The oxidation of aluminum in dry oxygen in the temperature range 400-650°C
-
D. W. Aylmore, S. J. Gregg, and W. B. Jepson, "The Oxidation of Aluminum in Dry Oxygen in the Temperature Range 400-650°C," J. Inst. Met., 88, 205-8 (1959).
-
(1959)
J. Inst. Met.
, vol.88
, pp. 205-208
-
-
Aylmore, D.W.1
Gregg, S.J.2
Jepson, W.B.3
-
2
-
-
84975348619
-
Oxidation of aluminum in the temperature range 400°C-600°C
-
W. W. Smeltzer, "Oxidation of Aluminum in the Temperature Range 400°C-600°C," J. Electrochem. Soc., 103 [4] 209-14 (1956).
-
(1956)
J. Electrochem. Soc.
, vol.103
, Issue.4
, pp. 209-214
-
-
Smeltzer, W.W.1
-
4
-
-
0002549784
-
The kinetics of the oxidation of Al in oxygen at high temperature
-
A. F. Beck, M. A. Heine, E. J. Caule, and M. J. Pryor, "The Kinetics of the Oxidation of Al in Oxygen at High Temperature," Corrosion Science, 7, 1-22 (1967).
-
(1967)
Corrosion Science
, vol.7
, pp. 1-22
-
-
Beck, A.F.1
Heine, M.A.2
Caule, E.J.3
Pryor, M.J.4
-
5
-
-
0016576039
-
In situ observations of crystalline oxide formation during aluminum and aluminum alloy oxidation
-
G. M. Scamans and E. P. Butler, "In Situ Observations of Crystalline Oxide Formation During Aluminum and Aluminum Alloy Oxidation," Metall. Trans. A, 6, 2055-63 (1975).
-
(1975)
Metall. Trans. A
, vol.6
, pp. 2055-2063
-
-
Scamans, G.M.1
Butler, E.P.2
-
6
-
-
84948219533
-
Natural and thermally formed oxide films on aluminum
-
M. S. Hunter and P. Fowle, "Natural and Thermally Formed Oxide Films on Aluminum," J. Electrochem. Soc., 103 [9] 482-5 (1956).
-
(1956)
J. Electrochem. Soc.
, vol.103
, Issue.9
, pp. 482-485
-
-
Hunter, M.S.1
Fowle, P.2
-
7
-
-
0028530736
-
Effect of processing parameters on phase and microstructure evolution in RBAO ceramics
-
D. Holz, S. Wu, S. Scheppokat, and N. Claussen, "Effect of Processing Parameters on Phase and Microstructure Evolution in RBAO Ceramics," J. Am. Ceram. Soc., 77 [10] 2509-17 (1994).
-
(1994)
J. Am. Ceram. Soc.
, vol.77
, Issue.10
, pp. 2509-2517
-
-
Holz, D.1
Wu, S.2
Scheppokat, S.3
Claussen, N.4
-
8
-
-
0029352499
-
Reaction Bonding of Aluminum Oxide (RBAO)
-
N. Claussen, R. Janssen, and D. Holz, "Reaction Bonding of Aluminum Oxide (RBAO)," J. Ceram. Soc. Japan, 103 [8] 749-58 (1995).
-
(1995)
J. Ceram. Soc. Japan
, vol.103
, Issue.8
, pp. 749-758
-
-
Claussen, N.1
Janssen, R.2
Holz, D.3
-
9
-
-
29744469928
-
Reaction Bonded Aluminum Oxide (RBAO) - A material for rapid product development
-
Stuttgart
-
M. Roger, R. Discherl, R. Janssen, and N. Claussen. "Reaction Bonded Aluminum Oxide (RBAO) - A Material for Rapid Product Development;" pp. 265-74, Proceedings of the International Consortium on Rapid Product Development, Stuttgart, 1997.
-
(1997)
Proceedings of the International Consortium on Rapid Product Development
, pp. 265-274
-
-
Roger, M.1
Discherl, R.2
Janssen, R.3
Claussen, N.4
-
10
-
-
0030214114
-
Oxidation of an aluminum-0,4wt% magnesium alloy
-
D. H. Kim, E. P. Yoon, and J. S. Kim, "Oxidation of an Aluminum-0,4wt% Magnesium Alloy," J. Mater. Sci. Lett., 15, 1429-31 (1996).
-
(1996)
J. Mater. Sci. Lett.
, vol.15
, pp. 1429-1431
-
-
Kim, D.H.1
Yoon, E.P.2
Kim, J.S.3
-
11
-
-
0014999208
-
Oxidation of a dilute aluminum magnesium alloy
-
I. M. Ritchie, J. V. Sanders, and P. L. Weickhardt, "Oxidation of a Dilute Aluminum Magnesium Alloy," Oxid. Met., 3 [1] 91-101 (1971).
-
(1971)
Oxid. Met.
, vol.3
, Issue.1
, pp. 91-101
-
-
Ritchie, I.M.1
Sanders, J.V.2
Weickhardt, P.L.3
-
12
-
-
0001877594
-
High-temperature oxidation of Al-Mg-alloys
-
M. H. Zayan, O. M. Jamjoom, and N. A. Razik, "High-Temperature Oxidation of Al-Mg-Alloys," Oxid. Met., 34 [3/4] 323-33 (1990).
-
(1990)
Oxid. Met.
, vol.34
, Issue.3-4
, pp. 323-333
-
-
Zayan, M.H.1
Jamjoom, O.M.2
Razik, N.A.3
-
13
-
-
0023305813
-
The high temperature oxidation of Al-4.2 wt. pet. Mg alloy
-
D. J. Field, G. M. Scamans, and E. P. Butler, "The High Temperature Oxidation of Al-4.2 wt. pet. Mg Alloy," Metall. Trans. A, 18, 463-72 (1987).
-
(1987)
Metall. Trans. A
, vol.18
, pp. 463-472
-
-
Field, D.J.1
Scamans, G.M.2
Butler, E.P.3
-
14
-
-
0020809766
-
Oxidation of molten Al-Mg alloys
-
I. Haginoya and T. Fukusako, "Oxidation of Molten Al-Mg Alloys," Trans. Jpn. Inst. Met, 24 [9] 613-9 (1983).
-
(1983)
Trans. Jpn. Inst. Met
, vol.24
, Issue.9
, pp. 613-619
-
-
Haginoya, I.1
Fukusako, T.2
-
15
-
-
0022593510
-
Formation of lanxide ceramic composite materials
-
M. S. Newkirk, A. W. Urquhart, H. R. Zwicker, and E. Breval, "Formation of Lanxide Ceramic Composite Materials," J. Mater. Res., 1 [1] 81-9 (1986).
-
(1986)
J. Mater. Res.
, vol.1
, Issue.1
, pp. 81-89
-
-
Newkirk, M.S.1
Urquhart, A.W.2
Zwicker, H.R.3
Breval, E.4
-
16
-
-
0026221278
-
3/Al alloy composites
-
3/Al Alloy Composites," J. Mater. Res., 6 [9] 1982-95 (1991).
-
(1991)
J. Mater. Res.
, vol.6
, Issue.9
, pp. 1982-1995
-
-
Vlach, K.C.1
Salas, O.2
Ni, H.3
Jayaram, V.4
Levi, C.G.5
Mehrabian, R.6
-
17
-
-
0029271564
-
Early stages of composite formation by oxidation of liquid aluminum alloys
-
O. Salas, H. Ni, V. Jayaram, K. C. Vlach, C. G. Levi, and R. Mehrabian, "Early Stages of Composite Formation by Oxidation of Liquid Aluminum Alloys," J. Am. Ceram. Soc., 78 [3] 609-22 (1995).
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.3
, pp. 609-622
-
-
Salas, O.1
Ni, H.2
Jayaram, V.3
Vlach, K.C.4
Levi, C.G.5
Mehrabian, R.6
-
19
-
-
0029321588
-
Microstructural development in the Directed Melt-Oxidized (DIMOX) Al-Mg-Si alloys
-
V. S. R. Murthy and B. S. Rao, "Microstructural Development in the Directed Melt-Oxidized (DIMOX) Al-Mg-Si Alloys," J. Mater. Sci., 30, 3091-7 (1995).
-
(1995)
J. Mater. Sci.
, vol.30
, pp. 3091-3097
-
-
Murthy, V.S.R.1
Rao, B.S.2
-
20
-
-
0026219865
-
3/metal composites by oxidation of aluminum alloys
-
3/Metal Composites by Oxidation of Aluminum Alloys," J. Mater. Res., 6, 1964-81 (1991).
-
(1991)
J. Mater. Res.
, vol.6
, pp. 1964-1981
-
-
Salas, O.1
Ni, H.2
Jayaram, V.3
Vlach, K.C.4
Levi, C.G.5
Mehrabian, R.6
-
21
-
-
0028478665
-
Alumina/aluminum composites formed by the directed oxidation of aluminum using magnesia as a surface dopant
-
P. Xiao and B. Derby, "Alumina/Aluminum Composites Formed by the Directed Oxidation of Aluminum Using Magnesia as a Surface Dopant," J. Am. Ceram. Soc., 77 [7] 1761-70 (1994).
-
(1994)
J. Am. Ceram. Soc.
, vol.77
, Issue.7
, pp. 1761-1770
-
-
Xiao, P.1
Derby, B.2
-
23
-
-
0034226791
-
Deterioration in the final stage sintering of magnesium aluminate spinel
-
C.-J. Ting and H.-Y. Lu, "Deterioration in the Final Stage Sintering of Magnesium Aluminate Spinel," J. Am. Ceram. Soc, 83 [7] 1592-8 (2000).
-
(2000)
J. Am. Ceram. Soc
, vol.83
, Issue.7
, pp. 1592-1598
-
-
Ting, C.-J.1
Lu, H.-Y.2
-
24
-
-
0034319613
-
Fabrication of translucent magnesium aluminum spinel ceramics
-
J.-G. Li, T. Ikegami, J.-H. Lee, and T. Mori, "Fabrication of Translucent Magnesium Aluminum Spinel Ceramics," J. Am. Ceram. Soc., 83 [11] 2866-8 (2000).
-
(2000)
J. Am. Ceram. Soc.
, vol.83
, Issue.11
, pp. 2866-2868
-
-
Li, J.-G.1
Ikegami, T.2
Lee, J.-H.3
Mori, T.4
-
25
-
-
0344012219
-
Synthesis of magnesium aluminate spinel platelets from a-alumina platelet and magnesium sulfate precursors
-
S. Hashimoto, S. Zhang, W. E. Lee, and A. Yamaguchi, "Synthesis of Magnesium Aluminate Spinel Platelets from a-Alumina Platelet and Magnesium Sulfate Precursors," J. Am. Ceram. Soc., 86 [11] 1959-61 (2003).
-
(2003)
J. Am. Ceram. Soc.
, vol.86
, Issue.11
, pp. 1959-1961
-
-
Hashimoto, S.1
Zhang, S.2
Lee, W.E.3
Yamaguchi, A.4
-
26
-
-
0024051051
-
Wettability of monocrystalline alumina by aluminum between its melting point and 1273 K
-
V. Laurent, D. Chatain, C. Chatillon, and N. Eustathopoulos, "Wettability of Monocrystalline Alumina by Aluminum Between its Melting Point and 1273 K," Acta Metall., 36, 1797-803 (1988).
-
(1988)
Acta Metall.
, vol.36
, pp. 1797-1803
-
-
Laurent, V.1
Chatain, D.2
Chatillon, C.3
Eustathopoulos, N.4
-
27
-
-
0001858650
-
Wetting of aluminum oxide by molten aluminum and other metals
-
J. A. Champion, B. J. Keene, and J. M. Sillwood, "Wetting of Aluminum Oxide by Molten Aluminum and Other Metals," J. Mater. Sci., 4, 39-49 (1969).
-
(1969)
J. Mater. Sci.
, vol.4
, pp. 39-49
-
-
Champion, J.A.1
Keene, B.J.2
Sillwood, J.M.3
-
28
-
-
0024281753
-
Interfacial phenomena involving liquid metals and solid oxides in the Mg-Al-O system
-
D. A. Weihrauch Jr., "Interfacial Phenomena Involving Liquid Metals and Solid Oxides in the Mg-Al-O System," J. Mater. Res., 4, 729-39 (1988).
-
(1988)
J. Mater. Res.
, vol.4
, pp. 729-739
-
-
Weihrauch Jr., D.A.1
-
29
-
-
0030242525
-
Equilibrium contact angle in the magnesium oxide/aluminum system
-
H. Fujii and H. Nakae, "Equilibrium Contact Angle in the Magnesium Oxide/Aluminum System," Acta Mater., 44 [9] 3567-73 (1996).
-
(1996)
Acta Mater.
, vol.44
, Issue.9
, pp. 3567-3573
-
-
Fujii, H.1
Nakae, H.2
-
30
-
-
0016921595
-
Metal/non-metal interfaces. The wetting of magnesium oxide by aluminum and other metals
-
A. J. McEvoy, R. H. Williams, and I. G. Higginbotham, "Metal/Non-Metal Interfaces. The Wetting of Magnesium Oxide by Aluminum and Other Metals," J. Mater. Sci., 11, 297-302 (1976).
-
(1976)
J. Mater. Sci.
, vol.11
, pp. 297-302
-
-
McEvoy, A.J.1
Williams, R.H.2
Higginbotham, I.G.3
-
31
-
-
0001787446
-
Whisker-metal matrix bonding
-
S. M. Wolf, A. P. Levitt, and J. Brown, "Whisker-Metal Matrix Bonding," Chem. Eng. Prog., 62 [2] 74-8 (1966).
-
(1966)
Chem. Eng. Prog.
, vol.62
, Issue.2
, pp. 74-78
-
-
Wolf, S.M.1
Levitt, A.P.2
Brown, J.3
-
32
-
-
0021452740
-
Role of wettability in the preparation of metal-matrix composites (a review)
-
A. Banerji, P. K. Rohatgi, and W. Reif, "Role of Wettability in the Preparation of Metal-Matrix Composites (a Review)," Metall, 38 [7] 656-61 (1984).
-
(1984)
Metall
, vol.38
, Issue.7
, pp. 656-661
-
-
Banerji, A.1
Rohatgi, P.K.2
Reif, W.3
-
33
-
-
0012977802
-
Gas entrapment and evolution in prealloyed aluminum powders
-
J. L. Estrada, J. Duszczyk, and B. M. Korevaar, "Gas Entrapment and Evolution in Prealloyed Aluminum Powders," J. Mater. Sci., 26, 1431-42 (1991).
-
(1991)
J. Mater. Sci.
, vol.26
, pp. 1431-1442
-
-
Estrada, J.L.1
Duszczyk, J.2
Korevaar, B.M.3
|