메뉴 건너뛰기




Volumn 402, Issue 1-2, 2005, Pages 177-187

Analysis and prevention of side cracking phenomenon occurring during hot rolling of thick low-carbon steel plates

Author keywords

Hot rolling; Iron oxide layer; Low carbon steel plate; Pearlite band structure; Side cracking

Indexed keywords

BAND STRUCTURE; CRACKING (CHEMICAL); CRACKS; HIGH TEMPERATURE EFFECTS; IRON OXIDES; MICROSTRUCTURE; OXIDATION; PLATES (STRUCTURAL COMPONENTS);

EID: 23044450879     PISSN: 09215093     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.msea.2005.04.045     Document Type: Article
Times cited : (35)