1
-
-
0035749346
-
The metal-free practice: Myth? Reality? Desirable goal?
-
F.M. Spear The metal-free practice: Myth? Reality? Desirable goal? J Esthet Restor Dent 13 2001 59 67
-
(2001)
J Esthet Restor Dent
, vol.13
, pp. 59-67
-
-
Spear, F.M.1
-
2
-
-
0021403252
-
Long-term clinical study of porcelain-fused-to-gold restorations
-
J. Coornaert, P. Adriaens, and J. De Boever Long-term clinical study of porcelain-fused-to-gold restorations J Prosthet Dent 51 1984 338 342
-
(1984)
J Prosthet Dent
, vol.51
, pp. 338-342
-
-
Coornaert, J.1
Adriaens, P.2
De Boever, J.3
-
5
-
-
0033223147
-
A 10-year longitudinal study of fixed prosthodontics: Clinical characteristics and outcome of single-unit metal-ceramic crowns
-
T.R. Walton A 10-year longitudinal study of fixed prosthodontics: clinical characteristics and outcome of single-unit metal-ceramic crowns Int J Prosthodont 12 1999 519 526
-
(1999)
Int J Prosthodont
, vol.12
, pp. 519-526
-
-
Walton, T.R.1
-
6
-
-
0028412610
-
Five years' clinical experience with a leucite-reinforced porcelain crown system
-
J.A. Hankinson, and E.G. Cappetta Five years' clinical experience with a leucite-reinforced porcelain crown system Int J Periodontics Restorative Dent 14 1994 138 153
-
(1994)
Int J Periodontics Restorative Dent
, vol.14
, pp. 138-153
-
-
Hankinson, J.A.1
Cappetta, E.G.2
-
9
-
-
0035502392
-
Procera All Ceram crowns followed for 5 to 10.5 years: A prospective clinical study
-
P. Odman, and B. Andersson Procera All Ceram crowns followed for 5 to 10.5 years: a prospective clinical study Int J Prosthodont 14 2001 504 509
-
(2001)
Int J Prosthodont
, vol.14
, pp. 504-509
-
-
Odman, P.1
Andersson, B.2
-
11
-
-
0025492382
-
Fracture surface analysis of dental ceramics: Clinically failed restorations
-
J.R. Kelly, R. Giordano, R. Pober, and M.J. Cima Fracture surface analysis of dental ceramics: clinically failed restorations Int J Prosthodont 3 1990 430 440
-
(1990)
Int J Prosthodont
, vol.3
, pp. 430-440
-
-
Kelly, J.R.1
Giordano, R.2
Pober, R.3
Cima, M.J.4
-
12
-
-
0028369111
-
Effect of surface etching on the flexure strength and fracture toughness of Dicor disks containing controlled flaws
-
J.Y. Thompson, and K.J. Anusavice Effect of surface etching on the flexure strength and fracture toughness of Dicor disks containing controlled flaws J Dent Res 73 1994 505 510 [Erratum in: J Dent Res 1994;73:710]
-
(1994)
J Dent Res
, vol.73
, pp. 505-510
-
-
Thompson, J.Y.1
Anusavice, K.J.2
-
13
-
-
0034202903
-
Effects of surface treatments on shear bond strengths between a resin cement and an alumina core
-
M. Madani, F.C. Chu, A.V. McDonald, and R.J. Smales Effects of surface treatments on shear bond strengths between a resin cement and an alumina core J Prosthet Dent 83 2000 644 647
-
(2000)
J Prosthet Dent
, vol.83
, pp. 644-647
-
-
Madani, M.1
Chu, F.C.2
McDonald, A.V.3
Smales, R.J.4
-
14
-
-
0028523833
-
Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain
-
J.W. Thurmond, W.W. Barkmeier, and T.M. Wilwerding Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain J Prosthet Dent 72 1994 355 359
-
(1994)
J Prosthet Dent
, vol.72
, pp. 355-359
-
-
Thurmond, J.W.1
Barkmeier, W.W.2
Wilwerding, T.M.3
-
15
-
-
1842855215
-
Durability of the resin bond strength to the alumina ceramic procera
-
M. Hummel, and M. Kern Durability of the resin bond strength to the alumina ceramic procera Dent Mater 20 2004 498 508
-
(2004)
Dent Mater
, vol.20
, pp. 498-508
-
-
Hummel, M.1
Kern, M.2
-
16
-
-
0041888380
-
Effect of surface topography on the bond strength of a composite to three different types of ceramic
-
O. Won-suck, and C. Shen Effect of surface topography on the bond strength of a composite to three different types of ceramic J Prosthet Dent 90 2003 241 246
-
(2003)
J Prosthet Dent
, vol.90
, pp. 241-246
-
-
Won-Suck, O.1
Shen, C.2
-
17
-
-
0033222358
-
The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
-
T. Kosmac, C. Oblak, P. Jevnikar, N. Funduk, and L. Marion The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic Dent Mater 15 1999 426 433
-
(1999)
Dent Mater
, vol.15
, pp. 426-433
-
-
Kosmac, T.1
Oblak, C.2
Jevnikar, P.3
Funduk, N.4
Marion, L.5
-
18
-
-
0034331731
-
The influence of surface roughness on porcelain strength
-
N. De Jager, A.J. Feilzer, and C.L. Davidson The influence of surface roughness on porcelain strength Dent Mater 16 2000 381 388
-
(2000)
Dent Mater
, vol.16
, pp. 381-388
-
-
De Jager, N.1
Feilzer, A.J.2
Davidson, C.L.3
-
19
-
-
5244274356
-
The effects of hydrofluoric acid etching on the strength of glasses
-
B. Proctor The effects of hydrofluoric acid etching on the strength of glasses Phys Chem Glasses 3 1962 7 27
-
(1962)
Phys Chem Glasses
, vol.3
, pp. 7-27
-
-
Proctor, B.1
-
20
-
-
0023348257
-
2 glass strength improvement by etching
-
2 glass strength improvement by etching Am Ceram Soc Bull 66 1987 807 809
-
(1987)
Am Ceram Soc Bull
, vol.66
, pp. 807-809
-
-
Kobayashi, K.1
-
21
-
-
84980127254
-
Experimental study of fracture of glass: I, the fracture process
-
E.B. Shand Experimental study of fracture of glass: I, the fracture process J Am Ceram Soc 37 1954 52 60
-
(1954)
J Am Ceram Soc
, vol.37
, pp. 52-60
-
-
Shand, E.B.1
-
22
-
-
2542554125
-
Fracture in polycrystalline ceramics
-
H. Liebowitz Academic Press New York
-
R.L. Coble, and N.M. Parikh Fracture in polycrystalline ceramics H. Liebowitz Fracture: an advanced treatise 1972 Academic Press New York 243 310
-
(1972)
Fracture: An Advanced Treatise
, pp. 243-310
-
-
Coble, R.L.1
Parikh, N.M.2
-
24
-
-
0020843026
-
Effect of chemical etching on the strength of undamaged glass
-
L.G. Bailova, V.P. Pukh, and T.I. Pesina Effect of chemical etching on the strength of undamaged glass Soviet J Glass Phys Chem 9 1983 452 456
-
(1983)
Soviet J Glass Phys Chem
, vol.9
, pp. 452-456
-
-
Bailova, L.G.1
Pukh, V.P.2
Pesina, T.I.3
-
25
-
-
0018797988
-
Effect of etching on the strength of aluminous porcelain jacket crowns
-
M.A. Hussain, E.W. Bradford, and G. Charlton Effect of etching on the strength of aluminous porcelain jacket crowns Br Dent J 147 1979 89 90
-
(1979)
Br Dent J
, vol.147
, pp. 89-90
-
-
Hussain, M.A.1
Bradford, E.W.2
Charlton, G.3
-
26
-
-
0027661848
-
Effect of acid etching on the flexural strength of a feldspathic porcelain and a castable glass ceramic
-
T.W. Yen, R.B. Blackman, and R.J. Baez Effect of acid etching on the flexural strength of a feldspathic porcelain and a castable glass ceramic J Prosthet Dent 70 1993 224 233
-
(1993)
J Prosthet Dent
, vol.70
, pp. 224-233
-
-
Yen, T.W.1
Blackman, R.B.2
Baez, R.J.3
-
27
-
-
0035514971
-
Survival of Dicor glass-ceramic dental restorations over 16 years. Part III: Effect of luting agent and tooth or tooth-substitute core structure
-
K.A. Malament, and S.S. Socransky Survival of Dicor glass-ceramic dental restorations over 16 years. Part III: Effect of luting agent and tooth or tooth-substitute core structure J Prosthet Dent 86 2001 511 519
-
(2001)
J Prosthet Dent
, vol.86
, pp. 511-519
-
-
Malament, K.A.1
Socransky, S.S.2
-
28
-
-
0032608003
-
Survival of Dicor glass-ceramic dental restorations over 14 years: Part I. Survival of Dicor complete coverage restorations and effect of internal surface acid etching, tooth position, gender, and age
-
K.A. Malament, and S.S. Socransky Survival of Dicor glass-ceramic dental restorations over 14 years: Part I. Survival of Dicor complete coverage restorations and effect of internal surface acid etching, tooth position, gender, and age J Prosthet Dent 81 1999 23 32
-
(1999)
J Prosthet Dent
, vol.81
, pp. 23-32
-
-
Malament, K.A.1
Socransky, S.S.2
-
29
-
-
0034174580
-
Role of adhesive interlayer on transverse fracture of brittle layer structures
-
H. Chai, and B. Lawn Role of adhesive interlayer on transverse fracture of brittle layer structures J Mater Res 15 2000 1017 1024
-
(2000)
J Mater Res
, vol.15
, pp. 1017-1024
-
-
Chai, H.1
Lawn, B.2
|