Hydrogen-assisted materials processing

Author keywords

[No Author keywords available]

Indexed keywords

ALLOYING; AMORPHIZATION; ANNEALING; DECOMPOSITION; HYDROGEN; HYDROGENATION; MICROSTRUCTURE;

EID: 23844496253     PISSN: None     EISSN: None     Source Type: Conference Proceeding    
DOI: None     Document Type: Conference Paper
Times cited : (3)

References (75)
  • 9
    • 0040164340 scopus 로고
    • eds. F.H. Froes and I.L. Caplan (Warrendale, PA: TMS)
    • B.A. Kolachev et al., in Titanium'92: Science and Technology, vol. 1, eds. F.H. Froes and I.L. Caplan (Warrendale, PA: TMS, 1993), 861.
    • (1993) Titanium'92: Science and Technology , vol.1 , pp. 861
    • Kolachev, B.A.1
  • 12
    • 0019107034 scopus 로고
    • eds. H. Kimura and O. Izumi (Warrendale, PA: TMS)
    • W.R. Kerr et al., in Titanium'80: Science and Technology, vol. 4, eds. H. Kimura and O. Izumi (Warrendale, PA: TMS, 1980), 2477.
    • (1980) Titanium'80: Science and Technology , vol.4 , pp. 2477
    • Kerr, W.R.1
  • 13
    • 0039572996 scopus 로고
    • Moscow, Russia: Aviation Publishing House
    • B.A. Kolachev and V.D. Talalaev, Titan (Titanium), vol. 1 (Moscow, Russia: Aviation Publishing House, 1993), 43.
    • (1993) Titan (Titanium) , vol.1 , pp. 43
    • Kolachev, B.A.1    Talalaev, V.D.2
  • 14
  • 16
  • 22
    • 0025475637 scopus 로고
    • J. Wittenauer, JOM, 42 (8) ( 1990), 7.
    • (1990) JOM , vol.42 , Issue.8 , pp. 7
    • Wittenauer, J.1
  • 25
    • 0023670543 scopus 로고
    • eds. R.A. Oriani, J.P. Hirth, and M. Smialowski (Park Ridge, NJ: Noyes Publ.)
    • E. Lunarska, in Hydrogen Degradation of Ferrous Alloys, eds. R.A. Oriani, J.P. Hirth, and M. Smialowski (Park Ridge, NJ: Noyes Publ., 1985), 321.
    • (1985) Hydrogen Degradation of Ferrous Alloys , pp. 321
    • Lunarska, E.1
  • 26
    • 0023670091 scopus 로고
    • eds. R.A. Oriani, J.P. Hirth, and M. Smialowski (Park Ridge, NJ: Noyes Publ.)
    • R.A. Oriani, in Hydrogen Degradation of Ferrous Alloys, eds. R.A. Oriani, J.P. Hirth, and M. Smialowski (Park Ridge, NJ: Noyes Publ., 1985), 353.
    • (1985) Hydrogen Degradation of Ferrous Alloys , pp. 353
    • Oriani, R.A.1
  • 32
    • 0040540478 scopus 로고
    • A.A. Popov et al., Metals, 5 ( 1994), 109.
    • (1994) Metals , vol.5 , pp. 109
    • Popov, A.A.1
  • 48
  • 52
  • 65
    • 33645254331 scopus 로고    scopus 로고
    • Ph.D. thesis (Logos-Verlag: Berlin)
    • D. Zander, Ph.D. thesis (Logos-Verlag: Berlin, 2001).
    • (2001)
    • Zander, D.1
  • 71
    • 33645263632 scopus 로고
    • British Patent 1,554,384, October
    • I.R. Harris, J. Evans, and P. Nyholm, British Patent 1,554,384, October 1979.
    • (1979)
    • Harris, I.R.1    Evans, J.2    Nyholm, P.3
  • 72


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.