Boron carbide films grown from microwave plasma chemical vapour deposition
-
K.W. Lee, and S.J. Harris Boron carbide films grown from microwave plasma chemical vapour deposition Diamond Relat. Mater. 7 1998 1539 1543
-
(1998)
Diamond Relat. Mater.
, vol.7
, pp. 1539-1543
-
-
Lee, K.W.1
Harris, S.J.2
-
3
-
-
0032053294
-
A numerical investigation of solid particle erosion within oilfield control valves
-
A. Forder, M. Thew, and D. Harrison A numerical investigation of solid particle erosion within oilfield control valves Wear 216 1998 184 193
-
(1998)
Wear
, vol.216
, pp. 184-193
-
-
Forder, A.1
Thew, M.2
Harrison, D.3
-
4
-
-
0029328969
-
Sand erosion of wear-resistant materials: Erosion in choke valves
-
K. Haugen, O. Kvernvold, A. Ronald, and R. Sandberg Sand erosion of wear-resistant materials: erosion in choke valves Wear 186-187 1995 179 188
-
(1995)
Wear
, vol.186-187
, pp. 179-188
-
-
Haugen, K.1
Kvernvold, O.2
Ronald, A.3
Sandberg, R.4
-
5
-
-
0035270001
-
Nanoindentation of CVD diamond: Comparison of an FE model with analytical and experimental data
-
L. De Fazio, S. Syngellakis, R.J.K. Wood, F.M. Fugiuele, and G. Sciumé Nanoindentation of CVD diamond: comparison of an FE model with analytical and experimental data Diamond Relat. Mater. 10 2001 765 769
-
(2001)
Diamond Relat. Mater.
, vol.10
, pp. 765-769
-
-
De Fazio, L.1
Syngellakis, S.2
Wood, R.J.K.3
Fugiuele, F.M.4
Sciumé, G.5
-
7
-
-
0018305252
-
Strength degradation of glass impacted with sharp particles
-
S.M. Wiederhorn, and B.R. Lawn Strength degradation of glass impacted with sharp particles J. Am. Ceram. Soc. 62 1979 66 70
-
(1979)
J. Am. Ceram. Soc.
, vol.62
, pp. 66-70
-
-
Wiederhorn, S.M.1
Lawn, B.R.2
-
8
-
-
0030213928
-
Solid particle erosion mechanism in glass
-
Y. Ballout, J.A. Mathis, and J.E. Talia Solid particle erosion mechanism in glass Wear 196 1996 263 269
-
(1996)
Wear
, vol.196
, pp. 263-269
-
-
Ballout, Y.1
Mathis, J.A.2
Talia, J.E.3
-
9
-
-
0033367033
-
Indentation fracture of glass and mechanisms of material removal
-
D.A. Gorham, and A.D. Salman Indentation fracture of glass and mechanisms of material removal Wear 233-235 1999 151 156
-
(1999)
Wear
, vol.233-235
, pp. 151-156
-
-
Gorham, D.A.1
Salman, A.D.2
-
10
-
-
0026617225
-
Ductile-brittle transitions and wear maps for erosion and abrasion of brittle materials
-
I.M. Hutchings Ductile-brittle transitions and wear maps for erosion and abrasion of brittle materials J. Phys. D 25 1992 A212 A221
-
(1992)
J. Phys. D
, vol.25
-
-
Hutchings, I.M.1
-
11
-
-
0000433955
-
Transitions, threshold effect and erosion maps
-
I.M. Hutchings Transitions, threshold effect and erosion maps Key Eng. Mater. 71 1992 75 92
-
(1992)
Key Eng. Mater.
, vol.71
, pp. 75-92
-
-
Hutchings, I.M.1
-
12
-
-
0019937282
-
The response of solids to elastic/plastic indentation I: Stresses and residual stresses
-
S.S. Chiang, D.B. Marshall, and A.G. Evans The response of solids to elastic/plastic indentation I: stresses and residual stresses J. Appl. Phys. 53 1 1982 298 311
-
(1982)
J. Appl. Phys.
, vol.53
, Issue.1
, pp. 298-311
-
-
Chiang, S.S.1
Marshall, D.B.2
Evans, A.G.3
-
13
-
-
0021121730
-
Geometrical effects in elastic/plastic indentation
-
D.B. Marshall Geometrical effects in elastic/plastic indentation J. Am. Ceram. Soc. 67 1 1984 57 60
-
(1984)
J. Am. Ceram. Soc.
, vol.67
, Issue.1
, pp. 57-60
-
-
Marshall, D.B.1
-
14
-
-
0032029291
-
Validation of the erosion map of spherical particle impacts on glass
-
M.A. Verspui, P.J. Slikkerveer, G.J.E. Skerka, I. Oomen, and G. de With Validation of the erosion map of spherical particle impacts on glass Wear 215 1998 77 82
-
(1998)
Wear
, vol.215
, pp. 77-82
-
-
Verspui, M.A.1
Slikkerveer, P.J.2
Skerka, G.J.E.3
Oomen, I.4
De With, G.5
-
15
-
-
0033389712
-
Simulation model for the erosion of brittle materials
-
M.A. Verspui, G. de With, A. Corbijn, and P.J. Slikkerveer Simulation model for the erosion of brittle materials Wear 233-235 1999 436 443
-
(1999)
Wear
, vol.233-235
, pp. 436-443
-
-
Verspui, M.A.1
De With, G.2
Corbijn, A.3
Slikkerveer, P.J.4
-
17
-
-
0036850679
-
A closer look at ductile brittle transition in solid particle erosion
-
H. Wensink, and M.C. Elwenspoek A closer look at ductile brittle transition in solid particle erosion Wear 253 2002 1035 1043
-
(2002)
Wear
, vol.253
, pp. 1035-1043
-
-
Wensink, H.1
Elwenspoek, M.C.2
-
18
-
-
0013578571
-
Erosive wear mapping of pipeline materials
-
The Plastic and Rubber Institute, Koninshof, The Netherlands, 21-24 September paper E1/4
-
A.J. Moore, R.J.K. Wood, Erosive wear mapping of pipeline materials. Plastic Pipes VIII, The Plastic and Rubber Institute, Koninshof, The Netherlands, 21-24 September 1992, pp. 1-10, paper E1/4.
-
(1992)
Plastic Pipes VIII
, pp. 1-10
-
-
Moore, A.J.1
Wood, R.J.K.2
-
19
-
-
0032194358
-
Design and performance of a high velocity air-sand jet impingement erosion facility
-
R.J.K. Wood, and D.W. Wheeler Design and performance of a high velocity air-sand jet impingement erosion facility Wear 220 1999 95 112
-
(1999)
Wear
, vol.220
, pp. 95-112
-
-
Wood, R.J.K.1
Wheeler, D.W.2
-
21
-
-
0026223449
-
The role of particle properties on the erosive wear of sintered boron carbide
-
P.H. Shipway, and I.M. Hutchings The role of particle properties on the erosive wear of sintered boron carbide Wear 149 1991 85 98
-
(1991)
Wear
, vol.149
, pp. 85-98
-
-
Shipway, P.H.1
Hutchings, I.M.2
-
22
-
-
0030111777
-
The role of particle properties in the erosion of brittle materials
-
P.H. Shipway, and I.M. Hutchings The role of particle properties in the erosion of brittle materials Wear 193 1996 105 113
-
(1996)
Wear
, vol.193
, pp. 105-113
-
-
Shipway, P.H.1
Hutchings, I.M.2
-
23
-
-
1542316665
-
CVD diamond: Erosion-resistant hard material
-
D.W. Wheeler, and R.J.K. Wood CVD diamond: erosion-resistant hard material Surf. Eng. 19 2003 466 470
-
(2003)
Surf. Eng.
, vol.19
, pp. 466-470
-
-
Wheeler, D.W.1
Wood, R.J.K.2
-
24
-
-
0035270946
-
High velocity sand impact damage on CVD diamond
-
D.W. Wheeler, and R.J.K. Wood High velocity sand impact damage on CVD diamond Diamond Relat. Mater. 10 2001 459 462
-
(2001)
Diamond Relat. Mater.
, vol.10
, pp. 459-462
-
-
Wheeler, D.W.1
Wood, R.J.K.2
-
26
-
-
0023210614
-
Solid particle erosion in brittle materials. Part 3. The interaction with material properties and that of the impingement particle on erosive wear mechanism
-
S. Wada, and W. Watanabe Solid particle erosion in brittle materials. Part 3. The interaction with material properties and that of the impingement particle on erosive wear mechanism Yogyo-Kyokai Shi 1987 573 578
-
(1987)
Yogyo-Kyokai Shi
, pp. 573-578
-
-
Wada, S.1
Watanabe, W.2
-
27
-
-
0024141945
-
Effect of erodent hardness on erosion of brittle materials
-
S. Srinivasan, and R. Scattergood Effect of erodent hardness on erosion of brittle materials Wear 128 1988 139 152
-
(1988)
Wear
, vol.128
, pp. 139-152
-
-
Srinivasan, S.1
Scattergood, R.2
-
28
-
-
17544398023
-
Sand erosion performance of CVD boron carbide coated tungsten carbide
-
R.J.K. Wood, D.W. Wheeler, D.C. Lejeau, and B.G. Mellor Sand erosion performance of CVD boron carbide coated tungsten carbide Wear 233-235 1999 134 150
-
(1999)
Wear
, vol.233-235
, pp. 134-150
-
-
Wood, R.J.K.1
Wheeler, D.W.2
Lejeau, D.C.3
Mellor, B.G.4
-
29
-
-
4244063461
-
Erosive wear behaviour of thick chemical vapour deposited diamond coatings
-
D.W. Wheeler, and R.J.K. Wood Erosive wear behaviour of thick chemical vapour deposited diamond coatings Wear 225-229 1999 523 536
-
(1999)
Wear
, vol.225-229
, pp. 523-536
-
-
Wheeler, D.W.1
Wood, R.J.K.2
-
30
-
-
10644261997
-
High velocity solid particle erosion behaviour of CVD boron carbide on tungsten carbide
-
K. Bose, and R.J.K. Wood High velocity solid particle erosion behaviour of CVD boron carbide on tungsten carbide Wear 258 2005 366 376
-
(2005)
Wear
, vol.258
, pp. 366-376
-
-
Bose, K.1
Wood, R.J.K.2
|