Volumn 94, Issue 4, 2005, Pages 350-356

Effect of surface treatment on bond strength of low-fusing porcelain to commercially pure titanium

Author keywords

[No Author keywords available]

Indexed keywords

BIOMEDICAL AND DENTAL MATERIALS; HYDROCHLORIC ACID; TITANIUM;

EID: 25844527238     PISSN: 00223913     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.prosdent.2005.07.007     Document Type: Article
Times cited : (80)

References (35)
  • 2
    • 0030203769 scopus 로고    scopus 로고
    • Dental ceramic restorative systems
    • R.A. Giordano Dental ceramic restorative systems Compend Contin Educ Dent 17 1996 779 786
    • (1996) Compend Contin Educ Dent , vol.17 , pp. 779-786
    • Giordano, R.A.1
  • 3
    • 0023395756 scopus 로고
    • Effect of incompatibility stress on the fit of metal-ceramic crowns
    • K.J. Anusavice, and J.E. Carroll Effect of incompatibility stress on the fit of metal-ceramic crowns J Dent Res 66 1987 1341 1345
    • (1987) J Dent Res , vol.66 , pp. 1341-1345
    • Anusavice, K.J.1    Carroll, J.E.2
  • 4
    • 0018038715 scopus 로고
    • Allergy to a partial denture casting: Case report
    • A.H. Fenton, and J.D. Jeffrey Allergy to a partial denture casting: case report Dent J 44 1978 466 468
    • (1978) Dent J , vol.44 , pp. 466-468
    • Fenton, A.H.1    Jeffrey, J.D.2
  • 6
    • 0023375433 scopus 로고
    • Veterans Administration Cooperative Studies Project No. 147. Part IV: Biocompatibility of base metal alloys
    • H.F. Morris Veterans Administration Cooperative Studies Project No. 147. Part IV: biocompatibility of base metal alloys J Prosthet Dent 58 1987 1 5
    • (1987) J Prosthet Dent , vol.58 , pp. 1-5
    • Morris, H.F.1
  • 7
    • 0036077987 scopus 로고    scopus 로고
    • Biocompatibility of dental casting alloys
    • W. Geurtsen Biocompatibility of dental casting alloys Crit Rev Oral Biol Med 13 2002 71 84
    • (2002) Crit Rev Oral Biol Med , vol.13 , pp. 71-84
    • Geurtsen, W.1
  • 8
    • 0034134024 scopus 로고    scopus 로고
    • Biocompatibility of dental casting alloys: A review
    • J.C. Wataha Biocompatibility of dental casting alloys: a review J Prosthet Dent 83 2000 223 234
    • (2000) J Prosthet Dent , vol.83 , pp. 223-234
    • Wataha, J.C.1
  • 9
    • 0020771092 scopus 로고
    • Biocompatibility of titanium implants: Surface science aspects
    • B. Kasemo Biocompatibility of titanium implants: surface science aspects J Prosthet Dent 49 1983 832 837
    • (1983) J Prosthet Dent , vol.49 , pp. 832-837
    • Kasemo, B.1
  • 10
    • 0027616999 scopus 로고
    • Titanium and titanium alloys as dental materials
    • E.P. Lautenschlager, and P. Monaghan Titanium and titanium alloys as dental materials Int Dent J 43 1993 245 253
    • (1993) Int Dent J , vol.43 , pp. 245-253
    • Lautenschlager, E.P.1    Monaghan, P.2
  • 11
    • 0028450707 scopus 로고
    • Study of corrosion between a titanium implant and dental alloys
    • L. Reclaru, and J.M. Meyer Study of corrosion between a titanium implant and dental alloys J Dent 22 1994 159 168
    • (1994) J Dent , vol.22 , pp. 159-168
    • Reclaru, L.1    Meyer, J.M.2
  • 12
    • 0030155746 scopus 로고    scopus 로고
    • Titanium for prosthodontic applications: A review of the literature
    • R.R. Wang, and A. Fenton Titanium for prosthodontic applications: a review of the literature Quintessence Int 27 1996 401 408
    • (1996) Quintessence Int , vol.27 , pp. 401-408
    • Wang, R.R.1    Fenton, A.2
  • 13
    • 0026860865 scopus 로고
    • Non-cast titanium restorations in fixed prosthodontics
    • K.W. Boening, M.H. Walter, and P.D. Reppel Non-cast titanium restorations in fixed prosthodontics J Oral Rehabil 19 1992 281 287
    • (1992) J Oral Rehabil , vol.19 , pp. 281-287
    • Boening, K.W.1    Walter, M.H.2    Reppel, P.D.3
  • 14
    • 0031134391 scopus 로고    scopus 로고
    • Titanium for removable dentures. I. Laboratory procedures
    • T. Mori, T. Togaya, M. Jean-Louis, and M. Yabugami Titanium for removable dentures. I. Laboratory procedures J Oral Rehabil 24 1997 338 341
    • (1997) J Oral Rehabil , vol.24 , pp. 338-341
    • Mori, T.1    Togaya, T.2    Jean-Louis, M.3    Yabugami, M.4
  • 15
    • 0038488528 scopus 로고    scopus 로고
    • Comparisons of precision of fit between cast and CNC-milled titanium implant frameworks for the edentulous mandible
    • A. Ortorp, T. Jemt, T. Back, and T. Jalevic Comparisons of precision of fit between cast and CNC-milled titanium implant frameworks for the edentulous mandible Int J Prosthodont 16 2003 194 200
    • (2003) Int J Prosthodont , vol.16 , pp. 194-200
    • Ortorp, A.1    Jemt, T.2    Back, T.3    Jalevic, T.4
  • 16
    • 0025444240 scopus 로고
    • Oxidation effects on porcelain-titanium interface reactions and bond strength
    • H. Kimura, C.J. Horng, M. Okazaki, and J. Takahashi Oxidation effects on porcelain-titanium interface reactions and bond strength Dent Mater J 9 1990 91 99
    • (1990) Dent Mater J , vol.9 , pp. 91-99
    • Kimura, H.1    Horng, C.J.2    Okazaki, M.3    Takahashi, J.4
  • 17
    • 0025439635 scopus 로고
    • Oxide adherence and porcelain bonding to titanium and Ti-6Al-4V alloy
    • M. Adachi, J.R. Mackert Jr., E.E. Parry, and C.W. Fairhurst Oxide adherence and porcelain bonding to titanium and Ti-6Al-4V alloy J Dent Res 69 1990 1230 1235
    • (1990) J Dent Res , vol.69 , pp. 1230-1235
    • Adachi, M.1    Mackert Jr., J.R.2    Parry, E.E.3    Fairhurst, C.W.4
  • 18
    • 0017749852 scopus 로고
    • The chemical nature of dental porcelain
    • A.M. Lacy The chemical nature of dental porcelain Dent Clin North Am 21 1977 661 667
    • (1977) Dent Clin North Am , vol.21 , pp. 661-667
    • Lacy, A.M.1
  • 19
    • 0035294446 scopus 로고    scopus 로고
    • Thermal expansion coefficient of titanium casting
    • D. Low, T. Sumii, and M. Swain Thermal expansion coefficient of titanium casting J Oral Rehabil 28 2001 239 242
    • (2001) J Oral Rehabil , vol.28 , pp. 239-242
    • Low, D.1    Sumii, T.2    Swain, M.3
  • 20
    • 0029181886 scopus 로고
    • Bonding characteristics of low-fusing porcelain bonded to pure titanium and palladium-copper alloy
    • I.C. Pang, J.L. Gilbert, J. Chai, and E.P. Lautenschlager Bonding characteristics of low-fusing porcelain bonded to pure titanium and palladium-copper alloy J Prosthet Dent 73 1995 17 25
    • (1995) J Prosthet Dent , vol.73 , pp. 17-25
    • Pang, I.C.1    Gilbert, J.L.2    Chai, J.3    Lautenschlager, E.P.4
  • 21
    • 0033087402 scopus 로고    scopus 로고
    • Comparison of the bond compatibility of titanium and an NiCr alloy to dental porcelain
    • H. Yilmaz, and C. Dincer Comparison of the bond compatibility of titanium and an NiCr alloy to dental porcelain J Dent 27 1999 215 222
    • (1999) J Dent , vol.27 , pp. 215-222
    • Yilmaz, H.1    Dincer, C.2
  • 22
    • 0034328117 scopus 로고    scopus 로고
    • Bond strength of three porcelains to two forms of titanium using two firing atmospheres
    • S. Atsu, and S. Berksun Bond strength of three porcelains to two forms of titanium using two firing atmospheres J Prosthet Dent 84 2000 567 574
    • (2000) J Prosthet Dent , vol.84 , pp. 567-574
    • Atsu, S.1    Berksun, S.2
  • 23
    • 84989535713 scopus 로고
    • Bond strength of porcelain on cast vs. wrought titanium
    • T. Derand, and H. Hero Bond strength of porcelain on cast vs. wrought titanium Scand J Dent Res 100 1992 184 188
    • (1992) Scand J Dent Res , vol.100 , pp. 184-188
    • Derand, T.1    Hero, H.2
  • 24
    • 0028402743 scopus 로고
    • Bond characteristics of porcelain fused to milled titanium
    • J.L. Gilbert, D.A. Covey, and E.P. Lautenschlager Bond characteristics of porcelain fused to milled titanium Dent Mater 10 1994 134 140
    • (1994) Dent Mater , vol.10 , pp. 134-140
    • Gilbert, J.L.1    Covey, D.A.2    Lautenschlager, E.P.3
  • 25
    • 0030160162 scopus 로고    scopus 로고
    • Three-point bending strength of ceramics fused to cast titanium
    • L. Probster, U. Maiwald, and H. Weber Three-point bending strength of ceramics fused to cast titanium Eur J Oral Sci 104 1996 313 319
    • (1996) Eur J Oral Sci , vol.104 , pp. 313-319
    • Probster, L.1    Maiwald, U.2    Weber, H.3
  • 26
    • 17344374992 scopus 로고    scopus 로고
    • The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminum-vanadium alloy
    • M.G. Troia Jr., G.E. Henriques, M.A. Nobilo, and M.F. Mesquita The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminum-vanadium alloy Dent Mater 19 2003 790 796
    • (2003) Dent Mater , vol.19 , pp. 790-796
    • Troia Jr., M.G.1    Henriques, G.E.2    Nobilo, M.A.3    Mesquita, M.F.4
  • 27
    • 0035049885 scopus 로고    scopus 로고
    • Titanium-porcelain system. Part III: Effects of surface modification on bond strengths
    • M.J. Reyes, Y. Oshida, C.J. Andres, T. Barco, S. Hovijitra, and D. Brown Titanium-porcelain system. Part III: effects of surface modification on bond strengths Biomed Mater Eng 11 2001 117 136
    • (2001) Biomed Mater Eng , vol.11 , pp. 117-136
    • Reyes, M.J.1    Oshida, Y.2    Andres, C.J.3    Barco, T.4    Hovijitra, S.5    Brown, D.6
  • 30
    • 4243558954 scopus 로고    scopus 로고
    • International Organization for Standardization. ISO 9693: metal-ceramic dental restorative systems; 1999. Available at: http://www.iso.ch/iso/en/prods- services/ISOstore/store.html. Accessed August 28, 2005.
    • (1999) ISO 9693: Metal-ceramic Dental Restorative Systems
  • 31
    • 0031116287 scopus 로고    scopus 로고
    • Oxidation behavior of surface-modified titanium for titanium-ceramic restorations
    • R.R. Wang, and K.K. Fung Oxidation behavior of surface-modified titanium for titanium-ceramic restorations J Prosthet Dent 77 1997 423 434
    • (1997) J Prosthet Dent , vol.77 , pp. 423-434
    • Wang, R.R.1    Fung, K.K.2
  • 32
    • 0022666283 scopus 로고
    • Effect of metal surface treatment on ceramic bond strength
    • D.G. Jochen, A.A. Caputo, and J. Matyas Effect of metal surface treatment on ceramic bond strength J Prosthet Dent 55 1986 186 188
    • (1986) J Prosthet Dent , vol.55 , pp. 186-188
    • Jochen, D.G.1    Caputo, A.A.2    Matyas, J.3
  • 33
    • 0025443459 scopus 로고
    • A quantitative study for the bond and color of ceramometals. Part I
    • I.A. Hammad, and R.S. Stein A quantitative study for the bond and color of ceramometals. Part I J Prosthet Dent 63 1990 643 653
    • (1990) J Prosthet Dent , vol.63 , pp. 643-653
    • Hammad, I.A.1    Stein, R.S.2
  • 34
    • 0034277695 scopus 로고    scopus 로고
    • Influence of metal surface finishing on porcelain porosity and beam failure loads at the metal-ceramic interface
    • T.M. Hofstede, C. Ercoli, G.N. Graser, R.H. Tallents, M.E. Moss, and D.T. Zero Influence of metal surface finishing on porcelain porosity and beam failure loads at the metal-ceramic interface J Prosthet Dent 84 2000 309 317
    • (2000) J Prosthet Dent , vol.84 , pp. 309-317
    • Hofstede, T.M.1    Ercoli, C.2    Graser, G.N.3    Tallents, R.H.4    Moss, M.E.5    Zero, D.T.6
  • 35
    • 0014563748 scopus 로고
    • Tensile strength determination of the interface between porcelain fused to gold
    • M. Kelly, K. Asgar, and W.J. O'Brien Tensile strength determination of the interface between porcelain fused to gold J Biomed Mater Res 3 1969 403 408
    • (1969) J Biomed Mater Res , vol.3 , pp. 403-408
    • Kelly, M.1    Asgar, K.2    O'Brien, W.J.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.