Self-crack-healing behavior of mullite/SiC particle/SiC whisker multi-composites and potential use for ceramic springs

Author keywords

[No Author keywords available]

Indexed keywords

CRACKS; FRACTURE; HOT PRESSING; SILICON CARBIDE; SINTERING;

EID: 33645136608     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2005.00868.x     Document Type: Article
Times cited : (52)

References (13)
  • 1
    • 0029371327 scopus 로고
    • Damage healing and strengthealing behavior in intelligent mullite/SiC ceramics
    • M. C. Chu, S. Sato, Y. Kobayashi, and K. Ando, "Damage Healing and Strengthealing Behavior in Intelligent Mullite/SiC Ceramics," Fatigue Fract. Eng., Mater. Struct., 18 [9] 1019-29 (1995).
    • (1995) Fatigue Fract. Eng., Mater. Struct. , vol.18 , Issue.9 , pp. 1019-1029
    • Chu, M.C.1    Sato, S.2    Kobayashi, Y.3    Ando, K.4
  • 2
    • 0032072901 scopus 로고    scopus 로고
    • Effect of annealing environment on the crack healing and mechanical behavior of silicon carbide-reinforced alumina nanocomposites
    • I. A. Chou, H. M. Chan, and M. P. Harmer, "Effect of Annealing Environment on the Crack Healing and Mechanical Behavior of Silicon Carbide-Reinforced Alumina Nanocomposites," J. Am. Ceram. Soc., 81 [5] 1203-8 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.5 , pp. 1203-1208
    • Chou, I.A.1    Chan, H.M.2    Harmer, M.P.3
  • 3
    • 0041888384 scopus 로고    scopus 로고
    • Crack-healing behavior of monolithic alumina and strength of crack-healed member
    • B. S. Kim, K. Ando, M. C. Chu, and S. Saito, "Crack-Healing Behavior of Monolithic Alumina and Strength of Crack-Healed Member," J. Soc. Mater. Sci. Jpn., 52 [6] 667-73 (2003).
    • (2003) J. Soc. Mater. Sci. Jpn. , vol.52 , Issue.6 , pp. 667-673
    • Kim, B.S.1    Ando, K.2    Chu, M.C.3    Saito, S.4
  • 8
    • 0036740298 scopus 로고    scopus 로고
    • 4/SiC ceramics under cyclic stress and resultant strength at the crack-healing temperature
    • 4/SiC Ceramics Under Cyclic Stress and Resultant Strength at the Crack-Healing Temperature," J. Am. Ceram. Soc., 85 [9] 2268-72 (2002).
    • (2002) J. Am. Ceram. Soc. , vol.85 , Issue.9 , pp. 2268-2272
    • Ando, K.1    Takahashi, K.2    Nakayama, S.3    Sato, S.4
  • 9
    • 18344366146 scopus 로고    scopus 로고
    • Crack-healing behavior, high temperature strength and fracture toughness of mullite/SiC whisker composite ceramic
    • M. Ono, W. Ishida, W. Nakao, K. Ando, S. Mori, and M. Yokouchi, "Crack-Healing Behavior, High Temperature Strength and Fracture Toughness of Mullite/SiC Whisker Composite Ceramic," J. Soc. Mater. Sci. Jpn., 54 [2] 207-14 (2004).
    • (2004) J. Soc. Mater. Sci. Jpn. , vol.54 , Issue.2 , pp. 207-214
    • Ono, M.1    Ishida, W.2    Nakao, W.3    Ando, K.4    Mori, S.5    Yokouchi, M.6
  • 10
    • 26944470784 scopus 로고    scopus 로고
    • Crack-healing mechanism by alumina/SiC particles/SiC whiskers mvilli-composite
    • W. Nakao, T. Osada, K. Yamane, Koji Takahashi, and K. Ando, "Crack-Healing Mechanism by Alumina/SiC Particles/SiC Whiskers Mvilli-Composite," J. Jpn. Inst. Metals, 69 [8] 663-6.
    • J. Jpn. Inst. Metals , vol.69 , Issue.8 , pp. 663-666
    • Nakao, W.1    Osada, T.2    Yamane, K.3    Takahashi, K.4    Ando, K.5
  • 11
    • 33645138333 scopus 로고    scopus 로고
    • Japan Industrial Standard R1607 . Japan Standard Association, Tokyo, Japan
    • Japan Industrial Standard R1607 . Testing Methods for Fracture Toughness of Fine Ceramics. Japan Standard Association, Tokyo, Japan, 2003.
    • (2003) Testing Methods for Fracture Toughness of Fine Ceramics
  • 12
    • 0003955025 scopus 로고    scopus 로고
    • An introduction to the mechanical properties of ceramics
    • ed. D. R. Clarke, S. Suresh and I. M. Ward FRS. Cambridge University Press, Cambridge, U.K.
    • D. J. Green, "An Introduction to the Mechanical Properties of Ceramics"; pp. 25 and 78-87 in Cambridge Solid State Science Series, ed. D. R. Clarke, S. Suresh and I. M. Ward FRS. Cambridge University Press, Cambridge, U.K., 1998.
    • (1998) Cambridge Solid State Science Series , pp. 25
    • Green, D.J.1
  • 13
    • 33645165226 scopus 로고
    • Gihoudo Shuppan Co., Ltd., Tokyo, Japan
    • Japan Ceramics Society (Ed.). Handbook of Ceramics, p. 2011. Gihoudo Shuppan Co., Ltd., Tokyo, Japan, 1984.
    • (1984) Handbook of Ceramics , pp. 2011


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.