Volumn 51, Issue 23, 2006, Pages 4815-4820
|
Development of an environmentally friendly protective coating for the depleted uranium-0.75 wt.% titanium alloy. Part IV. Vibrational spectroscopy of the coating
|
Author keywords
Corrosion; FT IR; Molybdate coatings; Raman; Uranium alloys
|
Indexed keywords
ELECTROCHEMICAL CORROSION;
FOURIER TRANSFORM INFRARED SPECTROSCOPY;
MOLYBDENUM COMPOUNDS;
PROTECTIVE COATINGS;
RAMAN SPECTROSCOPY;
SPECTROSCOPIC ANALYSIS;
TITANIUM ALLOYS;
FT-IR;
MOLYBDATE COATINGS;
OCTAMOLYBDATE STRUCTURE;
VIBRATIONAL SPECTROSCOPY;
URANIUM ALLOYS;
|
EID: 33646820713
PISSN: 00134686
EISSN: None
Source Type: Journal
DOI: 10.1016/j.electacta.2006.01.027 Document Type: Article |
Times cited : (12)
|
References (71)
|