Volumn 256, Issue 7-8, 2004, Pages 714-719

Solid-particle erosion of a geopolymer containing fly ash and blast-furnace slag

Author keywords

Aluminosilicate; Erosion; Fracture; Geopolymer

Indexed keywords

ALUMINUM COMPOUNDS; BLAST FURNACES; CRACK PROPAGATION; ELASTOPLASTICITY; EROSION; MICROCRACKS; SCANNING TUNNELING MICROSCOPY; SLAGS; VELOCITY MEASUREMENT; WEAR OF MATERIALS;

EID: 1842732801     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0043-1648(03)00463-0     Document Type: Article
Times cited : (44)

References (36)
  • 3
    • 0018298070 scopus 로고
    • Synthesis of new high-temperature geo-polymers for reinforced plastics/composites
    • Society of Plastic Engineers, Brookfield, CT
    • J. Davidovits, Synthesis of new high-temperature geo-polymers for reinforced plastics/composites, in: Proceedings of PACTEC 79, Society of Plastic Engineers, Brookfield, CT, 1979, pp. 151-154.
    • (1979) Proceedings of PACTEC 79 , pp. 151-154
    • Davidovits, J.1
  • 4
    • 0026207945 scopus 로고
    • Geopolymers: Inorganic polymeric new materials
    • Davidovits J.Geopolymers: Inorganic polymeric new materials J. Therm. Anal. 37 1991 1633-1656
    • (1991) J. Therm. Anal. , vol.37 , pp. 1633-1656
    • Davidovits, J.1
  • 7
    • 0033740501 scopus 로고    scopus 로고
    • The geopolymerization of alumino-silicate minerals
    • Xu H.van Deventer J.S.J.The geopolymerization of alumino-silicate minerals Int. J. Miner. Proc. 59 2000 247-266
    • (2000) Int. J. Miner. Proc. , vol.59 , pp. 247-266
    • Xu, H.1    van Deventer, J.S.J.2
  • 8
    • 0034254016 scopus 로고    scopus 로고
    • Mechanism of polysialation in the incorporation of zirconia into fly ash-based geopolymers
    • Phair J.W.van Deventer J.S.J.Smith J.D.Mechanism of polysialation in the incorporation of zirconia into fly ash-based geopolymers Ind. Eng. Chem. Res. 39 2000 2925-2934
    • (2000) Ind. Eng. Chem. Res. , vol.39 , pp. 2925-2934
    • Phair, J.W.1    van Deventer, J.S.J.2    Smith, J.D.3
  • 9
    • 0037977532 scopus 로고
    • Stabilisation of cadmium and lead in Portland cement paste using a synthetic seawater leachant
    • Campbell K.M.El-Korchi T.Gress D.Bishop P.Stabilisation of cadmium and lead in Portland cement paste using a synthetic seawater leachant Environ. Prog. 6 1987 99-103
    • (1987) Environ. Prog. , vol.6 , pp. 99-103
    • Campbell, K.M.1    El-Korchi, T.2    Gress, D.3    Bishop, P.4
  • 10
    • 0345533622 scopus 로고
    • New Hope for Toxic Waste
    • Comrie D.C.New Hope for Toxic Waste The World and I 38 1988 171-177
    • (1988) The World and I , vol.38 , pp. 171-177
    • Comrie, D.C.1
  • 11
    • 0032712971 scopus 로고    scopus 로고
    • The potential use of geopolymeric materials to immobilise toxic metals. Part II. Material and leaching characteristics
    • van Jaarsveld J.G.S.van Deventer J.S.J.Schwartzmann A.The potential use of geopolymeric materials to immobilise toxic metals. Part II. Material and leaching characteristics Miner. Eng. 12 1999 75-91
    • (1999) Miner. Eng. , vol.12 , pp. 75-91
    • van Jaarsveld, J.G.S.1    van Deventer, J.S.J.2    Schwartzmann, A.3
  • 12
    • 0027307279 scopus 로고
    • Ordinary Portland cement based solidification of toxic waste: The role of OPC reviewed
    • Hills C.D.Sollars C.J.Perry R.Ordinary Portland cement based solidification of toxic waste: The role of OPC reviewed Cem. Concrete Res. 23 1993 196-212
    • (1993) Cem. Concrete Res. , vol.23 , pp. 196-212
    • Hills, C.D.1    Sollars, C.J.2    Perry, R.3
  • 13
    • 1842743440 scopus 로고
    • Stabilizing hazardous waste
    • Conner J.R.Stabilizing hazardous waste Chemtech 23 12 1993 35-44
    • (1993) Chemtech , vol.23 , Issue.12 , pp. 35-44
    • Conner, J.R.1
  • 14
    • 0031035986 scopus 로고    scopus 로고
    • Chemically bonded phosphate ceramics for low-level mixed-waste stabilization
    • Singh D.Wagh A.S.Cunnane J.Mayberry J.Chemically bonded phosphate ceramics for low-level mixed-waste stabilization J. Environ. Sci. Health A32 1997 527-541
    • (1997) J. Environ. Sci. Health , vol.A32 , pp. 527-541
    • Singh, D.1    Wagh, A.S.2    Cunnane, J.3    Mayberry, J.4
  • 15
    • 0033098486 scopus 로고    scopus 로고
    • Stabilization of rocky flats Pu-contaminated ash within chemically bonded phosphate ceramics
    • Wagh A.Strain R.Jeong S.Y.Reed D.Krause T.Singh D.Stabilization of rocky flats Pu-contaminated ash within chemically bonded phosphate ceramics J. Nucl. Mater. 265 1999 265-307
    • (1999) J. Nucl. Mater. , vol.265 , pp. 265-307
    • Wagh, A.1    Strain, R.2    Jeong, S.Y.3    Reed, D.4    Krause, T.5    Singh, D.6
  • 16
    • 0025596524 scopus 로고
    • Laboratory evaluation of wet and dry abrasion resistance of cement mortar
    • Fwa T.F.Low E.W.Laboratory evaluation of wet and dry abrasion resistance of cement mortar Cem. Concrete Aggreg. 12 1990 101-106
    • (1990) Cem. Concrete Aggreg. , vol.12 , pp. 101-106
    • Fwa, T.F.1    Low, E.W.2
  • 17
    • 0028501742 scopus 로고
    • Fundamental investigations on concrete wear by high velocity water flow
    • Momber A.Kovacevic R.Fundamental investigations on concrete wear by high velocity water flow Wear 177 1994 55-62
    • (1994) Wear , vol.177 , pp. 55-62
    • Momber, A.1    Kovacevic, R.2
  • 20
    • 0030368419 scopus 로고    scopus 로고
    • Degradation of structural ceramics by erosion
    • Routbort J.L.Degradation of structural ceramics by erosion J. Nondestr. Eval. 15 1996 107-112
    • (1996) J. Nondestr. Eval. , vol.15 , pp. 107-112
    • Routbort, J.L.1
  • 21
    • 0041113006 scopus 로고
    • Australian Standard AS 1012.9
    • Australian Standard AS 1012.9, Methods for Testing Concrete (1986).
    • (1986) Methods for Testing Concrete
  • 22
    • 0026416929 scopus 로고
    • Erosion of work-hardened copper, nickel, and 304 stainless steel
    • Goretta K.C.Arroyo R.C.Wu C.-T.Routbort J.L.Erosion of work-hardened copper, nickel, and 304 stainless steel Wear 147 1991 145-154
    • (1991) Wear , vol.147 , pp. 145-154
    • Goretta, K.C.1    Arroyo, R.C.2    Wu, C.-T.3    Routbort, J.L.4
  • 24
    • 0018305252 scopus 로고
    • Strength degradation of glass impacted with sharp particles
    • Wiederhorn S.M.Lawn B.R.Strength degradation of glass impacted with sharp particles. I J. Am. Ceram. Soc. 62 1979 66-70
    • (1979) I J. Am. Ceram. Soc. , vol.62 , pp. 66-70
    • Wiederhorn, S.M.1    Lawn, B.R.2
  • 25
    • 0020718748 scopus 로고
    • Effect of material parameters on the erosion resistance of brittle materials
    • Wiederhorn S.M.Hockey B.J.Effect of material parameters on the erosion resistance of brittle materials J. Mater. Sci. 18 1980 766-780
    • (1980) J. Mater. Sci. , vol.18 , pp. 766-780
    • Wiederhorn, S.M.1    Hockey, B.J.2
  • 27
    • 0002007637 scopus 로고
    • Solid-particle erosion of ceramics and ceramic composites
    • J.E. Ritter (Ed.), Trans Tech. Pub., Geneva
    • J.L. Routbort, R.O. Scattergood, Solid-particle erosion of ceramics and ceramic composites, in: J.E. Ritter (Ed.), Erosion of Ceramic Materials, Trans Tech. Pub., Geneva, 1992, pp. 23-51.
    • (1992) Erosion of Ceramic Materials , pp. 23-51
    • Routbort, J.L.1    Scattergood, R.O.2
  • 28
    • 0019058952 scopus 로고
    • Elastic/plastic indentation damage in ceramics: The median/radial crack system
    • Lawn B.R.Evans A.G.Marshall D.B.Elastic/plastic indentation damage in ceramics: The median/radial crack system J. Am. Ceram. Soc. 63 1980 574-581
    • (1980) J. Am. Ceram. Soc. , vol.63 , pp. 574-581
    • Lawn, B.R.1    Evans, A.G.2    Marshall, D.B.3
  • 29
    • 0020206952 scopus 로고
    • Elastic/plastic indentation damage in ceramics: The lateral crack system
    • Marshall D.B.Lawn B.R.Evans A.G.Elastic/plastic indentation damage in ceramics: The lateral crack system J. Am. Ceram. Soc. 65 1982 561-566
    • (1982) J. Am. Ceram. Soc. , vol.65 , pp. 561-566
    • Marshall, D.B.1    Lawn, B.R.2    Evans, A.G.3
  • 36
    • 0031640104 scopus 로고    scopus 로고
    • Influence of reinforcement types on the flexural properties of geopolymer composites
    • Hammell J.Balaguru P.Lyon R.Influence of reinforcement types on the flexural properties of geopolymer composites SAMPE Proc. 43 1998 1600-1608
    • (1998) SAMPE Proc. , vol.43 , pp. 1600-1608
    • Hammell, J.1    Balaguru, P.2    Lyon, R.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.