Volumn , Issue , 2004, Pages 1703-1708

Oilfield environment-induced stress corrosion cracking of CRAs in comoletion brines

Author keywords

[No Author keywords available]

Indexed keywords

BRINES; CORROSION; CORROSION RESISTANT ALLOYS; CRACK INITIATION; HIGH TEMPERATURE APPLICATIONS; NITROGEN; SAND; STRESS ANALYSIS; TEMPERATURE DISTRIBUTION; TUBING;

EID: 22044432878     PISSN: None     EISSN: None     Source Type: Conference Proceeding    
DOI: None     Document Type: Conference Paper
Times cited : (27)

References (11)
  • 1
    • 22044446521 scopus 로고    scopus 로고
    • Corrosion behavior of super 13Cr martensitic stainless steels in completion fluids
    • Ibrahim, M.Z., et.al. : "Corrosion Behavior of Super 13Cr Martensitic Stainless Steels in Completion Fluids," NACE Corrosion/03 Paper No. 03097.
    • NACE Corrosion/03 Paper No. 03097
    • Ibrahim, M.Z.1
  • 3
    • 22044443451 scopus 로고
    • 2 corrosion behavior of carbon and alloy steels in high concentration brine solution
    • St. Louis, Missouri, March 21-25
    • 2 Corrosion Behavior of Carbon and Alloy Steels in High Concentration Brine Solution," NACE Corrosion/88 Paper No. 212, St. Louis, Missouri, March 21-25, 1988.
    • (1988) NACE Corrosion/88 Paper No. 212 , vol.212
    • Burke, P.A.1
  • 4
    • 85085400838 scopus 로고    scopus 로고
    • Erskine field HPHT workover and tubing corrosion failure investigation
    • SPE/IADC 67779, presented at the The Netherlands, February 27-March 1
    • Mowat, D.E., et al: "Erskine Field HPHT Workover and Tubing Corrosion Failure Investigation," SPE/IADC 67779, presented at the 2001 SPE/IADC Drilling Conference in Amsterdam, The Netherlands, February 27-March 1, 2001.
    • (2001) 2001 SPE/IADC Drilling Conference in Amsterdam
    • Mowat, D.E.1
  • 5
    • 1142288576 scopus 로고    scopus 로고
    • Use of high-strength alloys and elastomers in heavy completion brines
    • SPE 84515, presented at the Colorado, October 5-8
    • Silverman, S.A. et al : "Use of High-Strength Alloys and Elastomers in Heavy Completion Brines," SPE 84515, presented at the SPE Annual Technical Conference and Exhibition in Denver, Colorado, October 5-8, 2003.
    • (2003) SPE Annual Technical Conference and Exhibition in Denver
    • Silverman, S.A.1
  • 6
    • 0022451274 scopus 로고
    • Corrosivity of heavy brines -understanding it and techniques operators can use to control it
    • OTC 5266, presented at the Texas, May 5-8
    • th Annual OTC in Houston, Texas, May 5-8, 1986.
    • (1986) th Annual OTC in Houston
    • Hudson, T.E.1
  • 7
    • 22044437252 scopus 로고    scopus 로고
    • Corrosion behavior of CRAs in high density packer fluids at high temperature
    • Paper 592, Houston, TX, NACE
    • Scorpio, L., et al.: "Corrosion Behavior of CRAs in High Density Packer Fluids at High Temperature," Corrosion 1999, Paper 592, Houston, TX, NACE 1999.
    • (1999) Corrosion 1999
    • Scorpio, L.1
  • 8
    • 0242321882 scopus 로고    scopus 로고
    • The chemistry of formate brines at downhole conditions
    • SPE 80211, presented at the Texas, February 5-8
    • Javora, P.H., et al. : "The Chemistry of Formate Brines at Downhole Conditions," SPE 80211, presented at the SPE International Symposium on Oilfield Chemistry in Houston, Texas, February 5-8, 2003.
    • (2003) SPE International Symposium on Oilfield Chemistry in Houston
    • Javora, P.H.1
  • 9
    • 0028268816 scopus 로고
    • Evaluation of potassium carbonate as a non-corrosive, chloride-free completion fluid
    • SPE 27392, presented at the Louisiana, February 7-10
    • Houchin, L.R., et al: "Evaluation of Potassium Carbonate as a Non-Corrosive, Chloride-Free Completion Fluid," SPE 27392, presented at the SPE International Symposium on Formation Damage Control in Lafayette, Louisiana, February 7-10, 1994.
    • (1994) SPE International Symposium on Formation Damage Control in Lafayette
    • Houchin, L.R.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.