.1    Morita, Y.2    Seguchi, T.3    Okamura, K.4
  • 3
    • 0026822033 scopus 로고
    • Synthesis of dense silicon-based ceramics at low-temperatures
    • R. Riedel, G. Passing, H. Schönfelder, and R. J. Brook, "Synthesis of Dense Silicon-Based Ceramics at Low-Temperatures," Nature, 355 [6362] 714-7 (1992).
    • (1992) Nature , vol.355 , Issue.6362 , pp. 714-717
    • Riedel, R.1    Passing, G.2    Schönfelder, H.3    Brook, R.J.4
  • 4
    • 0032206824 scopus 로고    scopus 로고
    • Decomposition-crystallization of polymer-derived Si-C-N ceramics
    • H.-J. Kleebe, D. Suttor, H. Mueller, and G. Ziegler, "Decomposition- Crystallization of Polymer-Derived Si-C-N Ceramics," J. Am. Ceram. Soc., 81 [11] 2971-7 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.11 , pp. 2971-2977
    • Kleebe, H.-J.1    Suttor, D.2    Mueller, H.3    Ziegler, G.4
  • 5
    • 0032667041 scopus 로고    scopus 로고
    • Fiber-reinforced composites with polymer-derived matrix: Processing, matrix formation and properties
    • G. Ziegler, I. Richter, and D. Suttor, "Fiber-Reinforced Composites with Polymer-Derived Matrix: Processing, Matrix Formation and Properties," Composites: Part A, 30 [4] 411-7 (1999).
    • (1999) Composites: Part A , vol.30 , Issue.4 , pp. 411-417
    • Ziegler, G.1    Richter, I.2    Suttor, D.3
  • 6
    • 0032668580 scopus 로고    scopus 로고
    • Processing aluminium nitride-silicon carbide composites via polymer infiltration and pyrolysis of polymethyl silane, a precursor to stoichiometric silicon carbide
    • K. W. Chew, A. Sellinger, and R. M. Laine, "Processing Aluminium Nitride-Silicon Carbide Composites via Polymer Infiltration and Pyrolysis of Polymethyl Silane, a Precursor to Stoichiometric Silicon Carbide," J. Am. Ceram. Soc., 82 [4] 857-66 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.4 , pp. 857-866
    • Chew, K.W.1    Sellinger, A.2    Laine, R.M.3
  • 7
    • 0035497649 scopus 로고    scopus 로고
    • f/SiC composites using liquid polymer infiltration
    • f/SiC Composites Using Liquid Polymer Infiltration," J. Am. Ceram. Soc., 84 [10] 2235-9 (2001).
    • (2001) J. Am. Ceram. Soc. , vol.84 , Issue.10 , pp. 2235-2239
    • Rak, Z.1
  • 8
    • 0033895468 scopus 로고    scopus 로고
    • Oxidation behavior of precursor-derived ceramics in the system Si-(B)-C-N
    • Edited by P. Sajgalík and Z. Lenčéš. Trans Tech Publications, Zurich
    • E. Butchereit and K. G. Nickel, "Oxidation Behavior of Precursor-Derived Ceramics in the System Si-(B)-C-N"; pp. 69-78 in Key Engineering Materials, Vols. 175-176, Edited by P. Sajgalík and Z. Lenčéš. Trans Tech Publications, Zurich, 2000.
    • (2000) Key Engineering Materials , vol.175-176 , pp. 69-78
    • Butchereit, E.1    Nickel, K.G.2
  • 9
    • 4344670043 scopus 로고    scopus 로고
    • Passive-oxidation kinetics of SiC microparticles
    • D. Das, J. Farjas, and P. Roura, "Passive-Oxidation Kinetics of SiC Microparticles," J. Am. Ceram. Soc., 87 [7] 1301-5 (2004).
    • (2004) J. Am. Ceram. Soc. , vol.87 , Issue.7 , pp. 1301-1305
    • Das, D.1    Farjas, J.2    Roura, P.3
  • 10
    • 0036722313 scopus 로고    scopus 로고
    • The ball on three balls test for strength testing of brittle discs: Stress distribution in the disc
    • A. Borger, P. Supancic, and R. Danzer, "The Ball on Three Balls Test for Strength Testing of Brittle Discs: Stress Distribution in the Disc," J. Eur. Ceram. Soc., 22 [9-10] 1425-36 (2002).
    • (2002) J. Eur. Ceram. Soc. , vol.22 , Issue.9-10 , pp. 1425-1436
    • Borger, A.1    Supancic, P.2    Danzer, R.3
  • 11
    • 84987335986 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness: 1, direct crack measurements
    • G. R. Anstis, P. Chantikul, B. R. Lawn, and D. B. Marshall, "A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: 1, Direct Crack Measurements," J. Am. Ceram. Soc., 64 [9] 533-8 (1981).
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.9 , pp. 533-538
    • Anstis, G.R.1    Chantikul, P.2    Lawn, B.R.3    Marshall, D.B.4
  • 12
    • 0033703215 scopus 로고    scopus 로고
    • Silicon carbonitride ceramics derived from polysilazane, part 1, investigation of compositional and structural properties
    • C. Haluschka, H.-J. Kleebe, R. Franke, and R. Riedel, "Silicon Carbonitride Ceramics Derived from Polysilazane, Part 1, Investigation of Compositional and Structural Properties," J. Eur. Ceram. Soc., 20 [9] 1355-64 (2000).
    • (2000) J. Eur. Ceram. Soc. , vol.20 , Issue.9 , pp. 1355-1364
    • Haluschka, C.1    Kleebe, H.-J.2    Franke, R.3    Riedel, R.4
  • 13
    • 0034135415 scopus 로고    scopus 로고
    • Structural characterization of silicon carbonitride ceramic derived from polymeric precursors
    • S. Traßl, D. Suttor, and O. Motz, "Structural Characterization of Silicon Carbonitride Ceramic Derived from Polymeric Precursors," J. Eur. Ceram. Soc., 20 [2] 215-25 (2000).
    • (2000) J. Eur. Ceram. Soc. , vol.20 , Issue.2 , pp. 215-225
    • Traßl, S.1    Suttor, D.2    Motz, O.3
  • 14
    • 0001235358 scopus 로고    scopus 로고
    • Advanced ceramics from inorganic polymers
    • Processing of Ceramics Part 2, Edited by R. J. Brook. VCH Verlagsgesellschaft mbH, Weinheim
    • R. Riedel, "Advanced Ceramics from Inorganic Polymers"; pp. 2-47 in Materials Science and Technology, Vol. 17B, Processing of Ceramics Part 2, Edited by R. J. Brook. VCH Verlagsgesellschaft mbH, Weinheim, 1996.
    • (1996) Materials Science and Technology , vol.17 B , pp. 2-47
    • Riedel, R.1
  • 15
    • 0036803810 scopus 로고    scopus 로고
    • Crystallization of polymer-derived silicon carbonitride at 1873 K under nitrogen overpressure
    • M. Freiss, J. Bill, J. Golczewski, A. Zimmermann, and F. Aldinger, "Crystallization of Polymer-Derived Silicon Carbonitride at 1873 K Under Nitrogen Overpressure," J. Am. Ceram. Soc., 85 [10] 2587-9 (2002).
    • (2002) J. Am. Ceram. Soc. , vol.85 , Issue.10 , pp. 2587-2589
    • Freiss, M.1    Bill, J.2    Golczewski, J.3    Zimmermann, A.4    Aldinger, F.5
  • 16
    • 0026626324 scopus 로고
    • Silicon carbonitride derived from an organometallic precursor; influence of the microstructure on the oxidation behavior
    • D. Bahloul, M. Pereira, and P. Goursat, "Silicon Carbonitride Derived from an Organometallic Precursor; Influence of the Microstructure on the Oxidation Behavior," Ceram. Int., 18 [1] 1-9 (1992).
    • (1992) Ceram. Int. , vol.18 , Issue.1 , pp. 1-9
    • Bahloul, D.1    Pereira, M.2    Goursat, P.3
  • 17
    • 0346062838 scopus 로고
    • Oxidation behavior of particulate and fibrous silicon carbide
    • D. W. Mckee and P. A. Siemers, "Oxidation Behavior of Particulate and Fibrous Silicon Carbide," Int. J. High Tech. Ceram., 4, 11-29 (1988).
    • (1988) Int. J. High Tech. Ceram. , vol.4 , pp. 11-29
    • Mckee, D.W.1    Siemers, P.A.2
  • 18
    • 0024716359 scopus 로고
    • High-temperature passive oxidation of chemically vapor deposited silicon carbide
    • T. Narushima, T. Goto, and T. Hirai, "High-Temperature Passive Oxidation of Chemically Vapor Deposited Silicon Carbide," J. Am. Ceram. Soc., 72 [8] 1386-90 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.8 , pp. 1386-1390
    • Narushima, T.1    Goto, T.2    Hirai, T.3
  • 19
    • 0010066704 scopus 로고    scopus 로고
    • Mass transfer within the gas-phase of porous media
    • W. Kast and C. -R. Hohenthanner, "Mass Transfer within the Gas-Phase of Porous Media," Int. J. Heat Mass. Tran., 43 [5] 807-23 (2000).
    • (2000) Int. J. Heat Mass. Tran. , vol.43 , Issue.5 , pp. 807-823
    • Kast, W.1    Hohenthanner, C.R.2
  • 21
    • 0004086855 scopus 로고    scopus 로고
    • Marcel Dekker Inc., New York
    • R. W. Rice, Porosity of Ceramics, pp. 73-4. Marcel Dekker Inc., New York, 1998.
    • (1998) Porosity of Ceramics , pp. 73-74
    • Rice, R.W.1
  • 22
    • 0035437640 scopus 로고    scopus 로고
    • Oxidation kinetics of an amorphous silicon carbonitride ceramic
    • R. Raj, L. An, S. Shah, R. Riedel, C. Fasel, and H.-J. Kleebe, "Oxidation Kinetics of an Amorphous Silicon Carbonitride Ceramic," J. Am. Ceram. Soc., 84 [8] 1803-10 (2001).
    • (2001) J. Am. Ceram. Soc. , vol.84 , Issue.8 , pp. 1803-1810
    • Raj, R.1    An, L.2    Shah, S.3    Riedel, R.4    Fasel, C.5    Kleebe, H.-J.6
  • 23
    • 0036734691 scopus 로고    scopus 로고
    • Oxidation bonding of porous silicon carbide ceramics
    • J. H. She, Z. Y. Deng, J. Daniel-Doni, and T. Ohji, "Oxidation Bonding of Porous Silicon Carbide Ceramics," J. Mater. Sci., 37 [17] 3615-22 (2002).
    • (2002) J. Mater. Sci. , vol.37 , Issue.17 , pp. 3615-3622
    • She, J.H.1    Deng, Z.Y.2    Daniel-Doni, J.3    Ohji, T.4
  • 24
    • 0029637640 scopus 로고
    • A covalenl micro/ nano-composite resistant to high-temperature oxidation
    • R. Riedel, H.-J. Kleebe, H. Schönfelder, and F. Aldinger, "A Covalenl Micro/ Nano-Composite Resistant to High-Temperature Oxidation," Nature, 374 [6522] 526-8 (1995).
    • (1995) Nature , vol.374 , Issue.6522 , pp. 526-528
    • Riedel, R.1    Kleebe, H.-J.2    Schönfelder, H.3    Aldinger, F.4
  • 25
    • 0027667682 scopus 로고
    • Effect of powder surface modification on the properties of silicon nitride ceramics
    • S. Natansohn, A. E. Pasto, and W. J. Rourke, "Effect of Powder Surface Modification on the Properties of Silicon Nitride Ceramics," J. Am. Ceram. Soc., 76 [9] 2273-84 (1993).
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.9 , pp. 2273-2284
    • Natansohn, S.1    Pasto, A.E.2    Rourke, W.J.3
  • 27
    • 0024664405 scopus 로고
    • Oxidation studies of crystalline CVD silicon nitride
    • H. Du, R. E. Tressler, K. E. Spear, and C. G. Pantano, "Oxidation Studies of Crystalline CVD Silicon Nitride," J. Electrochem. Soc., 136 [5] 1527-35 (1989).
    • (1989) J. Electrochem. Soc. , vol.136 , Issue.5 , pp. 1527-1535
    • Du, H.1    Tressler, R.E.2    Spear, K.E.3    Pantano, C.G.4
  • 28
    • 0025957615 scopus 로고
    • Effect of carbon monoxide partial pressure on the high-temperature decomposition of nicalon fiber
    • G. S. Bibbo, P. M. Benson, and C. G. Pantano, "Effect of Carbon Monoxide Partial Pressure on the High-Temperature Decomposition of Nicalon Fiber," J. Mater. Sci., 26 [18] 5075-80 (1991).
    • (1991) J. Mater. Sci. , vol.26 , Issue.18 , pp. 5075-5080
    • Bibbo, G.S.1    Benson, P.M.2    Pantano, C.G.3
  • 29
    • 0032667350 scopus 로고    scopus 로고
    • Silicon oxicarbide foams from a silicon preceramic polymer and polyurethane
    • P. Colombo and M. Modesti, "Silicon Oxicarbide Foams from a Silicon Preceramic Polymer and Polyurethane," J. Sol-Gel Sci. Tech., 14 [1] 103-11 (1999).
    • (1999) J. Sol-gel Sci. Tech. , vol.14 , Issue.1 , pp. 103-111
    • Colombo, P.1    Modesti, M.2
  • 30
    • 0033727860 scopus 로고    scopus 로고
    • Microstructure and oxidation behavior of silicon carbide fibers derived from polycarbosilane
    • M. Takeda, A. Urano, J. I. Sakamoto, and Y. Imai, "Microstructure and Oxidation Behavior of Silicon Carbide Fibers Derived from Polycarbosilane," J. Am. Ceram. Soc., 83 [5] 1171-6 (2000).
    • (2000) J. Am. Ceram. Soc. , vol.83 , Issue.5 , pp. 1171-1176
    • Takeda, M.1    Urano, A.2    Sakamoto, J.I.3    Imai, Y.4
  • 32
    • 84986364637 scopus 로고
    • Preparation of silicon carbonitrides from an organosilicon polymer: 1, thermal decomposition of the cross-linked polysilazane
    • D. Bahloul, M. Pereira, P. Goursat, N. S. Choong, K. Yive, and R. J. P. Corriu, "Preparation of Silicon Carbonitrides from an Organosilicon Polymer: 1, Thermal Decomposition of the Cross-Linked Polysilazane," J. Am. Ceram. Soc., 76 [5] 1156-62 (1993).
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.5 , pp. 1156-1162
    • Bahloul, D.1    Pereira, M.2    Goursat, P.3    Choong, N.S.4    Yive, K.5    Corriu, R.J.P.6
  • 33
    • 0035497621 scopus 로고    scopus 로고
    • Crystallization behavior of amorphous silicon carbide ceramics derived from organometallic precursors
    • Y. Iwamoto, W. Voelger, E. Kroke, and R. Riedel, "Crystallization Behavior of Amorphous Silicon Carbide Ceramics Derived from Organometallic Precursors," J. Am. Ceram. Soc., 84 [10] 2170-78 (2001).
    • (2001) J. Am. Ceram. Soc. , vol.84 , Issue.10 , pp. 2170-2178
    • Iwamoto, Y.1    Voelger, W.2    Kroke, E.3    Riedel, R.4
  • 34
    • 0036605154 scopus 로고    scopus 로고
    • Synthesis of a polycyclic silazane network and its evolution to silicon carbonitride glass
    • M. Schiavon, G. Soraru, and I. Yoshida, "Synthesis of a Polycyclic Silazane Network and Its Evolution to Silicon Carbonitride Glass," J. Non-Cryst. Solids, 304 [1-3] 76-83 (2002).
    • (2002) J. Non-cryst. Solids , vol.304 , Issue.1-3 , pp. 76-83
    • Schiavon, M.1    Soraru, G.2    Yoshida, I.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.