메뉴 건너뛰기




Volumn 20, Issue 7, 2004, Pages 635-642

Storage effect of a pre-activated silane on the resin to ceramic bond

Author keywords

Bond; Ceramic; Fourier transform infrared; Resin; Silane; Strength; Tensile

Indexed keywords

ACETIC ACID; BOND STRENGTH (CHEMICAL); CERAMIC MATERIALS; CHEMICAL BONDS; ETHANOL; FAILURE ANALYSIS; HYDROLYSIS; RESINS; SILANES; SPECTROPHOTOMETERS; STATISTICAL METHODS; STORAGE (MATERIALS); TENSILE TESTING;

EID: 3042852422     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2003.08.005     Document Type: Article
Times cited : (71)

References (23)
  • 1
    • 0026893507 scopus 로고
    • The influence of surface conditions and silane agents on the bond of resin to dental porcelain
    • Hayakawa T., Horie K., Aida M., Kanaya H., Kobayashi T., Murata Y. The influence of surface conditions and silane agents on the bond of resin to dental porcelain. Dent Mater. 8:1992;238-240.
    • (1992) Dent Mater , vol.8 , pp. 238-240
    • Hayakawa, T.1    Horie, K.2    Aida, M.3    Kanaya, H.4    Kobayashi, T.5    Murata, Y.6
  • 2
    • 0017932633 scopus 로고
    • Composite resins bonded to porcelain with silane solution
    • Newburg R., Pameijer C.H. Composite resins bonded to porcelain with silane solution. J Am Dent Assoc. 96:1978;288-291.
    • (1978) J Am Dent Assoc , vol.96 , pp. 288-291
    • Newburg, R.1    Pameijer, C.H.2
  • 4
    • 0010936471 scopus 로고
    • Fourier transform infrared spectroscopic study of the structure of silane coupling agent on E-glass fiber
    • Ishida H., Koenig J.L. Fourier transform infrared spectroscopic study of the structure of silane coupling agent on E-glass fiber. J Colloid Interface Sci. 64:(3):1978;565-576.
    • (1978) J Colloid Interface Sci , vol.64 , Issue.3 , pp. 565-576
    • Ishida, H.1    Koenig, J.L.2
  • 5
    • 0025798788 scopus 로고
    • Hydrolysis and condensation of alkoxysilanes investigated by internal reflection FTIR spectroscopy
    • Leyden D.E., Atwater J.B. Hydrolysis and condensation of alkoxysilanes investigated by internal reflection FTIR spectroscopy. J Adhesion Sci Technol. 5:(10):1991;815-829.
    • (1991) J Adhesion Sci Technol , vol.5 , Issue.10 , pp. 815-829
    • Leyden, D.E.1    Atwater, J.B.2
  • 6
    • 0027598804 scopus 로고
    • Composition, reactivity and surface interactions of three dental silane primers
    • Anagnostopoulos T., Eliades G., Palaghias G. Composition, reactivity and surface interactions of three dental silane primers. Dent Mater. 9:1993;182-190.
    • (1993) Dent Mater , vol.9 , pp. 182-190
    • Anagnostopoulos, T.1    Eliades, G.2    Palaghias, G.3
  • 7
    • 0024198476 scopus 로고
    • Effect of 6-month water storage on silane-treated resin/porcelain bonds
    • Stokes A.N., Hood J.A.A., Tidmarsh B.G. Effect of 6-month water storage on silane-treated resin/porcelain bonds. J Dent. 16:1988;294-296.
    • (1988) J Dent , vol.16 , pp. 294-296
    • Stokes, A.N.1    Hood, J.A.A.2    Tidmarsh, B.G.3
  • 8
    • 0031265663 scopus 로고    scopus 로고
    • Shear bond strength of feldspathic porcelain of two luting cements in combination with three surface treatments
    • Matsumara H., Kato H., Atsuta M. Shear bond strength of feldspathic porcelain of two luting cements in combination with three surface treatments. J Prosthet Dent. 78:1997;511-517.
    • (1997) J Prosthet Dent , vol.78 , pp. 511-517
    • Matsumara, H.1    Kato, H.2    Atsuta, M.3
  • 9
    • 0029299001 scopus 로고
    • Adhesion of composite to porcelain with various surface conditions
    • Aida M., Hayakawa T., Mizukawa K. Adhesion of composite to porcelain with various surface conditions. J Prosthet Dent. 73:1995;464-470.
    • (1995) J Prosthet Dent , vol.73 , pp. 464-470
    • Aida, M.1    Hayakawa, T.2    Mizukawa, K.3
  • 10
    • 3042849536 scopus 로고
    • Application method, timing, types of silane systems, bond strength testing
    • Abstr. No. 157
    • Della Bona A., Berry T., Barghi N. Application method, timing, types of silane systems, bond strength testing. J Dent Res. 71:1992;660. Abstr. No. 157.
    • (1992) J Dent Res , vol.71 , pp. 660
    • Della Bona, A.1    Berry, T.2    Barghi, N.3
  • 11
    • 0030075429 scopus 로고    scopus 로고
    • Bond strength and durability of porcelain bonding systems
    • Kato H., Matsumara H., Tanaka T., Atsuta M. Bond strength and durability of porcelain bonding systems. J Prosthet Dent. 75:1996;163-168.
    • (1996) J Prosthet Dent , vol.75 , pp. 163-168
    • Kato, H.1    Matsumara, H.2    Tanaka, T.3    Atsuta, M.4
  • 12
    • 0033144208 scopus 로고    scopus 로고
    • Effect of water storage on the silanization in porcelain repair strength
    • Berry T., Barghi N., Chung K. Effect of water storage on the silanization in porcelain repair strength. J Oral Rehabil. 26:(6):1999;459-463.
    • (1999) J Oral Rehabil , vol.26 , Issue.6 , pp. 459-463
    • Berry, T.1    Barghi, N.2    Chung, K.3
  • 13
    • 0029372422 scopus 로고
    • Shear vs. tensile bond strength of resin composite to ceramic
    • Della Bona A., van Noort R. Shear vs. tensile bond strength of resin composite to ceramic. J Dent Res. 74:(9):1995;1591-1596.
    • (1995) J Dent Res , vol.74 , Issue.9 , pp. 1591-1596
    • Della Bona, A.1    Van Noort, R.2
  • 15
    • 0031158361 scopus 로고    scopus 로고
    • Why do shear bond tests pull out dentin?
    • Versluis A., Tantbirojn D., Douglas W.H. Why do shear bond tests pull out dentin? J Dent Res. 76:1997;1298-1307.
    • (1997) J Dent Res , vol.76 , pp. 1298-1307
    • Versluis, A.1    Tantbirojn, D.2    Douglas, W.H.3
  • 16
    • 0036497561 scopus 로고    scopus 로고
    • Bond durability of the resin-bonded and silane treated ceramic surface
    • Hooshmand T., van Noort R., Keshvad A. Bond durability of the resin-bonded and silane treated ceramic surface. Dent Mater. 18:2002;179-188.
    • (2002) Dent Mater , vol.18 , pp. 179-188
    • Hooshmand, T.1    Van Noort, R.2    Keshvad, A.3
  • 17
    • 0018018346 scopus 로고
    • From treating solution to filler surface and beyond. The life history of a silane coupling agent
    • Rosen M.R. From treating solution to filler surface and beyond. The life history of a silane coupling agent. J Coat Technol. 50:(644):1978;70-82.
    • (1978) J Coat Technol , vol.50 , Issue.644 , pp. 70-82
    • Rosen, M.R.1
  • 18
    • 0025725580 scopus 로고
    • Hydrolysis, adsorption, and dynamics of silane coupling agents on silica surfaces
    • Blum F.D., Meesiri W., Kang H., Gambogi J.E. Hydrolysis, adsorption, and dynamics of silane coupling agents on silica surfaces. J Adhesion Sci Technol. 5:(6):1991;479-496.
    • (1991) J Adhesion Sci Technol , vol.5 , Issue.6 , pp. 479-496
    • Blum, F.D.1    Meesiri, W.2    Kang, H.3    Gambogi, J.E.4
  • 19
    • 0010936471 scopus 로고
    • Fourier transform infrared spectroscopic study of the structure of silane coupling agent on E-glass fiber
    • Ishida H., Koenig J.L. Fourier transform infrared spectroscopic study of the structure of silane coupling agent on E-glass fiber. J Colloid Interface Sci. 64:(3):1978;565-576.
    • (1978) J Colloid Interface Sci , vol.64 , Issue.3 , pp. 565-576
    • Ishida, H.1    Koenig, J.L.2
  • 20
    • 0021371210 scopus 로고
    • Structure and adsorption characteristics of silane coupling agents on silica and E-glass; dependence on pH
    • Naviroj S., Culler S.R., Koeing J.L., Ishida H. Structure and adsorption characteristics of silane coupling agents on silica and E-glass; dependence on pH. J Colloid Interface Sci. 97:(2):1984;308-317.
    • (1984) J Colloid Interface Sci , vol.97 , Issue.2 , pp. 308-317
    • Naviroj, S.1    Culler, S.R.2    Koeing, J.L.3    Ishida, H.4
  • 21
    • 0021408305 scopus 로고
    • Characterization of silane-treated glass fibers by diffuse reflectance Fourier transform spectroscopy
    • Graf R.T., Koenig J.L., Ishida H. Characterization of silane-treated glass fibers by diffuse reflectance Fourier transform spectroscopy. Anal Chem. 56:1984;773-778.
    • (1984) Anal Chem , vol.56 , pp. 773-778
    • Graf, R.T.1    Koenig, J.L.2    Ishida, H.3
  • 22
    • 0001043555 scopus 로고
    • Tracer study of kinetics and mechanism of hydrolytically induced interfacial failure
    • Schrader M.E., Block A. Tracer study of kinetics and mechanism of hydrolytically induced interfacial failure. J Polym Sci. 34C:1971;281-291.
    • (1971) J Polym Sci , vol.34 C , pp. 281-291
    • Schrader, M.E.1    Block, A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.