메뉴 건너뛰기




Volumn 373, Issue 1-2, 2004, Pages 195-203

Effect of laser surface melting on the corrosion and cavitation erosion behaviors of a manganese-nickel-aluminium bronze

Author keywords

Cavitation erosion; Corrosion; Cu Mn Al Ni Fe; Laser surface melting; Manganese nickel aluminium bronze; Synergism

Indexed keywords

ALUMINUM COMPOUNDS; EROSION; LASERS; MAGNESIUM COMPOUNDS; MELTING; NICKEL COMPOUNDS;

EID: 2442561275     PISSN: 09215093     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.msea.2004.01.016     Document Type: Article
Times cited : (122)

References (28)