Volumn 21, Issue 1, 2004, Pages 41-46

Creep strength and ductility of 9 to 12% chromium steels

(1)  Hald, J a  


Author keywords

9 12 chromium steels; Creep strength; Ductility

Indexed keywords

CHROMIUM PLATING; CREEP TESTING; DUCTILITY; LIGNITE; MATHEMATICAL MODELS; PRESSURE VESSELS; ROTORS; STEAM PIPING SYSTEMS; STRENGTH OF MATERIALS; TUNGSTEN ALLOYS; TURBINES;

EID: 2542523758     PISSN: 09603409     EISSN: None     Source Type: Journal    
DOI: 10.1179/mht.2004.006     Document Type: Conference Paper
Times cited : (57)