Volumn 69, Issue 1, 2004, Pages 105-113

Delayed fracture of Ni-Ti superelastic alloys in acidic and neutral fluoride solutions

Author keywords

Corrosion; Delayed fracture; Fluoride; Hydrogen embrittlement; Ni Ti

Indexed keywords

ACIDITY; BIODEGRADATION; ELASTICITY; FLUORIDE MINERALS; HYDROGEN EMBRITTLEMENT; STRESS ANALYSIS; SUPERALLOYS;

EID: 1642408779     PISSN: 00219304     EISSN: None     Source Type: Journal    
DOI: 10.1002/jbm.a.20122     Document Type: Article
Times cited : (61)

References (46)
  • 1
    • 0019627753 scopus 로고
    • Surface corrosion of nitinol and stainless steel under clinical conditions
    • Edie JW, Andreasen GF, Zaytoun MP. Surface corrosion of nitinol and stainless steel under clinical conditions. Angle Orthod 1981;51:319-324.
    • (1981) Angle Orthod , vol.51 , pp. 319-324
    • Edie, J.W.1    Andreasen, G.F.2    Zaytoun, M.P.3
  • 2
    • 0024023861 scopus 로고
    • Nitinol arch wire in a simulated oral environment: Changes in mechanical properties
    • Harris EF, Newman SM, Nicholson JA. Nitinol arch wire in a simulated oral environment: changes in mechanical properties. Am J Orthod Dentofac Orthop 1988;93:508-513.
    • (1988) Am J Orthod Dentofac Orthop , vol.93 , pp. 508-513
    • Harris, E.F.1    Newman, S.M.2    Nicholson, J.A.3
  • 3
    • 0025094610 scopus 로고
    • The effect of long-term deflection on permanent deformation of nickel-titanium archwires
    • Hudgins JJ, Bagby MD, Erickson LC. The effect of long-term deflection on permanent deformation of nickel-titanium archwires. Angle Orthod 1990;60:283-288.
    • (1990) Angle Orthod , vol.60 , pp. 283-288
    • Hudgins, J.J.1    Bagby, M.D.2    Erickson, L.C.3
  • 4
    • 0026235884 scopus 로고
    • Examination of Chinese NiTi wire by a combined clinical and laboratory approach
    • Mohlin B, Müller H, Ödman J, Thilander B. Examination of Chinese NiTi wire by a combined clinical and laboratory approach. Eur J Orthod 1991;13:386-391.
    • (1991) Eur J Orthod , vol.13 , pp. 386-391
    • Mohlin, B.1    Müller, H.2    Ödman, J.3    Thilander, B.4
  • 5
    • 0031129976 scopus 로고    scopus 로고
    • Surface analysis of nickeltitanium archwire used in vivo
    • Grimsdottir MR, Hensten-Pettersen A. Surface analysis of nickeltitanium archwire used in vivo. Dent Mater 1997;13:163-167.
    • (1997) Dent Mater , vol.13 , pp. 163-167
    • Grimsdottir, M.R.1    Hensten-Pettersen, A.2
  • 6
  • 7
    • 0034981405 scopus 로고    scopus 로고
    • Fracture analysis of hydrogen-charged nickel-titanium superelastic alloy
    • Yokoyama K, Hamada K, Asaoka K. Fracture analysis of hydrogen-charged nickel-titanium superelastic alloy. Mater Trans 2001;42:141-144.
    • (2001) Mater Trans , vol.42 , pp. 141-144
    • Yokoyama, K.1    Hamada, K.2    Asaoka, K.3
  • 8
    • 0035882635 scopus 로고    scopus 로고
    • Degradation and fracture of Ni-Ti superelastic wire in an oral cavity
    • Yokoyama K, Hamada K, Moriyama K, Asaoka K. Degradation and fracture of Ni-Ti superelastic wire in an oral cavity. Biomaterials 2001;22:2257-2262.
    • (2001) Biomaterials , vol.22 , pp. 2257-2262
    • Yokoyama, K.1    Hamada, K.2    Moriyama, K.3    Asaoka, K.4
  • 9
    • 0000088442 scopus 로고    scopus 로고
    • Hydrogen embrittlement of nickel-titanium alloy in biological environment
    • Asaoka K, Yokoyama K, Nagumo M. Hydrogen embrittlement of nickel-titanium alloy in biological environment. Metall Mater Trans A 2002;33A:495-501.
    • (2002) Metall Mater Trans A , vol.33 A , pp. 495-501
    • Asaoka, K.1    Yokoyama, K.2    Nagumo, M.3
  • 11
    • 0025444562 scopus 로고
    • A role of hydrogen in shape memory effect of Ti-Ni alloys
    • Wade N, Adachi Y, Hosoi Y. A role of hydrogen in shape memory effect of Ti-Ni alloys. Scripta Metall Mater 1990;24:1051-1055.
    • (1990) Scripta Metall Mater , vol.24 , pp. 1051-1055
    • Wade, N.1    Adachi, Y.2    Hosoi, Y.3
  • 12
    • 0025433782 scopus 로고
    • Effect of hydrogen on the shape memory effect and transformation behavior of Ti-Ni alloy
    • Adachi Y, Wade N, Hosoi Y. Effect of hydrogen on the shape memory effect and transformation behavior of Ti-Ni alloy. J Jpn Inst Metals 1990;54:525-531.
    • (1990) J Jpn Inst Metals , vol.54 , pp. 525-531
    • Adachi, Y.1    Wade, N.2    Hosoi, Y.3
  • 13
    • 0000330248 scopus 로고
    • Effect of a small amount of hydrogen on pseudo-elastic properties of Ti-Ni alloy
    • Asaoka T, Yamashita H, Saito H, Ishida Y. Effect of a small amount of hydrogen on pseudo-elastic properties of Ti-Ni alloy. J Jpn Inst Metals 1993;57:1123-1129.
    • (1993) J Jpn Inst Metals , vol.57 , pp. 1123-1129
    • Asaoka, T.1    Yamashita, H.2    Saito, H.3    Ishida, Y.4
  • 15
    • 0001368224 scopus 로고
    • Delayed fracture of metals under static load
    • Petch J, Stables P. Delayed fracture of metals under static load. Nature 1952;169:842-843.
    • (1952) Nature , vol.169 , pp. 842-843
    • Petch, J.1    Stables, P.2
  • 16
    • 0000934315 scopus 로고
    • Delayed failure and hydrogen embrittlement in steel
    • Frohmberg RP, Barnett WJ, Troiano AR. Delayed failure and hydrogen embrittlement in steel. Trans ASM 1955;47:892-925.
    • (1955) Trans ASM , vol.47 , pp. 892-925
    • Frohmberg, R.P.1    Barnett, W.J.2    Troiano, A.R.3
  • 18
    • 0015300738 scopus 로고
    • A new model for hydrogen-assisted cracking (hydrogen " embrittlement")
    • Beachem CD. A new model for hydrogen-assisted cracking (hydrogen "embrittlement"). Metall Trans 1972;3:437-451.
    • (1972) Metall Trans , vol.3 , pp. 437-451
    • Beachem, C.D.1
  • 19
    • 0019031617 scopus 로고
    • Effects of hydrogen on the properties of iron and steel
    • Hirth JP. Effects of hydrogen on the properties of iron and steel. Metall Trans A 1980;11A:861-890.
    • (1980) Metall Trans A , vol.11 A , pp. 861-890
    • Hirth, J.P.1
  • 20
    • 0000553707 scopus 로고
    • Delayed fracture of high strength steels
    • Matsuyama S. Delayed fracture of high strength steels. Tetsuto-Hagané 1994;80:679-684.
    • (1994) Tetsuto-Hagané , vol.80 , pp. 679-684
    • Matsuyama, S.1
  • 21
    • 0035246969 scopus 로고    scopus 로고
    • Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels
    • Nagumo M, Nakamura M, Takai K. Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels. Metall Mater Trans A 2001;32A:339-347.
    • (2001) Metall Mater Trans A , vol.32 A , pp. 339-347
    • Nagumo, M.1    Nakamura, M.2    Takai, K.3
  • 22
    • 0036817422 scopus 로고    scopus 로고
    • Evaluation method of delayed fracture property and overcoming techniques of delayed fracture of high strength steels
    • Tarui T, Yamasaki S. Evaluation method of delayed fracture property and overcoming techniques of delayed fracture of high strength steels. Tetsu-to-Hagané 2002;88:612-619.
    • (2002) Tetsu-to-Hagané , vol.88 , pp. 612-619
    • Tarui, T.1    Yamasaki, S.2
  • 23
    • 0021981642 scopus 로고
    • Accelerated oxide grown on titanium implants during autoclaving caused by fluorine contamination
    • Lausmaa J, Kasemo B, Hansson S. Accelerated oxide grown on titanium implants during autoclaving caused by fluorine contamination. Biomaterials 1985;6:23-27.
    • (1985) Biomaterials , vol.6 , pp. 23-27
    • Lausmaa, J.1    Kasemo, B.2    Hansson, S.3
  • 24
    • 0026124943 scopus 로고
    • The effect of oral topical fluorides on the surface of commercially pure titanium
    • Siirilä HS, Könn̈en M. The effect of oral topical fluorides on the surface of commercially pure titanium. Int J Oral Maxillofac Implants 1991;6:50-54.
    • (1991) Int J Oral Maxillofac Implants , vol.6 , pp. 50-54
    • Siirilä, H.S.1    Könn̈en, M.2
  • 26
    • 0029415082 scopus 로고
    • Influence of fluoride on titanium in an acidic environment measured by polarization resistance technique
    • Boere G. Influence of fluoride on titanium in an acidic environment measured by polarization resistance technique. J Appl Biomater 1995;6:283-288.
    • (1995) J Appl Biomater , vol.6 , pp. 283-288
    • Boere, G.1
  • 27
    • 0029685412 scopus 로고    scopus 로고
    • Corrosive properties of fluoride-containing odontologic gels against titanium
    • Toumelin-Chemla F, Rouelle F, Burdairon G. Corrosive properties of fluoride-containing odontologic gels against titanium. J Dent 1996;24:109-115.
    • (1996) J Dent , vol.24 , pp. 109-115
    • Toumelin-Chemla, F.1    Rouelle, F.2    Burdairon, G.3
  • 28
    • 0000823852 scopus 로고    scopus 로고
    • Electrochemical corrosion behavior of titanium castings. 1. Effects of degree of surface polishing and kind of solution
    • Mimura H, Miyagawa Y. Electrochemical corrosion behavior of titanium castings. 1. Effects of degree of surface polishing and kind of solution. Jpn J Dent Mater Dev 1996;15:283-295.
    • (1996) Jpn J Dent Mater Dev , vol.15 , pp. 283-295
    • Mimura, H.1    Miyagawa, Y.2
  • 29
    • 0001041398 scopus 로고    scopus 로고
    • The influence of fluoride concentration on the corrosion of titanium and titanium alloys
    • Oda Y, Kawada E, Yoshinari M, Hasegawa K, Okabe T. The influence of fluoride concentration on the corrosion of titanium and titanium alloys. Jpn J Dent Mater Dev 1996;15:317-322.
    • (1996) Jpn J Dent Mater Dev , vol.15 , pp. 317-322
    • Oda, Y.1    Kawada, E.2    Yoshinari, M.3    Hasegawa, K.4    Okabe, T.5
  • 30
    • 0031864346 scopus 로고    scopus 로고
    • Effects of fluorides on titanium and other dental alloys in dentistry
    • Reclaru L, Meyer J-M. Effects of fluorides on titanium and other dental alloys in dentistry. Biomaterials 1998;19:85-92.
    • (1998) Biomaterials , vol.19 , pp. 85-92
    • Reclaru, L.1    Meyer, J.-M.2
  • 31
    • 0033278195 scopus 로고    scopus 로고
    • Effect of fluoride concentration and pH on corrosion behavior of titanium for dental use
    • Nakagawa M, Matsuya S, Shiraishi T, Ohta M. Effect of fluoride concentration and pH on corrosion behavior of titanium for dental use. J Dent Res 1999;78:1568-1572.
    • (1999) J Dent Res , vol.78 , pp. 1568-1572
    • Nakagawa, M.1    Matsuya, S.2    Shiraishi, T.3    Ohta, M.4
  • 32
    • 0035757573 scopus 로고    scopus 로고
    • Corrosion behavior of pure titanium and titanium alloys in fluoride-containing solutions
    • Nakagawa M, Matsuya S, Udoh K. Corrosion behavior of pure titanium and titanium alloys in fluoride-containing solutions. Dent Mater J 2001;20:305-314.
    • (2001) Dent Mater J , vol.20 , pp. 305-314
    • Nakagawa, M.1    Matsuya, S.2    Udoh, K.3
  • 33
    • 0036617834 scopus 로고    scopus 로고
    • Effects of fluoride and dissolved oxygen concentrations on the corrosion behavior of pure titanium and titanium alloys
    • Nakagawa M, Matsuya S, Udoh K. Effects of fluoride and dissolved oxygen concentrations on the corrosion behavior of pure titanium and titanium alloys. Dent Mater J 2002;21:83-92.
    • (2002) Dent Mater J , vol.21 , pp. 83-92
    • Nakagawa, M.1    Matsuya, S.2    Udoh, K.3
  • 34
    • 0036027441 scopus 로고    scopus 로고
    • Effects of fluoride concentration and elastic tensile strain on the corrosion resistance of commercially pure titanium
    • Huang H-H. Effects of fluoride concentration and elastic tensile strain on the corrosion resistance of commercially pure titanium. Biomaterials 2002;23:59-63.
    • (2002) Biomaterials , vol.23 , pp. 59-63
    • Huang, H.-H.1
  • 35
    • 0037172274 scopus 로고    scopus 로고
    • Electrochemical impedance spectroscopy study of strained titanium in fluoride media
    • Huang H-H. Electrochemical impedance spectroscopy study of strained titanium in fluoride media. Elecrochimica Acta 2002;47:2311-2318.
    • (2002) Elecrochimica Acta , vol.47 , pp. 2311-2318
    • Huang, H.-H.1
  • 36
    • 0036210742 scopus 로고    scopus 로고
    • Influence of fluoride content and pH on the corrosion resistance of titanium and its alloys
    • Schiff N, Grosgogeat B, Lissac M, Dalard F. Influence of fluoride content and pH on the corrosion resistance of titanium and its alloys. Biomaterials 2002;23:1995-2002.
    • (2002) Biomaterials , vol.23 , pp. 1995-2002
    • Schiff, N.1    Grosgogeat, B.2    Lissac, M.3    Dalard, F.4
  • 37
    • 0035312719 scopus 로고    scopus 로고
    • Accelerated failure in high strength steel by alternating hydrogen-charging potential
    • Nagumo M, Uyama H, Yoshizawa M. Accelerated failure in high strength steel by alternating hydrogen-charging potential. Scripta Mater 2001;44:947-952.
    • (2001) Scripta Mater , vol.44 , pp. 947-952
    • Nagumo, M.1    Uyama, H.2    Yoshizawa, M.3
  • 39
    • 0000071418 scopus 로고    scopus 로고
    • XPS characterisation of surface modified Ni-Ti shape memory alloy
    • Green SM, Grant DM, Wood JV. XPS characterisation of surface modified Ni-Ti shape memory alloy. Mater Sci Eng A 1997;224:21-26.
    • (1997) Mater Sci Eng A , vol.224 , pp. 21-26
    • Green, S.M.1    Grant, D.M.2    Wood, J.V.3
  • 40
    • 0037190949 scopus 로고    scopus 로고
    • Surface characterization of NiTi modified by plasma source ion implantation
    • Tan L, Crone WC. Surface characterization of NiTi modified by plasma source ion implantation. Acta Mater 2002;50:4449-4460.
    • (2002) Acta Mater , vol.50 , pp. 4449-4460
    • Tan, L.1    Crone, W.C.2
  • 41
    • 0023995114 scopus 로고
    • Interstitial ordering of hydrogen and oxygen in TiNi alloys
    • Wu SK, Wayman CM. Interstitial ordering of hydrogen and oxygen in TiNi alloys. Acta Metall 1988;36:1005-1013.
    • (1988) Acta Metall , vol.36 , pp. 1005-1013
    • Wu, S.K.1    Wayman, C.M.2
  • 42
    • 0024719938 scopus 로고
    • Crystal structure of a hydride formed by electrochemical hydrogenation in a TiNi-Al alloy
    • Nam TH, Shimizu K, Saburi T, Nenno S. Crystal structure of a hydride formed by electrochemical hydrogenation in a TiNi-Al alloy. Mater Trans JIM 1989;30:539-548.
    • (1989) Mater Trans JIM , vol.30 , pp. 539-548
    • Nam, T.H.1    Shimizu, K.2    Saburi, T.3    Nenno, S.4
  • 44
    • 0141907230 scopus 로고    scopus 로고
    • Degradation of tensile strength of Ni-Ti superelastic alloy due to hydrogen absorption in methanol solution containing hydrochloric acid
    • Yokoyama K, Ogawa T, Asaoka K, Sakai J, Nagumo M. Degradation of tensile strength of Ni-Ti superelastic alloy due to hydrogen absorption in methanol solution containing hydrochloric acid. Mater Sci Eng A 2003;360:153-159.
    • (2003) Mater Sci Eng A , vol.360 , pp. 153-159
    • Yokoyama, K.1    Ogawa, T.2    Asaoka, K.3    Sakai, J.4    Nagumo, M.5
  • 45
    • 0016090988 scopus 로고
    • Stress corrosion and hydrogen embrittlement in an aluminum alloy
    • Gest RJ, Troiano AR. Stress corrosion and hydrogen embrittlement in an aluminum alloy. Corrosion 1974;30:274-279.
    • (1974) Corrosion , vol.30 , pp. 274-279
    • Gest, R.J.1    Troiano, A.R.2
  • 46
    • 0036604866 scopus 로고    scopus 로고
    • Hydrogen effects during IGSCC of pure A1-5Mg alloy in NaCl media
    • Tanguy D, Bayle B, Dif R, Magnin TH. Hydrogen effects during IGSCC of pure A1-5Mg alloy in NaCl media. Corros Sci 2002;44:1163-1175.
    • (2002) Corros Sci , vol.44 , pp. 1163-1175
    • Tanguy, D.1    Bayle, B.2    Dif, R.3    Magnin, T.H.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.