메뉴 건너뛰기




Volumn 21, Issue 11, 2005, Pages 999-1007

Micro-tensile bond strength of adhesives bonded to class-I cavity-bottom dentin after thermo-cycling

Author keywords

Adhesion; Bond strength; Dental adhesive; Dentin; Enamel; Thermo cycling

Indexed keywords

AGING OF MATERIALS; CHEMICAL BONDS; DEGRADATION; HYDROLYSIS; WATER;

EID: 26444583686     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2004.11.005     Document Type: Article
Times cited : (104)

References (33)
  • 2
    • 0033071448 scopus 로고    scopus 로고
    • Thermal cycling procedures for laboratory testing of dental restorations
    • M.S. Gale, and B.W. Darvell Thermal cycling procedures for laboratory testing of dental restorations J Dent 27 1999 89 99
    • (1999) J Dent , vol.27 , pp. 89-99
    • Gale, M.S.1    Darvell, B.W.2
  • 3
    • 0034443787 scopus 로고    scopus 로고
    • In vivo degradation of resin-dentin bonds in humans over 1 to 3 years
    • M. Hashimoto, H. Ohno, M. Kaga, K. Endo, H. Sano, and H. Oguchi In vivo degradation of resin-dentin bonds in humans over 1 to 3 years J Dent Res 79 2000 1385 1391
    • (2000) J Dent Res , vol.79 , pp. 1385-1391
    • Hashimoto, M.1    Ohno, H.2    Kaga, M.3    Endo, K.4    Sano, H.5    Oguchi, H.6
  • 4
  • 5
    • 0032105211 scopus 로고    scopus 로고
    • Influence of thermal cycling on dentin bond strength of two-step bonding systems
    • M. Miyazaki, M. Sato, H. Onose, and B.K. Moore Influence of thermal cycling on dentin bond strength of two-step bonding systems Am J Dent 11 1998 118 122
    • (1998) Am J Dent , vol.11 , pp. 118-122
    • Miyazaki, M.1    Sato, M.2    Onose, H.3    Moore, B.K.4
  • 6
    • 0030307239 scopus 로고    scopus 로고
    • Does an incremental filling technique reduce polymerization shrinkage stresses?
    • A. Versluis, W.H. Douglas, M. Cross, and R.L. Sakaguchi Does an incremental filling technique reduce polymerization shrinkage stresses? J Dent Res 75 1996 871 878
    • (1996) J Dent Res , vol.75 , pp. 871-878
    • Versluis, A.1    Douglas, W.H.2    Cross, M.3    Sakaguchi, R.L.4
  • 7
    • 0023457345 scopus 로고
    • Setting stress in composite resin in relation to configuration of the restauration
    • A.J. Feilzer, A.J. De Gee, and C.L. Davidson Setting stress in composite resin in relation to configuration of the restauration J Dent Res 66 1987 1636 1639
    • (1987) J Dent Res , vol.66 , pp. 1636-1639
    • Feilzer, A.J.1    De Gee, A.J.2    Davidson, C.L.3
  • 8
    • 0034783857 scopus 로고    scopus 로고
    • Meta-analytical review of factors involved in dentin adherence
    • G. Leloup, W. D'Hoore, D. Bouter, M. Degrange, and J. Vreven Meta-analytical review of factors involved in dentin adherence J Dent Res 80 2001 1605 1614
    • (2001) J Dent Res , vol.80 , pp. 1605-1614
    • Leloup, G.1    D'Hoore, W.2    Bouter, D.3    Degrange, M.4    Vreven, J.5
  • 9
    • 0036584074 scopus 로고    scopus 로고
    • Evaluation of thermal cycling and mechanical loading on bond strength of a self-etching primer system to dentin
    • T. Nikaido, K.H. Kunzelman, H. Chen, M. Ogata, N. Harada, and S. Yamaguchi Evaluation of thermal cycling and mechanical loading on bond strength of a self-etching primer system to dentin Dent Mater 18 2002 269 275
    • (2002) Dent Mater , vol.18 , pp. 269-275
    • Nikaido, T.1    Kunzelman, K.H.2    Chen, H.3    Ogata, M.4    Harada, N.5    Yamaguchi, S.6
  • 10
    • 0018978172 scopus 로고
    • In vivo measurements of thermal diffusion through restorations of various materials
    • R.H. Harper, R.J. Schnell, M.L. Swartz, and R.W. Phillips In vivo measurements of thermal diffusion through restorations of various materials J Prosthet Dent 43 1980 180 185
    • (1980) J Prosthet Dent , vol.43 , pp. 180-185
    • Harper, R.H.1    Schnell, R.J.2    Swartz, M.L.3    Phillips, R.W.4
  • 11
    • 0023428156 scopus 로고
    • Thermal diffusivity of composite restorative materials
    • D.C. Watts, R. McAndrew, and C.H. Lloyd Thermal diffusivity of composite restorative materials J Dent Res 66 1987 1576 1578
    • (1987) J Dent Res , vol.66 , pp. 1576-1578
    • Watts, D.C.1    McAndrew, R.2    Lloyd, C.H.3
  • 16
    • 12344284766 scopus 로고    scopus 로고
    • Effect of cavity configuration and aging on the bonding effectiveness of six adhesives to dentin
    • Shirai K, De Munck J, Yoshida Y, Inoue S, Lambrechts P, Shintani H, et al. Effect of cavity configuration and aging on the bonding effectiveness of six adhesives to dentin. Dent Mater 2005; 21:110-24.
    • (2005) Dent Mater , vol.21 , pp. 110-124
    • Shirai, K.1    De Munck, J.2    Yoshida, Y.3    Inoue, S.4    Lambrechts, P.5    Shintani, H.6
  • 18
    • 0141906516 scopus 로고    scopus 로고
    • Effect of one-year water storage on the effectiveness of dentin adhesives in class v composite resin restorations
    • U. Blunck, and J.F. Roulet Effect of one-year water storage on the effectiveness of dentin adhesives in class V composite resin restorations J Dent Res 81 2002 [Special Issue B, abstr. #946]
    • (2002) J Dent Res , vol.81
    • Blunck, U.1    Roulet, J.F.2
  • 20
    • 0028505296 scopus 로고
    • New adhesives in class v restorations under combined load and simulated dentinal fluid
    • I. Krejci, T. Häusler, D. Sägesser, and F. Lutz New adhesives in class V restorations under combined load and simulated dentinal fluid Dent Mater 10 1994 331 335
    • (1994) Dent Mater , vol.10 , pp. 331-335
    • Krejci, I.1    Häusler, T.2    Sägesser, D.3    Lutz, F.4
  • 21
    • 0035343992 scopus 로고    scopus 로고
    • Mode of failure in the dentin-adhesive resin-resin composite bonded joint as determined by strength-based (μTBS) and fracture-based (CNSB) mechanical testing
    • S.R. Armstrong, J.C. Keller, and D.B. Boyer Mode of failure in the dentin-adhesive resin-resin composite bonded joint as determined by strength-based (μTBS) and fracture-based (CNSB) mechanical testing Dent Mater 17 2001 201 210
    • (2001) Dent Mater , vol.17 , pp. 201-210
    • Armstrong, S.R.1    Keller, J.C.2    Boyer, D.B.3
  • 22
    • 0035350653 scopus 로고    scopus 로고
    • The influence of water storage and C-factor on the dentin-resin composite microtensile bond strength and debond pathway utilizing a filled and unfilled adhesive resin
    • S.R. Armstrong, J.C. Keller, and D.B. Boyer The influence of water storage and C-factor on the dentin-resin composite microtensile bond strength and debond pathway utilizing a filled and unfilled adhesive resin Dent Mater 17 2001 268 276
    • (2001) Dent Mater , vol.17 , pp. 268-276
    • Armstrong, S.R.1    Keller, J.C.2    Boyer, D.B.3
  • 23
    • 0042809966 scopus 로고    scopus 로고
    • Microtensile bond strength of a total-etch 3-step, total-etch 2-step, self-etch 2-step, and a self-etch 1-step dentin bonding system through 15-month water storage
    • S.R. Armstrong, M.A. Vargas, Q. Fang, and J.E. Laffoon Microtensile bond strength of a total-etch 3-step, total-etch 2-step, self-etch 2-step, and a self-etch 1-step dentin bonding system through 15-month water storage J Adhes Dent 5 2003 47 56
    • (2003) J Adhes Dent , vol.5 , pp. 47-56
    • Armstrong, S.R.1    Vargas, M.A.2    Fang, Q.3    Laffoon, J.E.4
  • 24
    • 4143149600 scopus 로고    scopus 로고
    • A Randomized controlled trial evaluating the three-year clinical effectiveness of two etch & rinse adhesives in cervical lesions
    • Van Meerbeek B, Kanumilli P, De Munck J, Van Landuyt K, Lambrechts P, Peumans M. A Randomized controlled trial evaluating the three-year clinical effectiveness of two etch & rinse adhesives in cervical lesions. Oper Dent 2004; 29:376-85.
    • (2004) Oper Dent , vol.29 , pp. 376-385
    • Van Meerbeek, B.1    Kanumilli, P.2    De Munck, J.3    Van Landuyt, K.4    Lambrechts, P.5    Peumans, M.6
  • 25
    • 0030203768 scopus 로고    scopus 로고
    • Clinical evaluation of a filled adhesive system in Class 5 restorations
    • A. Boghosian Clinical evaluation of a filled adhesive system in Class 5 restorations Compend Contin Educ Dent 17 1996 750 754
    • (1996) Compend Contin Educ Dent , vol.17 , pp. 750-754
    • Boghosian, A.1
  • 27
    • 0036617559 scopus 로고    scopus 로고
    • In vivo long-term durability of the bond to dentin using two adhesive systems
    • A. Takahashi, S. Inoue, C. Kawamoto, R. Ominato, T. Tanaka, and Y. Sato In vivo long-term durability of the bond to dentin using two adhesive systems J Adhes Dent 4 2002 151 159
    • (2002) J Adhes Dent , vol.4 , pp. 151-159
    • Takahashi, A.1    Inoue, S.2    Kawamoto, C.3    Ominato, R.4    Tanaka, T.5    Sato, Y.6
  • 28
    • 0141962407 scopus 로고    scopus 로고
    • Buonocore memorial lecture: Adhesion to enamel and dentin: Current status and future challenges
    • B. Van Meerbeek, J. De Munck, Y. Yoshida, S. Inoue, M. Vargas, and P. Vijay Buonocore memorial lecture: adhesion to enamel and dentin: current status and future challenges Oper Dent 28 2003 215 235
    • (2003) Oper Dent , vol.28 , pp. 215-235
    • Van Meerbeek, B.1    De Munck, J.2    Yoshida, Y.3    Inoue, S.4    Vargas, M.5    Vijay, P.6
  • 29
    • 0141682576 scopus 로고    scopus 로고
    • Clinical evaluation of a self-etching and a one-bottle adhesive system at two years
    • S.L. Türkün Clinical evaluation of a self-etching and a one-bottle adhesive system at two years J Dent 31 2003 527 534
    • (2003) J Dent , vol.31 , pp. 527-534
    • Türkün, S.L.1
  • 31
    • 0037640986 scopus 로고    scopus 로고
    • How can nanoleakage occur in self-etching adhesive systems that demineralize and infiltrate simultaneously?
    • F.R. Tay, N.M. King, K.M. Chan, and D.H. Pashley How can nanoleakage occur in self-etching adhesive systems that demineralize and infiltrate simultaneously? J Adhes Dent 4 2002 255 269
    • (2002) J Adhes Dent , vol.4 , pp. 255-269
    • Tay, F.R.1    King, N.M.2    Chan, K.M.3    Pashley, D.H.4
  • 32


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.