Volumn 22, Issue 1-2, 2005, Pages 105-112

Mechanisms of chromia scale failure during the course of 15-18Cr ferritic stainless steel oxidation in water vapour

Author keywords

Chromia scale; Ferritic stainless steel

Indexed keywords

ACIDITY; FERRITES; IRON OXIDES; OXIDATION; RAMAN SPECTROSCOPY;

EID: 24944554792     PISSN: 09603409     EISSN: None     Source Type: Journal    
DOI: 10.1179/mht.2005.012     Document Type: Conference Paper
Times cited : (77)

References (20)
  • 1
    • 24944502899 scopus 로고    scopus 로고
    • Study and imaging by photoelectrochemical techniques of films thermally grown on titanium
    • Newcomb, S.B. and Bennett, M.J. (eds). Institute of Materials, London
    • Wouters, Y., Galerie, A. Antoni, L. and Petit, J.P. Study and imaging by photoelectrochemical techniques of films thermally grown on titanium. In: Newcomb, S.B. and Bennett, M.J. (eds), Microscopy of Oxidation 3, pp.420-426. Institute of Materials, London (1997).
    • (1997) Microscopy of Oxidation , vol.3 , pp. 420-426
    • Wouters, Y.1    Galerie, A.2    Antoni, L.3    Petit, J.P.4
  • 2
    • 0033717401 scopus 로고    scopus 로고
    • Characterization of chromia scales grown on pure chromium in different oxidizing atmospheres
    • Henry, S., Mougin, J., Wouters, Y., Petit, J.P. and Galerie, A. Characterization of chromia scales grown on pure chromium in different oxidizing atmospheres. Mater. High Temp., 17(2), 231-235 (2000).
    • (2000) Mater. High Temp. , vol.17 , Issue.2 , pp. 231-235
    • Henry, S.1    Mougin, J.2    Wouters, Y.3    Petit, J.P.4    Galerie, A.5
  • 4
    • 8644278746 scopus 로고    scopus 로고
    • Study of the thermal oxidation of Fe-15Cr by combined Raman and photoelectrochemical imaging
    • Petit, J.P., Mermoux, M., Wouters, Y., Galerie, A. and Chemarin, C. Study of the thermal oxidation of Fe-15Cr by combined Raman and photoelectrochemical imaging. Mater. Sci. Forum, 461-464, 681-688 (2004).
    • (2004) Mater. Sci. Forum , vol.461-464 , pp. 681-688
    • Petit, J.P.1    Mermoux, M.2    Wouters, Y.3    Galerie, A.4    Chemarin, C.5
  • 5
    • 0035184376 scopus 로고    scopus 로고
    • Abnormal oxidation of stabilized ferritic stainless steels in water vapour
    • Henry, S., Galerie, A. and Antoni, L. Abnormal oxidation of stabilized ferritic stainless steels in water vapour. Mater. Sci. Forum, 369-372, 353-360 (2001).
    • (2001) Mater. Sci. Forum , vol.369-372 , pp. 353-360
    • Henry, S.1    Galerie, A.2    Antoni, L.3
  • 7
    • 0025890913 scopus 로고
    • Raman studies of corrosion films grown on Fe and Fe-6Mo in pitting conditions
    • Boucherit, N., Hugot-le-Goff, A. and Joiret, S. Raman studies of corrosion films grown on Fe and Fe-6Mo in pitting conditions. Corros. Sci., 32, 497-507 (1991).
    • (1991) Corros. Sci. , vol.32 , pp. 497-507
    • Boucherit, N.1    Hugot-Le-Goff, A.2    Joiret, S.3
  • 9
    • 24944508406 scopus 로고
    • The high-temperature oxidation of Fe-Cr alloys in the composition range of 25-95% Cr
    • Tedmon,C. S. The high-temperature oxidation of Fe-Cr alloys in the composition range of 25-95% Cr. J. Electrochem. Soc., 113, 766 (1966).
    • (1966) J. Electrochem. Soc. , vol.113 , pp. 766
    • Tedmon, C.S.1
  • 11
    • 0036529370 scopus 로고    scopus 로고
    • The high temperature oxidation of 11% chromium steel - Part I: Influence of pH2O
    • Segerdahl, K., Svensson, J.-E. and Johansson, L.-G. The high temperature oxidation of 11% chromium steel - Part I: influence of pH2O, Mater. Corros., 53, 247-255 (2002).
    • (2002) Mater. Corros. , vol.53 , pp. 247-255
    • Segerdahl, K.1    Svensson, J.-E.2    Johansson, L.-G.3
  • 12
    • 0036652366 scopus 로고    scopus 로고
    • The high temperature oxidation of 11%%chromium steel - Part II : Influence of flow rate
    • Segerdahl, K., Svensson, J.-E. and Johansson, L.-G. The high temperature oxidation of 11%%chromium steel - Part II : influence of flow rate, Mater. Corros., 53, 479-485 (2002).
    • (2002) Mater. Corros. , vol.53 , pp. 479-485
    • Segerdahl, K.1    Svensson, J.-E.2    Johansson, L.-G.3
  • 13
    • 0032655518 scopus 로고    scopus 로고
    • Mechanism of breakaway oxidation and application to a chromia forming steel
    • Evans, H. E., Donaldson, A. T. and Gilmour, T. C. Mechanism of breakaway oxidation and application to a chromia forming steel. Oxidat. Met., 52, 379-402 (1999).
    • (1999) Oxidat. Met. , vol.52 , pp. 379-402
    • Evans, H.E.1    Donaldson, A.T.2    Gilmour, T.C.3
  • 14
    • 0032625652 scopus 로고    scopus 로고
    • Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873K in the presence of 10% water vapour
    • Asteman, H., Svensson, J.-E., Johansson, L.-G. and Norell, M. Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873K in the presence of 10% water vapour. Oxidat. Met., 52, 95-111 (1999).
    • (1999) Oxidat. Met. , vol.52 , pp. 95-111
    • Asteman, H.1    Svensson, J.-E.2    Johansson, L.-G.3    Norell, M.4
  • 15
    • 0027587908 scopus 로고
    • Thermodynamics of gas phase chromium species: The chromium oxides, the chromium oxohydroxides, and volatility calculations in waste incineration process
    • Ebbinghaus B.B. Thermodynamics of gas phase chromium species: the chromium oxides, the chromium oxohydroxides, and volatility calculations in waste incineration process. Combustion and Flame, 93, 119-137 (1993).
    • (1993) Combustion and Flame , vol.93 , pp. 119-137
    • Ebbinghaus, B.B.1
  • 16
    • 0029212260 scopus 로고
    • Stress effects in high temperature oxidation of metals
    • Evans, H.E. Stress effects in high temperature oxidation of metals. Int. Mater. Rev., 40, 1-40 (1995).
    • (1995) Int. Mater. Rev. , vol.40 , pp. 1-40
    • Evans, H.E.1
  • 17
    • 0035283762 scopus 로고    scopus 로고
    • 3 obtained by high temperature oxidation by X-ray diffraction and Raman spectroscopy
    • 3 obtained by high temperature oxidation by X-ray diffraction and Raman spectroscopy. J. Phys. Chem. Solids, 62, 553-563 (2001).
    • (2001) J. Phys. Chem. Solids , vol.62 , pp. 553-563
    • Mougin, J.1    Le Bihan, T.2    Lucazeau, G.3
  • 18
    • 0026617049 scopus 로고
    • Ex-situ and in-situ determination of stress distribution in chromium oxide films by Raman spectroscopy
    • Birnie, J., Craggs, C., Gardiner, D.J. and Graves, P.R. Ex-situ and in-situ determination of stress distribution in chromium oxide films by Raman spectroscopy. Corros. Sci. 33, 1-12 (1992).
    • (1992) Corros. Sci. , vol.33 , pp. 1-12
    • Birnie, J.1    Craggs, C.2    Gardiner, D.J.3    Graves, P.R.4
  • 19
    • 0034809408 scopus 로고    scopus 로고
    • In-situ Raman monitoring of chromium oxide scale growth
    • Mougin, J., Rosman, N., Lucazeau, G. and Galerie, A. In-situ Raman monitoring of chromium oxide scale growth. J. Raman Spectrosc., 32, 739-744 (2001).
    • (2001) J. Raman Spectrosc. , vol.32 , pp. 739-744
    • Mougin, J.1    Rosman, N.2    Lucazeau, G.3    Galerie, A.4
  • 20
    • 0035190167 scopus 로고    scopus 로고
    • The kinetic behaviour of metals in water vapour at high temperatures : Can general rules be proposed ?
    • Galerie, A., Wouters, Y. and Caillet, M. The kinetic behaviour of metals in water vapour at high temperatures : can general rules be proposed ?, Mater. Sci. For., 369-372, 231-238 (2001).
    • (2001) Mater. Sci. For. , vol.369-372 , pp. 231-238
    • Galerie, A.1    Wouters, Y.2    Caillet, M.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.