메뉴 건너뛰기




Volumn 88, Issue 9, 2005, Pages 2645-2648

Strength analysis of self-supported films produced by aqueous electrophoretic deposition

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINA; CRACKS; ELECTRODEPOSITION; ELECTROPHORESIS; FRACTURE TOUGHNESS; GELATION; GRAPHITE; SINTERING; STRENGTH OF MATERIALS; THIN FILMS; WEIBULL DISTRIBUTION; ZIRCONIA;

EID: 27644526150     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2005.00483.x     Document Type: Article
Times cited : (10)

References (19)
  • 1
    • 0035297396 scopus 로고    scopus 로고
    • 2/TZ3Y composites produced by electrophoretic deposition
    • 2/TZ3Y Composites Produced by Electrophoretic Deposition," J. Am. Ceram. Soc., 84 [3] 571-6 (2001).
    • (2001) J. Am. Ceram. Soc. , vol.84 , Issue.3 , pp. 571-576
    • Hatton, B.1    Nicholson, P.S.2
  • 5
    • 84986357084 scopus 로고
    • Zireonia/lumina functionally gradient composites by electrophoretic deposition techniques
    • P. Sarkar, X. Haung, and P. S. Nicholson, "Zireonia/lumina Functionally Gradient Composites by Electrophoretic Deposition Techniques," J. Am. Ceram. Soc., 76, 1055-56 (1993).
    • (1993) J. Am. Ceram. Soc. , vol.76 , pp. 1055-1056
    • Sarkar, P.1    Haung, X.2    Nicholson, P.S.3
  • 9
    • 0037412084 scopus 로고    scopus 로고
    • 3 functionally graded composites of tubular shape from nano-sols using double-step eleclrophoretic deposition
    • 3 Functionally Graded Composites of Tubular Shape from Nano-Sols Using Double-Step Eleclrophoretic Deposition," J. Eur. Ceram. Soc., 23, 1655-60 (2003).
    • (2003) J. Eur. Ceram. Soc. , vol.23 , pp. 1655-1660
    • Kaya, C.1
  • 11
    • 27744591107 scopus 로고    scopus 로고
    • Multilayer coatings with improved reliability produced by aqueous eleclrophorelic deposition
    • in press
    • B. Ferrari, S. Gonzalez, R. Moreno, and C. Baudin, "Multilayer Coatings with Improved Reliability Produced by Aqueous Eleclrophorelic Deposition." J. Eur. Ceram. Soc. (in press).
    • J. Eur. Ceram. Soc.
    • Ferrari, B.1    Gonzalez, S.2    Moreno, R.3    Baudin, C.4
  • 12
    • 27644593099 scopus 로고
    • Fracture mechanics principles
    • Edited by Applied Science Publishers Ltd., London, U.K.
    • A. de S Jayatilaka, "Fracture Mechanics Principles;" pp. 37-79 in Fracture of Engineering Brittle Materials, Edited by Applied Science Publishers Ltd., London, U.K., 1979.
    • (1979) Fracture of Engineering Brittle Materials , pp. 37-79
    • De Jayatilaka, A.S.1
  • 13
    • 0029172147 scopus 로고
    • Strength and young's modulus behaviour of a partially sintered porous alumina
    • S. C. Nanjangud, R. Brezny, and D. J. Green, "Strength and Young's Modulus Behaviour of a Partially Sintered Porous Alumina," J. Am. Ceram. Soc., 78 [1] 266-8 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.1 , pp. 266-268
    • Nanjangud, S.C.1    Brezny, R.2    Green, D.J.3
  • 14
    • 0142183442 scopus 로고    scopus 로고
    • Statistical analysis of the fracture behaviour of porous ceramic raschig rings
    • M. Villora, P. Callejas, M. F. Barba, and C. Baudin, "Statistical Analysis of the Fracture Behaviour of Porous Ceramic Raschig Rings," J. Eur. Ceram. Soc., 24, 589-94 (2004).
    • (2004) J. Eur. Ceram. Soc. , vol.24 , pp. 589-594
    • Villora, M.1    Callejas, P.2    Barba, M.F.3    Baudin, C.4
  • 15
    • 0032625042 scopus 로고    scopus 로고
    • Weibvill parameters and the tensile strength of porous phosphate glass-ceramics
    • F. Pernot, P. Elienne, F. Boschel, and L. Datas, "Weibvill Parameters and the Tensile Strength of Porous Phosphate Glass-Ceramics,"J. Am. Ceram. Soc., 82 [3] 641-815 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.3 , pp. 641-815
    • Pernot, F.1    Elienne, P.2    Boschel, F.3    Datas, L.4
  • 16
    • 0032045420 scopus 로고    scopus 로고
    • Evaluation of fracture strength of porous alumina sintered by Hot Isostatic Pressing (HI-Ping)
    • Y. Kinemuchi, N. Fusamune, A. Takata, and K. Ishizaki, "Evaluation of Fracture Strength of Porous Alumina Sintered by Hot Isostatic Pressing (HI-Ping)," J. Ceram. Soc. Jpn., 106 [4] 435-40 (1998).
    • (1998) J. Ceram. Soc. Jpn. , vol.106 , Issue.4 , pp. 435-440
    • Kinemuchi, Y.1    Fusamune, N.2    Takata, A.3    Ishizaki, K.4
  • 17
    • 0001386158 scopus 로고
    • On the estimation of the weibull modulus
    • B. Bergman, "On the Estimation of the Weibull Modulus," J. Mater. Sci. Lett., 3, 689-90 (1984).
    • (1984) J. Mater. Sci. Lett. , vol.3 , pp. 689-690
    • Bergman, B.1
  • 18
    • 84975849031 scopus 로고
    • Effect of flaw shape on strength of ceramics
    • G. K. Bansal, "Effect of Flaw Shape on Strength of Ceramics," J. Am. Ceram. Soc., 59 [1-2] 87-8 (1976).
    • (1976) J. Am. Ceram. Soc. , vol.59 , Issue.1-2 , pp. 87-88
    • Bansal, G.K.1
  • 19
    • 0000747232 scopus 로고
    • Effects of microstructure on the stress to propagate inherent flaws
    • A. G. Evans and G. Tappin, "Effects of Microstructure on the Stress to Propagate Inherent Flaws," Proc. Br. Ceram. Soc., 2 [6] 275-97 (1973).
    • (1973) Proc. Br. Ceram. Soc. , vol.2 , Issue.6 , pp. 275-297
    • Evans, A.G.1    Tappin, G.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.