2
-
-
0027604980
-
Bonding durability of photocured phenyl-P in TEGDMA to smear layer-retained bovine dentin
-
Watanabe I, Nakabayashi N. Bonding durability of photocured phenyl-P in TEGDMA to smear layer-retained bovine dentin. Quintessence Int 1993;24:335-342.
-
(1993)
Quintessence Int
, vol.24
, pp. 335-342
-
-
Watanabe, I.1
Nakabayashi, N.2
-
3
-
-
0033233508
-
Durability of resin-dentin bonds
-
Shono Y, Terashita M, Shimada J, Kozono Y, Carvalho RM, Russell CM, Pashley DH. Durability of resin-dentin bonds. J Adhes Dent 1999;1:211-218.
-
(1999)
J Adhes Dent
, vol.1
, pp. 211-218
-
-
Shono, Y.1
Terashita, M.2
Shimada, J.3
Kozono, Y.4
Carvalho, R.M.5
Russell, C.M.6
Pashley, D.H.7
-
4
-
-
0035350653
-
The influence of water storage and C-factor on the dentin-resin composite microtensile bond strength and debond pathway utilizing a filled and unfilled adhesive resin
-
Armstrong SR, Keller JC, Boyer DB. The influence of water storage and C-factor on the dentin-resin composite microtensile bond strength and debond pathway utilizing a filled and unfilled adhesive resin. Dent Mater 2001;17:268-276.
-
(2001)
Dent Mater
, vol.17
, pp. 268-276
-
-
Armstrong, S.R.1
Keller, J.C.2
Boyer, D.B.3
-
5
-
-
0033278196
-
Long-term durability of dentin bonds made with a self-etching primer, in vivo
-
Sano H, Yoshikawa T, Pereira PNR, Kanemura N, Morigama M, Tagami J, Pashley DH. Long-term durability of dentin bonds made with a self-etching primer, in vivo. J Dent Res 1999;78:906-911.
-
(1999)
J Dent Res
, vol.78
, pp. 906-911
-
-
Sano, H.1
Yoshikawa, T.2
Pereira, P.N.R.3
Kanemura, N.4
Morigama, M.5
Tagami, J.6
Pashley, D.H.7
-
6
-
-
0034443787
-
In vivo degradation of resin-dentin bonds in humans over 1 to 3 years
-
Hashimoto M, Ohno H, Kaga M, Endo K, Sano H, Oguchi H. In vivo degradation of resin-dentin bonds in humans over 1 to 3 years. J Dent Res 2000;79:1385-1391.
-
(2000)
J Dent Res
, vol.79
, pp. 1385-1391
-
-
Hashimoto, M.1
Ohno, H.2
Kaga, M.3
Endo, K.4
Sano, H.5
Oguchi, H.6
-
7
-
-
0035434420
-
Resin-tooth adhesive interfaces after long-term function
-
Hashimoto M, Ohno H, Kaga M, Endo K, Sano H, Oguchi H. Resin-tooth adhesive interfaces after long-term function. Am J Dent 2001;14:211-215.
-
(2001)
Am J Dent
, vol.14
, pp. 211-215
-
-
Hashimoto, M.1
Ohno, H.2
Kaga, M.3
Endo, K.4
Sano, H.5
Oguchi, H.6
-
8
-
-
0026811976
-
Identification of a resin-dentin hydrid layer in vital human dentin created in vivo: Durable bonding to vital dentin
-
Nakabayashi N, Ashizawa M, Nakamura M. Identification of a resin-dentin hydrid layer in vital human dentin created in vivo: Durable bonding to vital dentin. Quintessence Int 1992;23:135-141.
-
(1992)
Quintessence Int
, vol.23
, pp. 135-141
-
-
Nakabayashi, N.1
Ashizawa, M.2
Nakamura, M.3
-
9
-
-
0032062062
-
A tensile test to facilitate identification of defects in dentin bonded specimens
-
Nakabayashi N, Watanabe A, Arao T. A tensile test to facilitate identification of defects in dentin bonded specimens. J Dent 1998;26:379-385.
-
(1998)
J Dent
, vol.26
, pp. 379-385
-
-
Nakabayashi, N.1
Watanabe, A.2
Arao, T.3
-
10
-
-
0029171782
-
Nanolekeage: Leakage within the hydrid layer
-
Sano H, Takatsu T, Ciucchi B, Homer JA, Matthews WG, Pashley DH. Nanolekeage: Leakage within the hydrid layer. Oper Dent 1995;20:18-25.
-
(1995)
Oper Dent
, vol.20
, pp. 18-25
-
-
Sano, H.1
Takatsu, T.2
Ciucchi, B.3
Homer, J.A.4
Matthews, W.G.5
Pashley, D.H.6
-
11
-
-
0033222614
-
Effect of mechanical properties of resin composite on the efficacy of the dentin bonding systems
-
Hasegawa T, Itoh K, Koike T, Yukitani W, Hisamitsu H, Wakumoto S, Fujishima A. Effect of mechanical properties of resin composite on the efficacy of the dentin bonding systems. Oper Dent 1999;24:323-330.
-
(1999)
Oper Dent
, vol.24
, pp. 323-330
-
-
Hasegawa, T.1
Itoh, K.2
Koike, T.3
Yukitani, W.4
Hisamitsu, H.5
Wakumoto, S.6
Fujishima, A.7
-
12
-
-
0036580064
-
Effects of mechanical properties of adhesives on bond strength to dentin
-
Takahashi A, Sato Y, Uno S, Pereira PN, Sano H. Effects of mechanical properties of adhesives on bond strength to dentin. Dent Mater 2002;18:263-268.
-
(2002)
Dent Mater
, vol.18
, pp. 263-268
-
-
Takahashi, A.1
Sato, Y.2
Uno, S.3
Pereira, P.N.4
Sano, H.5
-
13
-
-
0034279952
-
Long-term mechanical properties of EDTA-demineralized dentin matrix
-
Carvalho RM, Tay FR, Sano H, Yoshiyama M, Pashley DH. Long-term mechanical properties of EDTA-demineralized dentin matrix. J Adhes Dent 2000;2:193-199.
-
(2000)
J Adhes Dent
, vol.2
, pp. 193-199
-
-
Carvalho, R.M.1
Tay, F.R.2
Sano, H.3
Yoshiyama, M.4
Pashley, D.H.5
-
14
-
-
0035011396
-
Relation of dental composite formulations to their degradation and release of hydrolyzed polymericresin-derived products
-
Santerre JP, Shajii L, Leung BW. Relation of dental composite formulations to their degradation and release of hydrolyzed polymericresin- derived products. Crit Rev Oral Biol Med 2001;12:136-151.
-
(2001)
Crit Rev Oral Biol Med
, vol.12
, pp. 136-151
-
-
Santerre, J.P.1
Shajii, L.2
Leung, B.W.3
-
15
-
-
0030033719
-
Mechanism of polymer degradation and erosion
-
Göpferich A. Mechanism of polymer degradation and erosion. Biomaterials 1996;17:103-114.
-
(1996)
Biomaterials
, vol.17
, pp. 103-114
-
-
Göpferich, A.1
-
16
-
-
0026059172
-
Physico-mechanical properties of degradable polymers used in medical applications: A comparative study
-
Engelberg I, Kohn J. Physico-mechanical properties of degradable polymers used in medical applications: A comparative study. Biomaterials 1991;12:292-304.
-
(1991)
Biomaterials
, vol.12
, pp. 292-304
-
-
Engelberg, I.1
Kohn, J.2
-
17
-
-
0027572106
-
Effect of crosslinking agent content, monomer functionally, and repeat unit chemistry on properties of unfilled resins
-
Beatty MW, Swartz ML, Moore BK, Phillips RW, Roberts TA. Effect of crosslinking agent content, monomer functionally, and repeat unit chemistry on properties of unfilled resins. J Biomed Mater Res 1993;27:403-413.
-
(1993)
J Biomed Mater Res
, vol.27
, pp. 403-413
-
-
Beatty, M.W.1
Swartz, M.L.2
Moore, B.K.3
Phillips, R.W.4
Roberts, T.A.5
-
18
-
-
0033085891
-
Correlation of dentin bond durability with water absorption of bonding layer
-
Tanaka J, Ishikawa K, Yatani H, Yamashita A, Suzuki K. Correlation of dentin bond durability with water absorption of bonding layer. Dent Mater J 1999;18:11-18.
-
(1999)
Dent Mater J
, vol.18
, pp. 11-18
-
-
Tanaka, J.1
Ishikawa, K.2
Yatani, H.3
Yamashita, A.4
Suzuki, K.5
-
19
-
-
0025508450
-
Rate of elution of leachable components from composite
-
Ferracane JL, Condon JR. Rate of elution of leachable components from composite. Dent Mater 1990;6:282-287.
-
(1990)
Dent Mater
, vol.6
, pp. 282-287
-
-
Ferracane, J.L.1
Condon, J.R.2
-
21
-
-
0035227053
-
Influence of pH and storage time on the sorption and solubility behaviour of three composite resin materials
-
Örtengren U, Andersson F, Elgh U, Terselius B, Karlsson S. Influence of pH and storage time on the sorption and solubility behaviour of three composite resin materials. J Dent 2001;29:35-41.
-
(2001)
J Dent
, vol.29
, pp. 35-41
-
-
Örtengren, U.1
Andersson, F.2
Elgh, U.3
Terselius, B.4
Karlsson, S.5
-
22
-
-
0033288182
-
Water sorption of several bonding resins
-
Burrow MF, Inokoshi S, Tagami J. Water sorption of several bonding resins. Am J Dent 1999;12:295-298.
-
(1999)
Am J Dent
, vol.12
, pp. 295-298
-
-
Burrow, M.F.1
Inokoshi, S.2
Tagami, J.3
-
23
-
-
0032488231
-
In vitro aging of dental composites in water. Effect of degree of conversion, filler volume, and filler/matrix coupling
-
Ferracane JL, Berge HX, Condon JR. In vitro aging of dental composites in water. Effect of degree of conversion, filler volume, and filler/matrix coupling. J Biomed Mater Res 1998;42:465-472.
-
(1998)
J Biomed Mater Res
, vol.42
, pp. 465-472
-
-
Ferracane, J.L.1
Berge, H.X.2
Condon, J.R.3
-
24
-
-
0033088522
-
Effect of water content on the physical properties of model dentin primer and bonding resins
-
Paul SJ, Leach M, Rueggeberg FA, Pashley DH. Effect of water content on the physical properties of model dentin primer and bonding resins. J Dent 1999;27:209-214.
-
(1999)
J Dent
, vol.27
, pp. 209-214
-
-
Paul, S.J.1
Leach, M.2
Rueggeberg, F.A.3
Pashley, D.H.4
-
25
-
-
0021689933
-
Water absorption characteristics of dental microfine composite filling materials. II. Experimental materials
-
Braden M. Water absorption characteristics of dental microfine composite filling materials. II. Experimental materials. Biomaterials 1984;5:373-375.
-
(1984)
Biomaterials
, vol.5
, pp. 373-375
-
-
Braden, M.1
-
26
-
-
0035753917
-
Water sorption and solubility of dental composites and identification of monomers released in an aqueous environment
-
Örtengren U, Wellendorf H, Karlsson S, Ruytor IE. Water sorption and solubility of dental composites and identification of monomers released in an aqueous environment. J Oral Rehabil 2001;28:1106-1115.
-
(2001)
J Oral Rehabil
, vol.28
, pp. 1106-1115
-
-
Örtengren, U.1
Wellendorf, H.2
Karlsson, S.3
Ruytor, I.E.4
-
27
-
-
0035892391
-
The stability of methacrylate biomaterials when enzyme challenged: Kinetic and systematic evaluation
-
Yourtee DM, Smith RE, Russo KA, Burmaster S, Cannon JM, Eick JD, Kostoryz EL. The stability of methacrylate biomaterials when enzyme challenged: Kinetic and systematic evaluation. J Biomed Mater Res 2001;57:522-531.
-
(2001)
J Biomed Mater Res
, vol.57
, pp. 522-531
-
-
Yourtee, D.M.1
Smith, R.E.2
Russo, K.A.3
Burmaster, S.4
Cannon, J.M.5
Eick, J.D.6
Kostoryz, E.L.7
-
28
-
-
0033754376
-
The influence of storage solution on dentin bond durability of resin cement
-
Kitasako Y, Burrow MF, Nikaido T, Tagami J. The influence of storage solution on dentin bond durability of resin cement. Dent Mater 2000;16:1-6.
-
(2000)
Dent Mater
, vol.16
, pp. 1-6
-
-
Kitasako, Y.1
Burrow, M.F.2
Nikaido, T.3
Tagami, J.4
-
29
-
-
58149326616
-
Properties of heat-treated composites after aging in water
-
Ferracane JL, Hopkin JK, Condon JR. Properties of heat-treated composites after aging in water. Dent Mater 1995;11:354-358.
-
(1995)
Dent Mater
, vol.11
, pp. 354-358
-
-
Ferracane, J.L.1
Hopkin, J.K.2
Condon, J.R.3
-
30
-
-
0029281078
-
Tensile properties of resin-infiltrated demineralized human dentin
-
Sano H, Takatsu T, Ciucchi B, Russell CM, Pashley DH. Tensile properties of resin-infiltrated demineralized human dentin. J Dent Res 1995;74:1093-1102.
-
(1995)
J Dent Res
, vol.74
, pp. 1093-1102
-
-
Sano, H.1
Takatsu, T.2
Ciucchi, B.3
Russell, C.M.4
Pashley, D.H.5
-
31
-
-
0032133246
-
Ten-year clinical assessment of three posterior resin composites and two amalgams
-
Mair LH. Ten-year clinical assessment of three posterior resin composites and two amalgams. Quintessence Int 1998;29:483-490.
-
(1998)
Quintessence Int
, vol.29
, pp. 483-490
-
-
Mair, L.H.1
-
32
-
-
0033288181
-
1-year clinical evaluation of one-step in non-carious cervical lesions
-
Burrow MF, Tyas MJ. 1-year clinical evaluation of one-step in non-carious cervical lesions. Am J Dent 1999;12:283-285.
-
(1999)
Am J Dent
, vol.12
, pp. 283-285
-
-
Burrow, M.F.1
Tyas, M.J.2
-
33
-
-
0033140079
-
In vivo comparation of a microfilled and a hydrid minifilled composite resin in class III restoration: 2-Year follow-up
-
Reusens B, D'hoore W, Vreven J. In vivo comparation of a microfilled and a hydrid minifilled composite resin in class III restoration: 2-year follow-up. Clin Oral Investig 1999;3:62-69.
-
(1999)
Clin Oral Investig
, vol.3
, pp. 62-69
-
-
Reusens, B.1
D'hoore, W.2
Vreven, J.3
|