Volumn 2006, Issue , 2006, Pages 367-372

Effect of hot torsion deformation on microstructure in AZ31 magnesium alloy

Author keywords

Hot rolling; Recrystallization; Torsion deformation; Twinning

Indexed keywords

INDUSTRIAL SHEET ROLLING; NECKLACING; THERMOMECHANICAL CONDITIONS; TORSION DEFORMATION;

EID: 33646168380     PISSN: 15454150     EISSN: None     Source Type: Conference Proceeding    
DOI: None     Document Type: Conference Paper
Times cited : (2)

References (15)
  • 2
    • 33646193055 scopus 로고    scopus 로고
    • Corrosion and corrosion protection of magnesium
    • ed. K.U. Kainer (Wiley-VCH, Weinheim)
    • P. Kurze, "Corrosion and Corrosion Protection of Magnesium", Magnesium Alloys and Technology, ed. K.U. Kainer (Wiley-VCH, Weinheim, 2003), 218-225.
    • (2003) Magnesium Alloys and Technology , pp. 218-225
    • Kurze, P.1
  • 3
    • 0037247212 scopus 로고    scopus 로고
    • Guide for enhancement of room temperature ductility in Mg alloys at high strain rates
    • T. Mukai, et al., "Guide for Enhancement of Room Temperature Ductility in Mg alloys at High Strain Rates", Materials Science Forum, 419-422 (2003), 171-176.
    • (2003) Materials Science Forum , vol.419-422 , pp. 171-176
    • Mukai, T.1
  • 4
    • 5744227425 scopus 로고    scopus 로고
    • Deformation microstructures and textures of some cold rolled Mg alloys
    • M.R. Barnett, M.D. Nave, and C.J. Bettles, "Deformation Microstructures and Textures of some Cold Rolled Mg Alloys", Materials Science and Engineering A, 386 (2004), 205-211.
    • (2004) Materials Science and Engineering A , vol.386 , pp. 205-211
    • Barnett, M.R.1    Nave, M.D.2    Bettles, C.J.3
  • 5
    • 4344568184 scopus 로고    scopus 로고
    • Microstructures and textures of pure magnesium deformed in plane-strain compression
    • M.D. Nave and M.R. Barnett, "Microstructures and Textures of Pure magnesium Deformed in Plane-Strain Compression", Scripta Materialia, 51 (2004), 881-885.
    • (2004) Scripta Materialia , vol.51 , pp. 881-885
    • Nave, M.D.1    Barnett, M.R.2
  • 7
    • 26244468631 scopus 로고
    • Shear accommodation kinking at second order twin in magnesium
    • W.H. Hartt and R.E. Reed-Hill, "Shear Accommodation Kinking at Second Order Twin in Magnesium", Transactions of Metallurgical Society AIME, 242 (10) (1968), 2207-2210.
    • (1968) Transactions of Metallurgical Society AIME , vol.242 , Issue.10 , pp. 2207-2210
    • Hartt, W.H.1    Reed-Hill, R.E.2
  • 9
    • 2642571747 scopus 로고    scopus 로고
    • Dynamic recrystallization of AZ31 magnesium alloy during torsion deformation at elevated temperatures
    • ed. Alan Luo (Warrendale, PA: The Minerals, Metals, and Materials Society)
    • W.J. Liu, et al., "Dynamic Recrystallization of AZ31 Magnesium alloy during Torsion Deformation at Elevated Temperatures", Magnesium Technology 2004, ed. Alan Luo (Warrendale, PA: The Minerals, Metals, and Materials Society, 2004), 73-78.
    • (2004) Magnesium Technology 2004 , pp. 73-78
    • Liu, W.J.1
  • 10
    • 0035860886 scopus 로고    scopus 로고
    • The onset of twinning in metals, a constitutive description
    • M.A. Meyers, O. Vohringer, and V.A. Lubarda, "The Onset of Twinning in Metals, A Constitutive Description", Acta Materialia, 39 (2001), 4025-4039.
    • (2001) Acta Materialia , vol.39 , pp. 4025-4039
    • Meyers, M.A.1    Vohringer, O.2    Lubarda, V.A.3
  • 11
    • 0031351412 scopus 로고    scopus 로고
    • Microstructural development in Mg alloy AZ31 during hot working
    • A. Mwembela, E.B. Konopleva, and H.J. McQueen, "Microstructural Development in Mg Alloy AZ31 during Hot Working", Scripta Materialia, 37 (11) (1997), 1789-1795.
    • (1997) Scripta Materialia , vol.37 , Issue.11 , pp. 1789-1795
    • Mwembela, A.1    Konopleva, E.B.2    McQueen, H.J.3
  • 12
    • 0020197298 scopus 로고
    • Dynamic recrystallization and the development of microstructure during the high-temperature deformation of magnesium
    • S.E. Ion, F.J. Humphreys, and S.H. White, "Dynamic Recrystallization and the Development of Microstructure during the High-Temperature Deformation of Magnesium", Acta Metallurgica, 30 (10) (1982), 1909-1919.
    • (1982) Acta Metallurgica , vol.30 , Issue.10 , pp. 1909-1919
    • Ion, S.E.1    Humphreys, F.J.2    White, S.H.3
  • 13
    • 0000094398 scopus 로고    scopus 로고
    • Influence of deformation conditions and texture on the high temperature flow stress of magnesium AZ31
    • M.R. Barnett, "Influence of Deformation Conditions and Texture on the High Temperature Flow Stress of Magnesium AZ31", Journal of Light Metals, 1 (2001), 167-177.
    • (2001) Journal of Light Metals , vol.1 , pp. 167-177
    • Barnett, M.R.1
  • 15
    • 33646199588 scopus 로고    scopus 로고
    • Effect of aluminum additions on the deformation behavior of magnesium alloys
    • ed. Alan Luo (Warrendale, PA: The Minerals, Metals, and Materials Society)
    • G. Seale et al., "Effect of Aluminum Additions on the Deformation Behavior of Magnesium Alloys", Magnesium Technology 2006, ed. Alan Luo (Warrendale, PA: The Minerals, Metals, and Materials Society, 2006).
    • (2006) Magnesium Technology 2006
    • Seale, G.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.