메뉴 건너뛰기




Volumn 52, Issue 4, 2005, Pages 207-213

A comparative study on the corrosion behaviour of simulated archaeological iron in Cl-, NO3- and HSO3 - bearing pollutants

Author keywords

Corrosion; Iron

Indexed keywords

ADSORPTION; CHLORINE; ELECTROCHEMISTRY; IRON; NEGATIVE IONS; NITROGEN OXIDES; POLARIZATION; SCANNING ELECTRON MICROSCOPY; X RAY DIFFRACTION ANALYSIS;

EID: 21544459864     PISSN: 00035599     EISSN: None     Source Type: Journal    
DOI: 10.1108/00035590510603229     Document Type: Article
Times cited : (4)

References (11)
  • 1
    • 21544472380 scopus 로고
    • The corrosion of iron/ and zinc by atmospheric hydrogen chloride
    • Askey, A. and Blyon, S. (1990), "The corrosion of iron/ and zinc by atmospheric hydrogen chloride", Corrosion Science, Vol. 25, p. 379.
    • (1990) Corrosion Science , vol.25 , pp. 379
    • Askey, A.1    Blyon, S.2
  • 2
    • 21544432453 scopus 로고    scopus 로고
    • Synergistic effect of chloride and sulphur-bearing pollutant in atmospheric corrosion of mild steel
    • Cai, J. (1996), "Synergistic effect of chloride and sulphur-bearing pollutant in atmospheric corrosion of mild steel", Journal of Chinese for Corrosion and Protection, Vol. 16 No. 4, p. 303.
    • (1996) Journal of Chinese for Corrosion and Protection , vol.16 , Issue.4 , pp. 303
    • Cai, J.1
  • 4
    • 0037374985 scopus 로고    scopus 로고
    • The effect of environmental and meteorological variables on atmospheric corrosion of carbon steel, copper, zinc and aluminium in a limited geographic zone with different types of environment
    • Juan, J. and Rodriyuez, S. (2003), "The effect of environmental and meteorological variables on atmospheric corrosion of carbon steel, copper, zinc and aluminium in a limited geographic zone with different types of environment", Corrosion Science, Vol. 45, pp. 799-815.
    • (2003) Corrosion Science , vol.45 , pp. 799-815
    • Juan, J.1    Rodriyuez, S.2
  • 5
    • 21544471247 scopus 로고    scopus 로고
    • Li, D. BUAA Press Beijing
    • Li, D. (2002) in Li, D. (Ed.), Electrochemistry, BUAA Press, Beijing, p. 163.
    • (2002) Electrochemistry , pp. 163
    • Li, D.1
  • 6
    • 0031231256 scopus 로고
    • 3 on the corrosion of copper, zinc and aluminium
    • 3 on the corrosion of copper, zinc and aluminium", Corrosion Science, Vol. 39 No. 9, p. 1505.
    • (1991) Corrosion Science , vol.39 , Issue.9 , pp. 1505
    • Oesch, S.1    Faller, M.2
  • 7
    • 0027593997 scopus 로고
    • The oxidation of Ferrous hydroxide in chloride containing aqueous media and pourbaix diagram of Green rust one
    • Re Fai, T.P.H. and Enin, J-M.R.G. (1993), "The oxidation of Ferrous hydroxide in chloride containing aqueous media and pourbaix diagram of Green rust one", Corrosion Science, Vol. 34 No. 5, pp. 797-819.
    • (1993) Corrosion Science , vol.34 , Issue.5 , pp. 797-819
    • Re Fai, T.P.H.1    Enin, J.-M.R.G.2
  • 8
    • 2442613774 scopus 로고    scopus 로고
    • Formation and growth of micro-droplets during the initial stage of atmospheric corrosion
    • Tsuru, T., Ken-Ichiro, T. and Nishikatal, A. (2004), "Formation and growth of micro-droplets during the initial stage of atmospheric corrosion", Electrochimica Acta, Vol. 49, p. 2709.
    • (2004) Electrochimica Acta , vol.49 , pp. 2709
    • Tsuru, T.1    Ken-Ichiro, T.2    Nishikatal, A.3
  • 11
    • 21544477010 scopus 로고
    • Factors that effect the atmospheric corrosion of steel and iron
    • Zhang, A. (1989), "Factors that effect the atmospheric corrosion of steel and iron", Material protection, Vol. 22 No. 2, p. 15.
    • (1989) Material Protection , vol.22 , Issue.2 , pp. 15
    • Zhang, A.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.