Volumn 25, Issue 12 SPEC. ISS., 2005, Pages 2587-2591
|
Characterization of (1 - x) La0.83Sr0.17 Ga0.83Mg0.17O2.83 - xLa0.8 Sr0.2MnO3 (0≤x≤1) composite cathodes
|
Author keywords
Composites; Electrical conductivity; Fuel cells; LSGM; Perovskites
|
Indexed keywords
ELECTRIC CONDUCTIVITY;
ELECTRIC IMPEDANCE;
ENERGY DISPERSIVE SPECTROSCOPY;
GALLIUM COMPOUNDS;
GRAIN SIZE AND SHAPE;
HEAT TREATMENT;
SINTERING;
X RAY POWDER DIFFRACTION;
IMPEDANCE SPECTROSCOPY;
PHASE ANALYSIS;
RELATIVE DENSITIES;
LANTHANUM COMPOUNDS;
CERAMICS;
|
EID: 20644446262
PISSN: 09552219
EISSN: None
Source Type: Journal
DOI: 10.1016/j.jeurceramsoc.2005.03.107 Document Type: Article |
Times cited : (22)
|
References (13)
|