-
1
-
-
0035899584
-
High-strength Cu-based bulk glassy alloys in Cu-Zr-Ti and Cu-Hf-Ti ternary systems
-
A. Inoue, W. Zhang, T. Zhang, and K. Kurosaka: High-strength Cu-based bulk glassy alloys in Cu-Zr-Ti and Cu-Hf-Ti ternary systems. Acta Mater. 49, 2645 (2001).
-
(2001)
Acta Mater.
, vol.49
, pp. 2645
-
-
Inoue, A.1
Zhang, W.2
Zhang, T.3
Kurosaka, K.4
-
2
-
-
0036605134
-
Cu-based bulk glassy alloys with high tensile strength of over 2000 MPa
-
A. Inoue, W. Zhang, T. Zhang, and K. Kurosaka: Cu-based bulk glassy alloys with high tensile strength of over 2000 MPa. J. Non-Cryst. Solids 304, 200 (2002).
-
(2002)
J. Non-Cryst. Solids
, vol.304
, pp. 200
-
-
Inoue, A.1
Zhang, W.2
Zhang, T.3
Kurosaka, K.4
-
3
-
-
0039130878
-
Stabilization and high strain-rate superplasticity of metallic supercooled liquid
-
A. Inoue: Stabilization and high strain-rate superplasticity of metallic supercooled liquid. Mater. Sci. Eng. A 267, 171 (1999).
-
(1999)
Mater. Sci. Eng. A
, vol.267
, pp. 171
-
-
Inoue, A.1
-
5
-
-
3142775599
-
Catastrophic oxidation of Zr-TM (noble metals) glasses
-
L. Jastrow, U. Köster, and M. Meuris: Catastrophic oxidation of Zr-TM (noble metals) glasses. Mater. Sci. Eng. A 375-377, 440 (2004).
-
(2004)
Mater. Sci. Eng. A
, vol.375-377
, pp. 440
-
-
Jastrow, L.1
Köster, U.2
Meuris, M.3
-
6
-
-
0026121774
-
Oxidation and crystallization studies of Fe-22.5Al-10Zr rapidly solidified metallic glass ribbons
-
M.C. Kim and M.J. Mcnallan: Oxidation and crystallization studies of Fe-22.5Al-10Zr rapidly solidified metallic glass ribbons. Mater. Sci. Eng. A 134, 1078 (1991).
-
(1991)
Mater. Sci. Eng. A
, vol.134
, pp. 1078
-
-
Kim, M.C.1
Mcnallan, M.J.2
-
8
-
-
0023966730
-
The oxidation behavior of some cobalt-based amorphous-alloys
-
A.M. Dark, G. Wei, and B. Cantor: The oxidation behavior of some cobalt-based amorphous-alloys. Mater. Sci. Eng. 99, 533 (1988).
-
(1988)
Mater. Sci. Eng.
, vol.99
, pp. 533
-
-
Dark, A.M.1
Wei, G.2
Cantor, B.3
-
10
-
-
0035906783
-
Environmental properties of Zr-based metallic glasses and nanocrystalline alloys
-
U. Köster, D. Zander, Triwikantoro, A. Rüdiger, and L. Jastrow: Environmental properties of Zr-based metallic glasses and nanocrystalline alloys. Scripta Mater. 44, 1649 (2001).
-
(2001)
Scripta Mater.
, vol.44
, pp. 1649
-
-
Köster, U.1
Zander, D.2
Triwikantoro3
Rüdiger, A.4
Jastrow, L.5
-
11
-
-
0033309171
-
27.5
-
edited by W.L. Johnson, A. Inoue, and C.T. Liu (Mater. Res. Soc. Symp. Proc. Warrendale, PA)
-
27.5, in Bulk Metallic Glasses, edited by W.L. Johnson, A. Inoue, and C.T. Liu (Mater. Res. Soc. Symp. Proc. 554, Warrendale, PA, 1999), p. 167.
-
(1999)
Bulk Metallic Glasses
, vol.554
, pp. 167
-
-
Kiene, M.1
Strunskus, T.2
Hasse, G.3
Faupel, F.4
-
13
-
-
0036858454
-
Oxidation behavior of a Zr-Cu-Al-Ni amorphous alloy in air at 300-425 °C
-
W. Kai, H.H. Hsieh, T.G. Nieh, and Y. Kawamura: Oxidation behavior of a Zr-Cu-Al-Ni amorphous alloy in air at 300-425 °C. Intermetallics 10, 1265 (2002).
-
(2002)
Intermetallics
, vol.10
, pp. 1265
-
-
Kai, W.1
Hsieh, H.H.2
Nieh, T.G.3
Kawamura, Y.4
-
14
-
-
0027812730
-
The oxidation of amorphous Zr-base binary alloys in air
-
H.M. Kimura, K. Asami, A. Inoue, and T. Masumoto: The oxidation of amorphous Zr-base binary alloys in air. Corros. Sci. 35, 909 (1993).
-
(1993)
Corros. Sci.
, vol.35
, pp. 909
-
-
Kimura, H.M.1
Asami, K.2
Inoue, A.3
Masumoto, T.4
-
15
-
-
0030125870
-
Reaction induced surface segregation in amorphous CuZr, NiZr and PdZr alloys - An XPS and SIMS depth profiling study
-
M. Kilo, M. Hund, G. Sauer, A. Baiker, and A. Wokaun: Reaction induced surface segregation in amorphous CuZr, NiZr and PdZr alloys - An XPS and SIMS depth profiling study. J. Alloy Compds. 236, 137 (1996).
-
(1996)
J. Alloy Compds.
, vol.236
, pp. 137
-
-
Kilo, M.1
Hund, M.2
Sauer, G.3
Baiker, A.4
Wokaun, A.5
-
16
-
-
0037204452
-
Effect of ageing in air on morphology and surface-enhanced Raman scattering (SERS) activity of Cu-based amorphous alloys
-
A. Kudelski, M. Janik-Czachor, J. Bukowska, M. Pisarek, and A. Szummer: Effect of ageing in air on morphology and surface-enhanced Raman scattering (SERS) activity of Cu-based amorphous alloys. Mater. Sci. Eng. A 326, 364 (2002).
-
(2002)
Mater. Sci. Eng. A
, vol.326
, pp. 364
-
-
Kudelski, A.1
Janik-Czachor, M.2
Bukowska, J.3
Pisarek, M.4
Szummer, A.5
-
18
-
-
0343617262
-
iAl
-
edited by M.A. Otooni (NATO ASI Series 278, Dordrecht, The Netherlands, and Boston, MA)
-
iAl, in Science and Technology of Rapid Solidification and Processing, edited by M.A. Otooni (NATO ASI Series 278, Dordrecht, The Netherlands, and Boston, MA, 1995), p. 317.
-
(1995)
Science and Technology of Rapid Solidification and Processing
, pp. 317
-
-
Schneider, S.1
Sun, X.2
Nicolet, M.-A.3
Johnson, W.L.4
-
21
-
-
0003477976
-
-
2nd ed. (VCH, Weinheim, New York) pp. 483, 485, 1067, 1544, 1546
-
I. Barin: Thermochemical Data of Pure Substances, 2nd ed. (VCH, Weinheim, New York, 1993), pp. 483, 485, 1067, 1544, 1546, 1734.
-
(1993)
Thermochemical Data of Pure Substances
, pp. 1734
-
-
Barin, I.1
-
22
-
-
4644363478
-
22.5 bulk metallic glass under different oxidizing environments
-
22.5 bulk metallic glass under different oxidizing environments. Intermetallics 12, 1257 (2004).
-
(2004)
Intermetallics
, vol.12
, pp. 1257
-
-
Wong, C.H.1
Shek, C.H.2
-
23
-
-
0019913116
-
On the thermal oxidation kinetics of two metallic glasses
-
O. Hunderi and R. Bergersen: On the thermal oxidation kinetics of two metallic glasses. Corros. Sci. 22, 135 (1982).
-
(1982)
Corros. Sci.
, vol.22
, pp. 135
-
-
Hunderi, O.1
Bergersen, R.2
-
24
-
-
29144454367
-
-
(ASM International, Materials Park, OH)
-
S.A. Bradford: ASM Handbook, Vol. 13 (ASM International, Materials Park, OH, 1990), p. 64.
-
(1990)
ASM Handbook
, vol.13
, pp. 64
-
-
Bradford, S.A.1
-
27
-
-
29144437465
-
-
(ASM International, Materials Park, OH)
-
S.A. Bradford: ASM Handbook, Vol. 13 (ASM International, Materials Park, OH, 1990), p. 68.
-
(1990)
ASM Handbook
, vol.13
, pp. 68
-
-
Bradford, S.A.1
-
28
-
-
0001719735
-
Oxidation of copper and electronic transport in copper oxides
-
J-H. Park and K. Natesan: Oxidation of copper and electronic transport in copper oxides. Oxid. Met. 39, 411 (1993).
-
(1993)
Oxid. Met.
, vol.39
, pp. 411
-
-
Park, J.-H.1
Natesan, K.2
-
30
-
-
0034499153
-
Oxidation behavior of amorphous Ni-Zr and Ni-Zr-Sm alloys
-
M. Yamasaki, H. Nabazaki, K. Asami, and K. Hashimoto: Oxidation behavior of amorphous Ni-Zr and Ni-Zr-Sm alloys. J. Electrochem. Soc. 147, 4502 (2000).
-
(2000)
J. Electrochem. Soc.
, vol.147
, pp. 4502
-
-
Yamasaki, M.1
Nabazaki, H.2
Asami, K.3
Hashimoto, K.4
|