The durability of bonded aluminium joints: A comparison of AC and DC anodising pretreatments

Author keywords

B. Aluminium and alloys; B. Surface treatment; C. Infrared spectra; C. Wedge tests

Indexed keywords

ALUMINUM ALLOYS; ALUMINUM COMPOUNDS; ANODIC OXIDATION; CORROSION RESISTANCE; CURING; DURABILITY; FOURIER TRANSFORM INFRARED SPECTROSCOPY; HEAT TREATMENT; HYDRATES; JOINTS (STRUCTURAL COMPONENTS); SEALING (CLOSING); SULFURIC ACID; SURFACE TREATMENT;

EID: 1642519686     PISSN: 01437496     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ijadhadh.2003.09.003     Document Type: Article
Times cited : (24)

References (31)
  • 7
    • 0003916388 scopus 로고
    • E.W. Thrall, & R.W. Shannon. New York: Marcel Dekker
    • Rogers N.L. Thrall E.W., Shannon R.W. Adhesive bonding of aluminum alloys. 1985;41-50 Marcel Dekker, New York.
    • (1985) Adhesive Bonding of Aluminum Alloys , pp. 41-50
    • Rogers, N.L.1
  • 26
    • 0001351461 scopus 로고
    • J.W. Diggle, Vijh A.K. New York: Marcel Dekker
    • Alwitt R.S. Diggle J.W., Vijh A.K. Oxides and oxide films. Vol. 4:1976;169-254 Marcel Dekker, New York.
    • (1976) Oxides and Oxide Films , vol.4 , pp. 169-254
    • Alwitt, R.S.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.