Improvement of wood properties by impregnation with polyglycerol methacrylate

Author keywords

[No Author keywords available]

Indexed keywords

BIOCIDES; CHEMICAL MODIFICATION; CONCENTRATION (PROCESS); CURING; DIMENSIONAL STABILITY; ESTERS; FUNGUS ATTACK; GLYCEROL; MOLECULAR WEIGHT; POLYMERS;

EID: 21044440878     PISSN: 00183768     EISSN: None     Source Type: Trade Journal    
DOI: 10.1007/s00107-004-0485-y     Document Type: Article
Times cited : (23)

References (16)
  • 1
    • 0029469296 scopus 로고
    • Wood preservation. The classics and the new age
    • Barnes HM, Murphy RJ (1995) Wood preservation. The classics and the new age. Forest Prod J 45(9): 16-23
    • (1995) Forest Prod J , vol.45 , Issue.9 , pp. 16-23
    • Barnes, H.M.1    Murphy, R.J.2
  • 2
    • 0026416710 scopus 로고
    • Impregnation of white pine wood with unsaturated polyesters to produce wood-plastic combinations
    • Doss NL, Elawady MM, Elawady NI, Mansour SH (1991) Impregnation of white pine wood with unsaturated polyesters to produce wood-plastic combinations. J Appl Polym Sci 42(9): 2589-2594
    • (1991) J Appl Polym Sci , vol.42 , Issue.9 , pp. 2589-2594
    • Doss, N.L.1    Elawady, M.M.2    Elawady, N.I.3    Mansour, S.H.4
  • 3
    • 0004892347 scopus 로고
    • Durability of wood with acrylic-high-pomymer. Dimensional stability with crosslinked acrylic copolymer in wood
    • Fujimara T, Inoue M, Vemura I (1990) Durability of wood with acrylic-high-pomymer. Dimensional stability with crosslinked acrylic copolymer in wood. Mokuzai Gakkaishi 36(10):851-859
    • (1990) Mokuzai Gakkaishi , vol.36 , Issue.10 , pp. 851-859
    • Fujimara, T.1    Inoue, M.2    Vemura, I.3
  • 4
    • 84975027523 scopus 로고
    • On the stabilization of water logged oakwood in polyethyleneglycol (PEG) II. Designing a two step treatment for multiquality timbers
    • Hoffmann P (1988a) On the stabilization of water logged oakwood in polyethyleneglycol (PEG) II. Designing a two step treatment for multiquality timbers. Studies Conservat 31:103-113
    • (1988) Studies Conservat , vol.31 , pp. 103-113
    • Hoffmann, P.1
  • 5
    • 0000069972 scopus 로고
    • On the stabilization of water logged oakwood in polyethyleneglycol (PEG) III. Testing the oligomers
    • Hoffmann P (1988b) On the stabilization of water logged oakwood in polyethyleneglycol (PEG) III. Testing the oligomers. Holzforschung 42(5): 289-294
    • (1988) Holzforschung , vol.42 , Issue.5 , pp. 289-294
    • Hoffmann, P.1
  • 6
    • 0000424507 scopus 로고
    • On the stabilization of water logged oakwood in polyethyleneglycol (PEG) IV. Species from China and Corea
    • Hoffmann P (1990) On the stabilization of water logged oakwood in polyethyleneglycol (PEG) IV. Species from China and Corea. Holzforschung 44(2): 87-93
    • (1990) Holzforschung , vol.44 , Issue.2 , pp. 87-93
    • Hoffmann, P.1
  • 7
    • 0004620157 scopus 로고
    • Wood-polymer materials in chemistry of solid wood
    • Meyer JA (1984) Wood-polymer materials in chemistry of solid wood. Adv Chem Series 257-289
    • (1984) Adv Chem Series , pp. 257-289
    • Meyer, J.A.1
  • 8
    • 0002682262 scopus 로고
    • Reaction of glyoxal and glyoxal/glycol with wood
    • Nakano T (1994) Reaction of glyoxal and glyoxal/glycol with wood. Wood Sci Technol 28:23-33
    • (1994) Wood Sci Technol , vol.28 , pp. 23-33
    • Nakano, T.1
  • 9
    • 0000290552 scopus 로고
    • Penetration and reactivity of cell wall components in chemistry of solid wood
    • Rowell RM (1984) Penetration and reactivity of cell wall components in chemistry of solid wood. Adv Chem Series 175-210
    • (1984) Adv Chem Series , pp. 175-210
    • Rowell, R.M.1
  • 10
    • 0001652472 scopus 로고
    • Wood polymer composites
    • Schneider MH (1994) Wood polymer composites. Wood Fiber Sci 26(1):142-151
    • (1994) Wood Fiber Sci , vol.26 , Issue.1 , pp. 142-151
    • Schneider, M.H.1
  • 11
    • 0001042430 scopus 로고
    • Effect of polyethyleneglycol on the dimensional stability of wood
    • Stamm AJ (1959) Effect of polyethyleneglycol on the dimensional stability of wood. Forest Prod J 9:375-381
    • (1959) Forest Prod J , vol.9 , pp. 375-381
    • Stamm, A.J.1
  • 12
    • 0000973141 scopus 로고
    • Factors affecting bulking and dimensional stability of wood
    • Stamm A J (1965) Factors affecting bulking and dimensional stability of wood. Forest Prod J 14:403-408
    • (1965) Forest Prod J , vol.14 , pp. 403-408
    • Stamm, A.J.1
  • 13
    • 0345812352 scopus 로고    scopus 로고
    • Novel wood preservatives
    • Suttie E (1997) Novel wood preservatives. Chem Ind 18:720-724
    • (1997) Chem Ind , vol.18 , pp. 720-724
    • Suttie, E.1
  • 16
    • 0001448043 scopus 로고
    • Chemical modification of wood by non formaldehyde cross-linking reagents
    • Yasuda R, Minato K (1995) Chemical modification of wood by non formaldehyde cross-linking reagents. Wood Sci Technol 29:243-251
    • (1995) Wood Sci Technol , vol.29 , pp. 243-251
    • Yasuda, R.1    Minato, K.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.