Volumn 166, Issue 2, 2005, Pages 256-267

Cathodic protection of cooling water systems and selection of appropriate materials

Author keywords

Appropriate materials; Cathodic protection; Cooling water systems

Indexed keywords

BIOCIDES; CATHODIC PROTECTION; CHEMICAL ACTIVATION; FOULING; MICROBIOLOGY; SOILS; WATER SUPPLY SYSTEMS;

EID: 22944475277     PISSN: 09240136     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jmatprotec.2004.09.074     Document Type: Article
Times cited : (76)

References (27)
  • 1
    • 2942705608 scopus 로고
    • Field testing a new aluminium anode: Al-Hg-Zn galvanic anode for seawater applications
    • C.F. Schrieber, and J.T. Reding Field testing a new aluminium anode: Al-Hg-Zn galvanic anode for seawater applications Mater. Prot. 6 1967 33 36
    • (1967) Mater. Prot. , vol.6 , pp. 33-36
    • Schrieber, C.F.1    Reding, J.T.2
  • 2
    • 84975382619 scopus 로고
    • Galvanic corrosion characteristics of aluminium alloyed with group IV metals
    • D.S. Keir, M.J. Pryor, and P.R. Sperry Galvanic corrosion characteristics of aluminium alloyed with group IV metals J. Electrochem. Soc. 114 1977 777 782
    • (1977) J. Electrochem. Soc. , vol.114 , pp. 777-782
    • Keir, D.S.1    Pryor, M.J.2    Sperry, P.R.3
  • 3
    • 0028519679 scopus 로고
    • The effect of tin activated aluminium alloy anodes of the addition of bismuth
    • I. Gurrappa, and J.A. Karnik The effect of tin activated aluminium alloy anodes of the addition of bismuth Corros. Prev. Control 41 1994 117 121
    • (1994) Corros. Prev. Control , vol.41 , pp. 117-121
    • Gurrappa, I.1    Karnik, J.A.2
  • 4
    • 0027395678 scopus 로고
    • The surface free energy and anode capacity of aluminium alloys
    • I. Gurrappa The surface free energy and anode capacity of aluminium alloys Corros. Prev. Control 40 1993 111 114
    • (1993) Corros. Prev. Control , vol.40 , pp. 111-114
    • Gurrappa, I.1
  • 6
    • 22944485806 scopus 로고    scopus 로고
    • U.S. Patent, 1968. No. 3.368958
    • U.S. Patent, 1968. No. 3.368958.
  • 8
    • 0002726038 scopus 로고
    • Tests on the effect of indium for high performance aluminium anodes
    • T. Sakano, K. Toda, and M. Hanada Tests on the effect of indium for high performance aluminium anodes Mater. Prot. 5 1966 45 50
    • (1966) Mater. Prot. , vol.5 , pp. 45-50
    • Sakano, T.1    Toda, K.2    Hanada, M.3
  • 9
    • 0026174117 scopus 로고
    • Electrochemical investigations of the activation mechanism of aluminium
    • J.U. Chavarin Electrochemical investigations of the activation mechanism of aluminium Corrosion 47 1991 472 479
    • (1991) Corrosion , vol.47 , pp. 472-479
    • Chavarin, J.U.1
  • 10
    • 0021468150 scopus 로고
    • A proposed activation mechanism for Al anodes
    • M.C. Reboul, P.H. Gimenez, and J.J. Rameau A proposed activation mechanism for Al anodes Corrosion 40 1984 366 371
    • (1984) Corrosion , vol.40 , pp. 366-371
    • Reboul, M.C.1    Gimenez, P.H.2    Rameau, J.J.3
  • 11
    • 0027545107 scopus 로고
    • The activation of aluminium by indium ions in chloride, bromide and iodide solutions
    • C.B. Breslin, and W.M. Carroll The activation of aluminium by indium ions in chloride, bromide and iodide solutions Corros. Sci. 34 1993 327 341
    • (1993) Corros. Sci. , vol.34 , pp. 327-341
    • Breslin, C.B.1    Carroll, W.M.2
  • 12
    • 0026892935 scopus 로고
    • Activation of aluminium in halide solutions containing activator ions
    • W.M. Carroll, and C.B. Breslin Activation of aluminium in halide solutions containing activator ions Corros. Sci. 33 1992 1161 1177
    • (1992) Corros. Sci. , vol.33 , pp. 1161-1177
    • Carroll, W.M.1    Breslin, C.B.2
  • 13
    • 0003281883 scopus 로고
    • Activation mechanism for sacrificial Al-Zn-Hg anodes
    • M.C. Reboul, and M.C. Delatte Activation mechanism for sacrificial Al-Zn-Hg anodes Mater. Perform. 19 1980 35 41
    • (1980) Mater. Perform. , vol.19 , pp. 35-41
    • Reboul, M.C.1    Delatte, M.C.2
  • 14
    • 0027333805 scopus 로고
    • Effect of magnesium addition on the surface free energy and anode capacity of indium activated aluminium alloys
    • A.G. Kulkarni, and I. Gurrappa Effect of magnesium addition on the surface free energy and anode capacity of indium activated aluminium alloys Br. Corros. J. 28 1993 67 70
    • (1993) Br. Corros. J. , vol.28 , pp. 67-70
    • Kulkarni, A.G.1    Gurrappa, I.2
  • 15
    • 0027545112 scopus 로고
    • The electrochemical characteristics of aluminium galvanic anodes in an arctic seawater
    • A. Tamada, and Y. Tamura The electrochemical characteristics of aluminium galvanic anodes in an arctic seawater Corros. Sci. 34 1993 261 277
    • (1993) Corros. Sci. , vol.34 , pp. 261-277
    • Tamada, A.1    Tamura, Y.2
  • 16
    • 0023331201 scopus 로고
    • Improvement of the current efficiency of an Al-Zn-In anodes by heat treatment
    • J.C. Lin, and H.C. Shih Improvement of the current efficiency of an Al-Zn-In anodes by heat treatment J. Electrochem. Soc. 134 1987 817 823
    • (1987) J. Electrochem. Soc. , vol.134 , pp. 817-823
    • Lin, J.C.1    Shih, H.C.2
  • 17
    • 3843088937 scopus 로고
    • Effect of heat treatment on anode capacity of indium activated aluminium alloys
    • I. Gurrappa, and J.A. Karnik Effect of heat treatment on anode capacity of indium activated aluminium alloys SAEST 28 1993 118 122
    • (1993) SAEST , vol.28 , pp. 118-122
    • Gurrappa, I.1    Karnik, J.A.2
  • 18
    • 0030153524 scopus 로고    scopus 로고
    • Development of aluminium alloy anodes for cathodic protection of ships
    • I. Gurrappa, and J.A. Karnik Development of aluminium alloy anodes for cathodic protection of ships Corros. Prev. Control 43 1996 77 82
    • (1996) Corros. Prev. Control , vol.43 , pp. 77-82
    • Gurrappa, I.1    Karnik, J.A.2
  • 19
    • 0019565781 scopus 로고
    • A comparison of anodes for impressed current systems
    • J.A. Jakobs A comparison of anodes for impressed current systems Mater. Perform. 20 1981 17 23
    • (1981) Mater. Perform. , vol.20 , pp. 17-23
    • Jakobs, J.A.1
  • 20
    • 22944465874 scopus 로고
    • Precious metal anodes-state of the art
    • E.W. Dreyman Precious metal anodes-state of the art Mater. Prot. Perform. 11 1972 17 20
    • (1972) Mater. Prot. Perform. , vol.11 , pp. 17-20
    • Dreyman, E.W.1
  • 21
    • 22944475066 scopus 로고
    • Performance of Pt anodes in impressed current cathodic protection
    • R. Babosian Performance of Pt anodes in impressed current cathodic protection Mater. Perform. 16 1977 20 25
    • (1977) Mater. Perform. , vol.16 , pp. 20-25
    • Babosian, R.1
  • 22
    • 0024096015 scopus 로고
    • Cathodic protection using ceramic-coated anodes
    • A. Kumar, and M.D. Armstrong Cathodic protection using ceramic-coated anodes Mater. Perform. 27 1988 19 23
    • (1988) Mater. Perform. , vol.27 , pp. 19-23
    • Kumar, A.1    Armstrong, M.D.2
  • 23
    • 0024571198 scopus 로고
    • Conductive rubber as an impressed anode-cathodic protection of steel-reinforced concrete
    • R.J. Kessler, and R.G. Powers Conductive rubber as an impressed anode-cathodic protection of steel-reinforced concrete Mater. Perform. 28 1989 24 27
    • (1989) Mater. Perform. , vol.28 , pp. 24-27
    • Kessler, R.J.1    Powers, R.G.2
  • 24
    • 22944469863 scopus 로고    scopus 로고
    • Applications of cathodic protection for the protection of aqueous and soil corrosion of power plant components
    • A.K. Sinha, A.K. Mitra, U.C. Bhakta, and S.K. Sanyal Applications of cathodic protection for the protection of aqueous and soil corrosion of power plant components CORRCORN 1 1999 837 845
    • (1999) CORRCORN , vol.1 , pp. 837-845
    • Sinha, A.K.1    Mitra, A.K.2    Bhakta, U.C.3    Sanyal, S.K.4
  • 27
    • 0022182427 scopus 로고
    • Development of an expert system for design consultation on marine corrosion
    • J.N. Wanklyn, and N.J.M. Wilkins Development of an expert system for design consultation on marine corrosion Br. Corros. J. 20 1985 161 166
    • (1985) Br. Corros. J. , vol.20 , pp. 161-166
    • Wanklyn, J.N.1    Wilkins, N.J.M.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.