Volumn 8, Issue 3, 2006, Pages 237-258

Influence of face/core interface on debond toughness of foam and balsa cored sandwich

Author keywords

Balsa core; Debonding; Foam core; Fracture toughness; Glass fiber; Interface; Vacuum infusion

Indexed keywords


EID: 33646393020     PISSN: 10996362     EISSN: 15307972     Source Type: Journal    
DOI: 10.1177/1099636206062570     Document Type: Article
Times cited : (27)

References (13)
  • 1
    • 0001878461 scopus 로고    scopus 로고
    • The Tilted Sandwich Debond (TSD) Specimen for Face/ Core Interface Characterization
    • Li, X. and Carlsson, L.A. (1999). The Tilted Sandwich Debond (TSD) Specimen for Face/ Core Interface Characterization, J. Sandwich Struct. Mater., 1 (1). 60 - 75.
    • (1999) J. Sandwich Struct. Mater. , vol.1 , Issue.1 , pp. 60-75
    • Li, X.1    Carlsson, L.A.2
  • 2
    • 84990348409 scopus 로고    scopus 로고
    • Influences of Foam Density and Core Thickness on Debond Toughness of Sandwich Specimens with PVC Foam Core
    • Viana, G.M. and Carlsson, L.A. (2003). Influences of Foam Density and Core Thickness on Debond Toughness of Sandwich Specimens with PVC Foam Core, J. Sandwich Struct. Mater., 5 (2). 103 - 118.
    • (2003) J. Sandwich Struct. Mater. , vol.5 , Issue.2 , pp. 103-118
    • Viana, G.M.1    Carlsson, L.A.2
  • 3
    • 2342620701 scopus 로고    scopus 로고
    • In-Situ Fracture Toughness Testing of Core Materials in Sandwich Panels
    • Shivakumar, K.N. and Smith, S.A. (2004). In-Situ Fracture Toughness Testing of Core Materials in Sandwich Panels, J. Compos. Mater., 38 (8). 655 - 668.
    • (2004) J. Compos. Mater. , vol.38 , Issue.8 , pp. 655-668
    • Shivakumar, K.N.1    Smith, S.A.2
  • 4
    • 0141753138 scopus 로고    scopus 로고
    • Effect of Processing Conditions and Material Properties on the Debond Fracture Toughness of Foam-core Sandwich Composites: Experimental Optimization
    • Majumdar, P., Srinivasagupta, D., Mahfuz, H., Joseph, B., Thomas, M. and Christensen, S. (2003). Effect of Processing Conditions and Material Properties on the Debond Fracture Toughness of Foam-core Sandwich Composites: Experimental Optimization, Composites: Part A, 34 (11). 1097 - 1104.
    • (2003) Composites: Part A , vol.34 , Issue.11 , pp. 1097-1104
    • Majumdar, P.1    Srinivasagupta, D.2    Mahfuz, H.3    Joseph, B.4    Thomas, M.5    Christensen, S.6
  • 8
    • 33646392804 scopus 로고    scopus 로고
    • Laholm, Sweden (available at
    • DIAB. ProBalsa Technical Manual, 10.00. DIAB AB, Laholm, Sweden (available at http://www.diabgroup.com ).
    • ProBalsa Technical Manual
  • 9
    • 0012283852 scopus 로고    scopus 로고
    • Laholm, Sweden (available at
    • DIAB. Divinycell H-Grade Technical Manual, 10.00. DIAB AB, Laholm, Sweden (available at http://www.diabgroup.com ).
    • Divinycell H-Grade Technical Manual
  • 10
    • 33646395747 scopus 로고    scopus 로고
    • One Owens Corning Parkway, Toledo, OH 43659 (available at
    • Owens Corning. Kyntex Woven Rovings Technical Data Sheet. One Owens Corning Parkway, Toledo, OH 43659 (available at http://secure.owenscorning.net ).
    • Kyntex Woven Rovings Technical Data Sheet
  • 12
    • 27644480020 scopus 로고    scopus 로고
    • Crack Path in Foam Cored DCB Sandwich Fracture Specimens
    • Carlsson, L.A., Matteson, R.C., Aviles, F. and Loup, D.C. (2005). Crack Path in Foam Cored DCB Sandwich Fracture Specimens, Compos. Sci. Tech., 65 (15-16). 2612 - 2621.
    • (2005) Compos. Sci. Tech. , vol.65 , Issue.15-16 , pp. 2612-2621
    • Carlsson, L.A.1    Matteson, R.C.2    Aviles, F.3    Loup, D.C.4
  • 13
    • 0026711933 scopus 로고
    • Mode i Interlaminar Fracture of Interleaved Graphite/ Epoxy
    • Ozdil, F. and Carlsson, L.A. (1992). Mode I Interlaminar Fracture of Interleaved Graphite/ Epoxy, J. Compos. Mater., 26 (3). 432 - 459.
    • (1992) J. Compos. Mater. , vol.26 , Issue.3 , pp. 432-459
    • Ozdil, F.1    Carlsson, L.A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.