Degradation of mechanical and electrical properties after long-term oxidation and corrosion of non-oxide structural ceramic composites

Author keywords

Composites; Corrosion; Electrical properties; Mechanical properties; Oxidation

Indexed keywords

COMPOSITE MATERIALS; CORROSION; DEGRADATION; ELECTRIC CONDUCTIVITY; OXIDATION; SILICON COMPOUNDS; STRENGTH OF MATERIALS;

EID: 18144379467     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2004.12.002     Document Type: Article
Times cited : (14)

References (36)
  • 1
    • 0028427496 scopus 로고
    • Review-particulate silicon nitride composite
    • Y.G. Gogotsi Review-particulate silicon nitride composite J. Mater. Sci. 29 1994 2541-2556
    • (1994) J. Mater. Sci. , vol.29 , pp. 2541-2556
    • Gogotsi, Y.G.1
  • 8
    • 0030146895 scopus 로고    scopus 로고
    • Investigation of SiC - AlN: Part II. Mechanical properties
    • J.-L. Huang and J.-M. Jih. Investigation of SiC - AlN: Part II. Mechanical properties J. Am. Ceram. Soc. 79 5 1996 1262-1264
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.5 , pp. 1262-1264
    • Huang, J.-L.1    Jih, J.-M.2
  • 9
    • 0027700947 scopus 로고
    • Properties of silicon nitride-molybdenum disilicide particulate ceramic composites
    • M.-Y. Kao Properties of silicon nitride-molybdenum disilicide particulate ceramic composites J. Am. Cerem. Soc. 76 1993 2879-2883
    • (1993) J. Am. Cerem. Soc. , vol.76 , pp. 2879-2883
    • Kao, M.-Y.1
  • 10
    • 0033189382 scopus 로고    scopus 로고
    • Microstructure-property relations of hot pressed silicon carbide-aluminum nitride compositions at room and elevated temperatures
    • A.H. Lubis N.L. Hecht and G.A. Graves Jr. Microstructure-property relations of hot pressed silicon carbide-aluminum nitride compositions at room and elevated temperatures J. Am. Ceram. Soc. 82 1999 2481-2489
    • (1999) J. Am. Ceram. Soc. , vol.82 , pp. 2481-2489
    • Lubis, A.H.1    Hecht, N.L.2    Graves Jr., G.A.3
  • 15
    • 0035254794 scopus 로고    scopus 로고
    • 4 - TaN Composites. Part I: Densification and microstructure
    • 4 - TaN Composites. Part I: Densification and microstructure J. Eur. Ceram. Soc. 21 2001 219-235
    • (2001) J. Eur. Ceram. Soc. , vol.21 , pp. 219-235
    • Petrovsky, V.Y.1    Rak, Z.S.2
  • 16
    • 0035254590 scopus 로고    scopus 로고
    • 4 - TaN Composites. Part II: Electrical and mechanical properties
    • 4 - TaN Composites. Part II: Electrical and mechanical properties J. Eur. Ceram. Soc. 21 2001 237-244
    • (2001) J. Eur. Ceram. Soc. , vol.21 , pp. 237-244
    • Petrovsky, V.Y.1    Rak, Z.S.2
  • 18
    • 0347926479 scopus 로고    scopus 로고
    • Influence of additive content on the high temperature oxidation of silicon nitride-based composites
    • R. Klein V. Medri M. Desmaison Brut A. Bellosi and J. Desmaison Influence of additive content on the high temperature oxidation of silicon nitride-based composites J. Eur. Ceram. Soc. 23 2003 603-611
    • (2003) J. Eur. Ceram. Soc. , vol.23 , pp. 603-611
    • Klein, R.1    Medri, V.2    Desmaison Brut, M.3    Bellosi, A.4    Desmaison, J.5
  • 19
    • 0026909398 scopus 로고
    • Effects of metallic boride dispersion on fracture toughness and oxidation resistance in SiC ceramics
    • T. Mizutani and A. Tsuge Effects of metallic boride dispersion on fracture toughness and oxidation resistance in SiC ceramics J. Ceram. Soc. Jpn. Int. Ed. 100 1992 979-982
    • (1992) J. Ceram. Soc. Jpn. Int. Ed. , vol.100 , pp. 979-982
    • Mizutani, T.1    Tsuge, A.2
  • 24
    • 9144235568 scopus 로고    scopus 로고
    • Oxidation behaviour of a pressureless sintered AlN - SiC composite
    • Sciti, D., Winterhalter, F. and Bellosi, A., Oxidation behaviour of a pressureless sintered AlN - SiC composite, J. Mater. Sci., 2004, 39 6965-6973.
    • (2004) J. Mater. Sci. , vol.39 , pp. 6965-6973
    • Sciti, D.1    Winterhalter, F.2    Bellosi, A.3
  • 25
  • 27
    • 0037377466 scopus 로고    scopus 로고
    • Long-term stability of nonoxide ceramics in an oxidative environment at 1500°C
    • H. Klemm C. Taut and G. Wötting Long-term stability of nonoxide ceramics in an oxidative environment at 1500 °C J. Eur. Ceram. Soc. 23 2003 619-627
    • (2003) J. Eur. Ceram. Soc. , vol.23 , pp. 619-627
    • Klemm, H.1    Taut, C.2    Wötting, G.3
  • 28
    • 0035497582 scopus 로고    scopus 로고
    • Silicon nitride/molybdenum disilicide composite with superior long-term oxidation resistance at 1500°C
    • H. Klemm and C. Schubert Silicon nitride/molybdenum disilicide composite with superior long-term oxidation resistance at 1500 °C J. Am. Ceram. Soc. 84 2001 2430-2432
    • (2001) J. Am. Ceram. Soc. , vol.84 , pp. 2430-2432
    • Klemm, H.1    Schubert, C.2
  • 29
    • 0030244426 scopus 로고    scopus 로고
    • Influence of molybdenum silicide additions on high-temperature oxidation resistance of silicon nitride materials
    • H. Klemm K. Tangermann C. Schubert and W. Hermel Influence of molybdenum silicide additions on high-temperature oxidation resistance of silicon nitride materials J. Am. Ceram. Soc. 79 1996 2429-2435
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 2429-2435
    • Klemm, H.1    Tangermann, K.2    Schubert, C.3    Hermel, W.4
  • 30
    • 1342347332 scopus 로고    scopus 로고
    • 2 ceramic composite in acid and basic aqueous environments: Surface modifications and properties degradation
    • 2 ceramic composite in acid and basic aqueous environments: Surface modifications and properties degradation Appl. Surf. Sci. 225 2004 100-115
    • (2004) Appl. Surf. Sci. , vol.225 , pp. 100-115
    • Winterhalter, F.1    Medri, V.2    Ruffini, A.3    Bellosi, A.4
  • 33
    • 0029276041 scopus 로고
    • Investigation of SiC - AlN system: Part I. Microstructure and solid solution
    • J.-L. Huang and J.-M. Jih Investigation of SiC - AlN system: Part I. Microstructure and solid solution J. Mater. Res. 10 1995 651-658
    • (1995) J. Mater. Res. , vol.10 , pp. 651-658
    • Huang, J.-L.1    Jih, J.-M.2
  • 34
    • 0020735560 scopus 로고
    • Investigation of phase stability in the system SiC - AlN
    • W. Rafaniello M.R. Plichta and A.V. Virkar Investigation of phase stability in the system SiC - AlN J. Am. Ceram. Soc. 66 1993 272-275
    • (1993) J. Am. Ceram. Soc. , vol.66 , pp. 272-275
    • Rafaniello, W.1    Plichta, M.R.2    Virkar, A.V.3
  • 35
    • 0032095370 scopus 로고    scopus 로고
    • Hot isostatically pressed SiC - AlN powder mixtures: Effect of milling on solid solution formation and related properties
    • J.-F. Li A. Kawasaki and R. Watanabe Hot isostatically pressed SiC - AlN powder mixtures: Effect of milling on solid solution formation and related properties J. Am. Ceram. Soc. 81 1998 1445-1452
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 1445-1452
    • Li, J.-F.1    Kawasaki, A.2    Watanabe, R.3
  • 36
    • 51249179091 scopus 로고
    • Preparation and mechanical properties of SiC - AlN ceramic alloy
    • J.-F. Li and R. Watanabe Preparation and mechanical properties of SiC - AlN ceramic alloy J. Mater. Sci. 26 1991 4813-4817
    • (1991) J. Mater. Sci. , vol.26 , pp. 4813-4817
    • Li, J.-F.1    Watanabe, R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.