Volumn 58, Issue 1, 2006, Pages 43-46

The oxidation properties of fourth generation single-crystal nickel-based superalloys

Author keywords

[No Author keywords available]

Indexed keywords

HIGH TEMPERATURE OXIDATION RESISTANCE; NICKEL BASED SUPERALLOYS; SINGLE CRYSTAL SUPERALLOYS;

EID: 31344453221     PISSN: 10474838     EISSN: None     Source Type: Journal    
DOI: 10.1007/s11837-006-0067-z     Document Type: Article
Times cited : (72)

References (18)
  • 1
    • 0012131245 scopus 로고
    • "Formation of Topologically Closed Packed Phases in Nickel Base Single Crystal Superalloys"
    • ed. S. Reichman at al. (Warrendale, PA: TMS)
    • R. Darolia et al., "Formation of Topologically Closed Packed Phases in Nickel Base Single Crystal Superalloys," Superalloys 1988, ed. S. Reichman at al. (Warrendale, PA: TMS, 1988), pp. 255-264.
    • (1988) Superalloys 1988 , pp. 255-264
    • Darolia, R.1
  • 2
    • 0002767084 scopus 로고    scopus 로고
    • "Development of a New Single Crystal Superalloy for Industrial Gas Turbines"
    • ed. T.M. Pollock et al. (Warrendale, PA: TMS)
    • T. Hino et al., "Development of a New Single Crystal Superalloy for Industrial Gas Turbines," Superalloys 2000, ed. T.M. Pollock et al. (Warrendale, PA: TMS, 2000), pp. 729-736.
    • (2000) Superalloys 2000 , pp. 729-736
    • Hino, T.1
  • 3
    • 6344278828 scopus 로고    scopus 로고
    • "TTT Diagram for TCP Phases Precipitations of 4th Generation Ni-Base Superalloys"
    • A. Sato et al., "TTT Diagram for TCP Phases Precipitations of 4th Generation Ni-Base Superalloys," J. Japan Inst. Metals, 68 (2004), pp. 507-510.
    • (2004) J. Japan Inst. Metals , vol.68 , pp. 507-510
    • Sato, A.1
  • 5
    • 0036989285 scopus 로고    scopus 로고
    • "Interfacial Dislocation Networks Strengthening a Fourth-Generation Single-Crystal TMS-138 Superalloy"
    • J.X. Zhang et al., "Interfacial Dislocation Networks Strengthening a Fourth-Generation Single-Crystal TMS-138 Superalloy," Metall. Mater. Trans. A, 33A (2002), pp. 3741-3746.
    • (2002) Metall. Mater. Trans. A , vol.33 A , pp. 3741-3746
    • Zhang, J.X.1
  • 6
    • 0012588101 scopus 로고    scopus 로고
    • "Studies on the Surface Chemistry of Oxide Films Formed on IN-738LC Superalloy at Elevated Temperatures in Dry Air"
    • S. Seal et al., "Studies on the Surface Chemistry of Oxide Films Formed on IN-738LC Superalloy at Elevated Temperatures in Dry Air," Oxid. Met., 56 (2001), pp. 581-603.
    • (2001) Oxid. Met. , vol.56 , pp. 581-603
    • Seal, S.1
  • 7
    • 0037570895 scopus 로고    scopus 로고
    • "Surface Chemistry of Oxide Scale on IN-738LC Superalloy: Effect of Long-Term Exposure in Air at 1173K"
    • S. Seal et al., "Surface Chemistry of Oxide Scale on IN-738LC Superalloy: Effect of Long-Term Exposure in Air at 1173K," Oxid. Met., 57 (2002), pp. 297-322.
    • (2002) Oxid. Met. , vol.57 , pp. 297-322
    • Seal, S.1
  • 8
    • 23744475468 scopus 로고    scopus 로고
    • "Oxidation Behavior of Two Nickel-Base Superalloys Used as Elevated Temperature Valves in Spark Ignited Engines and Diesel Exhaust Recirculation (EGR) Applications"
    • ad. K.A. Green et al. (Warrendale, PA: TMS)
    • S. Shinharoy and L. Narasimhan, "Oxidation Behavior of Two Nickel-Base Superalloys Used as Elevated Temperature Valves in Spark Ignited Engines and Diesel Exhaust Recirculation (EGR) Applications," Superalloys 2004, ad. K.A. Green et al. (Warrendale, PA: TMS, 2004), pp. 623-626.
    • (2004) Superalloys 2004 , pp. 623-626
    • Shinharoy, S.1    Narasimhan, L.2
  • 9
    • 0345357220 scopus 로고    scopus 로고
    • "Oxidation Behaviour of the Alloy IC-6 and Protective Coatings"
    • B. Wang et al., "Oxidation Behaviour of the Alloy IC-6 and Protective Coatings," Corros. Sci., 46 (2004), pp. 519-528.
    • (2004) Corros. Sci. , vol.46 , pp. 519-528
    • Wang, B.1
  • 10
    • 0038607070 scopus 로고    scopus 로고
    • "Oxidation Behavior of a Single-Crystal Ni-Base Superalloy in Air - I: At 800 and 900°C"
    • M.H. Li et al., "Oxidation Behavior of a Single-Crystal Ni-Base Superalloy in Air - I: At 800 and 900°C", Oxid, Met., 59 (2003), pp. 591-605.
    • (2003) Oxid. Met. , vol.59 , pp. 591-605
    • Li, M.H.1
  • 11
    • 0041438475 scopus 로고    scopus 로고
    • "Oxidation Behavior of a Single-Crystal Ni-Base Superalloy in Air - II: At 1000, 1100, and 1150°"
    • M.H. Li et al., "Oxidation Behavior of a Single-Crystal Ni-Base Superalloy in Air - II: At 1000, 1100, and 1150°," Oxid. Met., 60 (2003), pp. 195-210.
    • (2003) Oxid. Met. , vol.60 , pp. 195-210
    • Li, M.H.1
  • 12
    • 23744510479 scopus 로고    scopus 로고
    • "The Effect of Water Vapor on the Oxidation of Nickel-Base Superalloys and Coatings at Temperatures from 700° to 1100°C"
    • ed. K.A. Green et al. (Warrendale, PA: TMS)
    • K. Onal et al., "The Effect of Water Vapor on the Oxidation of Nickel-Base Superalloys and Coatings at Temperatures from 700° to 1100°C" Superalloys 2004, ed. K.A. Green et al. (Warrendale, PA: TMS, 2004), pp. 607-615.
    • (2004) Superalloys 2004 , pp. 607-615
    • Onal, K.1
  • 13
    • 31344445649 scopus 로고    scopus 로고
    • "Effect of Alloying Elements on the Oxidation Behavior of 4th Generation Ni-base Single-crystal Superalloys"
    • K. Kawagishi et al., "Effect of Alloying Elements on the Oxidation Behavior of 4th Generation Ni-base Single-crystal Superalloys," TMS Lett., 2 (2005), pp. 23-24.
    • (2005) TMS Lett. , vol.2 , pp. 23-24
    • Kawagishi, K.1
  • 14
    • 85086680698 scopus 로고    scopus 로고
    • "Oxidation Behavior of Rucontaining Ni-base Single-crystal Superalloys"
    • Submitted to
    • K. Kawagishi et al., "Oxidation Behavior of Rucontaining Ni-base Single-crystal Superalloys," submitted to Mater. Sci. Forum.
    • Mater. Sci. Forum.
    • Kawagishi, K.1
  • 15
    • 31344448565 scopus 로고    scopus 로고
    • "Yttrium Doping for Oxidation Resistance of a 4th Generation Ni-Base Superalloy TMS-138"
    • A. Sato et al., "Yttrium Doping for Oxidation Resistance of a 4th Generation Ni-Base Superalloy TMS-138," TMS Lett., 2 (2005), pp. 19-20.
    • (2005) TMS Lett. , vol.2 , pp. 19-20
    • Sato, A.1
  • 16
    • 0032076419 scopus 로고    scopus 로고
    • "Substrate and Bond Coat Compositions: Factors Affecting Alumina Scale Adhesion"
    • B.A. Pint et al., "Substrate and Bond Coat Compositions: Factors Affecting Alumina Scale Adhesion," Mater. Sci. Eng. A,245 (1998) pp. 201-211.
    • (1998) Mater. Sci. Eng. A , vol.245 , pp. 201-211
    • Pint, B.A.1
  • 17
    • 31344449600 scopus 로고    scopus 로고
    • "Improved Performance CMSX-4 Alloy Turbine Blades Utilising PPM Levels of Lanthanum and Yttrium"
    • (Paper presented at the 6th Liège Conference, Materials for Advanced Power Engineering, Liège, Belgium, 5-7 October)
    • D.A. Ford et al., "Improved Performance CMSX-4 Alloy Turbine Blades Utilising PPM Levels of Lanthanum and Yttrium" (Paper presented at the 6th Liège Conference, Materials for Advanced Power Engineering, Liège, Belgium, 5-7 October 1998).
    • (1998)
    • Ford, D.A.1
  • 18
    • 23744437074 scopus 로고    scopus 로고
    • "Development of Next Generation Nickel-Base Single Crystal Superalloys"
    • ed. K.A. Green et al. (Warrendale, PA: TMS)
    • Y. Koizumi et al., "Development of Next Generation Nickel-Base Single Crystal Superalloys," Superalloys 2004, ed. K.A. Green et al. (Warrendale, PA: TMS, 2004), pp. 35-43.
    • (2004) Superalloys 2004 , pp. 35-43
    • Koizumi, Y.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.